# US 2012/0251838 A1 · Coated article and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251838 A1
- Document ID: US20120251838A1
- Status: Published application
- Kind: A1
- Application number: 13/226,657
- Filed: 2011-09-07
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: FIH (Hong Kong) Limited; Shenzhen Futaihong Precision Industry Co., Ltd.
- Inventors: CHWAN-HWA CHIANG; JIA-LIN CHEN; YI-JUN HUANG; HAI-BO PAN; XU LI
- Web page: https://patentgrep.com/patent/US20120251838A1

## CPC

- C23C 14/0036: {Reactive sputtering}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/165: {by cathodic sputtering}
- C23C 14/46: by ion beam produced by an external ion source
- Y10T 428/12597: Noncrystalline silica or noncrystalline plural-oxide component [e.g., glass, etc.]
- Y10T 428/12729: Group IIA metal-base component
- Y10T 428/12743: Next to refractory [Group IVB, VB, or VIB] metal-base component
- Y10T 428/12806: Refractory [Group IVB, VB, or VIB] metal-base component
- Y10T 428/265: 1 mil or less
- Y10T 428/31678: Of metal
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A coated article is described. The coated article includes a substrate, a titanium bonding layer, a titanium-chromium alloy transition layer, and a titanium-chromium-nitrogen hard layer formed thereon, and in that order. The titanium bonding layer is a titanium layer. The titanium-chromium alloy transition layer is a titanium-chromium alloy layer. The titanium-chromium-nitrogen hard layer is a titanium-chromium-nitrogen layer. The titanium bonding layer, titanium-chromium alloy transition layer, and the titanium-chromium-nitrogen hard layer are formed by ion beam assisted sputtering.

## Claims

### Claim 1

A coated article, comprising:
a substrate;
a titanium bonding layer formed on the substrate;
a titanium-chromium alloy transition layer formed on the titanium bonding layer; and
a titanium-chromium-nitrogen hard layer formed on the titanium-chromium alloy transition layer.

### Claim 2 (depends on 1)

The coated article as claimed in claim 1, wherein within the titanium-chromium alloy transition layer, the titanium has an atomic percentage of about 30%-40%; the chromium has an atomic percentage of about 60%-70%.

### Claim 3 (depends on 1)

The coated article as claimed in claim 1, wherein within the titanium-chromium-nitrogen hard layer, the titanium has an atomic percentage of about 25.6%-37.0%, the chromium has an atomic percentage of about 51.7%-67.6%, and the nitrogen has an atomic percentage of about 5.4%-13.8%.

### Claim 4 (depends on 1)

The coated article as claimed in claim 1, wherein the titanium bonding layer and the titanium-chromium alloy transition layer each has a thickness of about 0.1 μm-0.4 μm.

### Claim 5 (depends on 1)

The coated article as claimed in claim 1, wherein the titanium-chromium-nitrogen hard layer has a thickness of about 1.3 μm-1.7 μm.

### Claim 6 (depends on 1)

The coated article as claimed in claim 1, wherein the coated article has a surface micro-hardness of about 600 HV0.025-700 HV0.025.

### Claim 7 (depends on 1)

The coated article as claimed in claim 1, wherein the titanium bonding layer, titanium-chromium alloy transition layer, and the titanium-chromium-nitrogen hard layer are formed by ion beam assisted sputtering.

### Claim 8 (depends on 1)

The coated article as claimed in claim 1, wherein the substrate is made of a material selected from the group consisting of high speed steel, hard alloy, stainless steel, titanium alloy, magnesium alloy, aluminum alloy, ceramic and glass.

### Claim 9

A method for manufacturing a coated article, comprising steps of:
providing a substrate;
forming a titanium bonding layer on the substrate by ion beam assisted sputtering;
forming a titanium-chromium alloy transition layer on the titanium bonding layer by ion beam assisted sputtering; and
forming a titanium-chromium-nitrogen hard layer on the titanium-chromium alloy transition layer by ion beam assisted sputtering.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein during the ion beam assisted sputtering of the titanium bonding layer, the titanium-chromium alloy transition layer, and the titanium-chromium-nitrogen hard layer, ion beams bombard the substrate.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein during the ion beam assisted sputtering of the titanium bonding layer, the substrate is placed in a vacuum chamber of an ion beam assisted sputtering machine; argon as a sputtering gas is fed into the vacuum chamber and create a pressure of about 0.3 Pa-0.5 Pa; the temperature in the vacuum chamber is maintained at about 150° C.-250 V; about 3.8 kW-4.2 kW of power is applied to at least one titanium target; the ion beams are generated by applying a power source at a power of about 1 kW-1.5 kW bombard the substrate.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein ion beam assisted sputtering the titanium bonding layer takes about 5 min-10 min.

### Claim 13 (depends on 11)

The method as claimed in claim 11, wherein during the ion beam assisted sputtering of the titanium-chromium alloy transition layer, the substrate is placed in a vacuum chamber of an ion beam assisted sputtering machine; argon as a sputtering gas is fed into the vacuum chamber and create a pressure of about 0.3 Pa-0.5 Pa; the temperature in the vacuum chamber is maintained at about 150° C.-250° C.; about 3.8 kW-4.2 kW of power is applied to at least one titanium target and at least one chromium target; the ion beams are generated by applying a power source at a power of about 1 kW-1.5 kW bombard the substrate.

### Claim 14 (depends on 13)

The method as claimed in claim 13, wherein ion beam assisted sputtering the titanium-chromium alloy transition layer takes about 5 min-10 min.

### Claim 15 (depends on 11)

The method as claimed in claim 11, wherein during the ion beam assisted sputtering of the titanium-chromium-nitrogen hard layer, the substrate is placed in a vacuum chamber of an ion beam assisted sputtering machine; argon and nitrogen are simultaneously is fed into the vacuum chamber, with the argon acting as a sputtering gas and the nitrogen acting as a reaction gas, argon creates a pressure of about 0.3 Pa-0.5 Pa, the ratio of pressure created by argon and pressure created by nitrogen is about 1.5 to about 2.0; the temperature in the vacuum chamber is maintained at about 150° C.-250° C.; about 3.8 kW-4.2 kW of power is applied to at least one titanium target and at least one chromium target; the ion beams are generated by applying a power source at a power of about 1 kW-1.5 kW bombard the substrate.

### Claim 16 (depends on 15)

The method as claimed in claim 15, wherein ion beam assisted sputtering the titanium-chromium-nitrogen hard layer takes about 30 min-50 min.