# US 2012/0251813 A1 · Light weight gypsum board

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251813 A1
- Document ID: US20120251813A1
- Status: Published application
- Kind: A1
- Application number: 13/493,941
- Filed: 2012-06-11
- Published: 2012-10-04
- Earliest claimed: 2005-06-09
- Assignees: United States Gypsum Company
- Inventors: Qiang YU; Weixin David SONG; Michael LYNN
- Web page: https://patentgrep.com/patent/US20120251813A1

## CPC

- C04B 11/00: Calcium sulfate cements
- C04B 22/16: containing phosphorus in the anion, e.g. phosphates
- C04B 24/226: {Sulfonated naphtalene-formaldehyde condensation products}
- C04B 24/383: {Cellulose or derivatives thereof}
- C04B 28/14: containing calcium sulfate cements {(gypsum-paper plates E04C)}
- C04B 2103/0045: {Polymers chosen for their physico-chemical characteristics}
- C04B 2103/408: {Dispersants}
- C04B 2111/0062: {Gypsum-paper board like materials}
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- Y10T 428/249953: Composite having voids in a component [e.g., porous, cellular, etc.]
- Y10T 428/2978: Surface characteristic
- Y10T 428/31971: Of carbohydrate
- Y10T 428/31993: Of paper
- Y10T 442/665: Including a layer derived from a water-settable material [e.g., cement, gypsum, etc.]
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention generally provides gypsum-containing slurries including stucco, naphthalenesulfonate dispersant, and pregelatinized starch. The naphthalenesulfonate dispersant is present in an amount of about 0.1%-3.0% by weight based on the weight of dry stucco. The pregelatinized starch is present in an amount of at least about 0.5% by weight up to about 10% by weight of pregelatinized starch by weight based on the weight of dry stucco in the formulation. Other slurry additives can include trimetaphosphate salts, accelerators, binders, paper fiber, glass fiber, and other known ingredients. The invention also comprises the gypsum-containing products made with such slurries, for example, gypsum wallboard, and a method of making gypsum wallboard.

## Claims

### Claim 1

A light weight gypsum board comprising:
a set gypsum composition disposed between two cover sheets, the gypsum composition formed from at least water, stucco, starch, and foaming agent;
the starch is in an amount from about 0.5% to about 10% by weight based on the weight of the stucco;
the foaming agent comprises a major weight portion of unstable component and a minor weight portion of stable component, the amount of foaming agent and the weight ratio of said unstable component to stable component effective to form a void distribution within said gypsum composition;
the starch and the void distribution are effective to provide a board density of about 34 lb/ft3 or less and a core hardness of at least about 11 lb, the core hardness determined according to ASTM standard C473.

### Claim 2 (depends on 1)

The light weight gypsum board of claim 1, wherein the foaming agent comprises a blend of the unstable and stable components.

### Claim 3 (depends on 1)

The light weight gypsum board of claim 1, wherein the foaming agent comprises at least about 65% by weight of unstable component.

### Claim 4 (depends on 1)

The light weight gypsum board of claim 1, wherein the foaming agent is in an amount of 0.1% or less by weight based on the weight of the stucco.

### Claim 5 (depends on 1)

The light weight gypsum board of claim 1, wherein the foaming agent is in an amount from about 0.02% to about 0.03% by weight based on the weight of the stucco.

### Claim 6 (depends on 1)

The light weight gypsum board of claim 1, wherein the gypsum composition is formed from a water to stucco weight ratio from about 0.7 to about 1.2.

### Claim 7 (depends on 1)

The light weight gypsum board of claim 1, wherein the starch is effective to increase the core hardness of the gypsum composition relative to the gypsum composition without the starch.

### Claim 8 (depends on 7)

The light weight gypsum board of claim 7, wherein the starch is in an amount from about 0.5% to about 3% by weight based on the weight of the stucco.

### Claim 9 (depends on 7)

The light weight gypsum board of claim 7, wherein the starch comprises a pregelatinized starch and is in an amount from about 0.5% to about 6% by weight based on the weight of the stucco.

### Claim 10 (depends on 1)

The light weight gypsum board of claim 1, wherein the board has a humidified bond load of at least about 15 lb after being (a) conditioned for about 6 hours in an environment sufficient to produce conditions of 90% relative humidity and 90° F. temperature, and (b) dried to constant weight.

### Claim 11 (depends on 1)

The light weight gypsum of claim 1, wherein the set gypsum composition is further formed from at least dispersant.

### Claim 12 (depends on 1)

The light weight gypsum of claim 1, wherein the set gypsum composition is further formed from at least naphthalenesulfonate dispersant in an amount from about 0.2% to about 3.0% by weight based on the weight of the stucco.

### Claim 13 (depends on 1)

The light weight gypsum board of claim 1, wherein the set gypsum composition is further formed from at least polyphosphate in an amount from about 0.12% to about 0.4% by weight based on the weight of the stucco.

### Claim 14 (depends on 1)

The light weight gypsum board of claim 1, wherein:
the starch is effective to increase the core hardness of the gypsum composition relative to the gypsum composition without the starch;
the board has a humidified bond load of at least about 15 lb after being (a) conditioned for about 6 hours in an environment sufficient to produce conditions of 90% relative humidity and 90° F. temperature, and (b) dried to constant weight; and
at a board thickness of about ½ inch, the board has a nail pull resistance of at least about 65 lb, as determined according to ASTM standard C473.

### Claim 15 (depends on 14)

The light weight gypsum board of claim 14, wherein:
the foaming agent is in an amount of 0.1% or less by weight based on the weight of the stucco; and
at a board thickness of about ½ inch, the board has a nail pull resistance of at least about 72 lb, as determined according to ASTM standard C473.

### Claim 16 (depends on 1)

The light weight gypsum board of claim 1, wherein:
the board has a humidified bond load of at least about 17 lb after being (a) conditioned for about 6 hours in an environment sufficient to produce conditions of 90% relative humidity and 90° F. temperature, and (b) dried to constant weight; and
at a board thickness of about ½ inch, the board has a nail pull resistance of at least about 77 lb, as determined according to ASTM standard C473.

### Claim 17 (depends on 15)

The light weight gypsum board of claim 15, wherein at a board thickness of about ½ inch, the board has flexural strength of at least about 36 lb in a machine direction and/or about 107 lb in a cross-machine direction, as determined according to ASTM standard C473.

### Claim 18 (depends on 17)

The light weight gypsum board of claim 17, wherein:
the set gypsum composition is further formed from dispersant in an amount from about 0.2% to about 3.0% by weight based on the weight of the stucco;
the gypsum composition is formed from a water to stucco weight ratio from about 0.7 to about 1.2; and
the board has a humidified bond load of at least about 17 lb after being (a) conditioned for about 6 hours in an environment sufficient to produce conditions of 90% relative humidity and 90° F. temperature, and (b) dried to constant weight.

### Claim 19 (depends on 18)

The light weight gypsum board of claim 18, wherein the set gypsum composition is further formed from sodium trimetaphosphate in an amount from about 0.12% to about 0.4% by weight based on the weight of the stucco.

### Claim 20

A light weight gypsum board comprising:
a set gypsum composition disposed between two cover sheets, the set gypsum composition formed from at least water, stucco, starch, dispersant, and polyphosphate;
the stucco is in an amount of at least about 700 lb/MSF;
the starch is in an amount from about 0.5% to about 10% by weight based on the weight of the stucco and is effective to increase the core hardness of the gypsum composition relative to the gypsum composition without the starch;
the dispersant is in an amount from about 0.1% to about 3.0% by weight based on the weight of the stucco;
the polyphosphate is in an amount from about 0.12% to about 0.4% by weight based on the weight of the stucco;
the board has a density of about 34 lb/ft3 or less; and
the board has a core hardness of at least about 11 lb, the core hardness determined according to ASTM standard C473.

### Claim 21 (depends on 20)

The light weight gypsum board of claim 20, wherein the stucco is in an amount from about 700 lb/MSF to about 1300 lb/MSF.

### Claim 22 (depends on 20)

The light weight gypsum board of claim 20, wherein the set gypsum composition is further formed from at least foaming agent having a major weight portion of unstable component and a minor weight portion of stable component, the amount of foaming agent and the weight ratio of said unstable component to stable component forming a void distribution within said gypsum composition.

### Claim 23 (depends on 22)

The light weight gypsum board of claim 22, wherein the foaming agent is in an amount of 0.1% or less by weight based on the weight of the stucco.

### Claim 24 (depends on 22)

The light weight gypsum board of claim 22, wherein the foaming agent is in an amount from about 0.02% to about 0.03% by weight based on the weight of the stucco.

### Claim 25 (depends on 20)

The light weight gypsum board of claim 20, further comprising paper fiber and/or glass fiber in an amount from about 0.20% to 1.30% based on the weight of the dry stucco.

### Claim 26 (depends on 20)

The light weight gypsum board of claim 20, further comprising accelerator in an amount from about 0.2% to about 0.9% based on the weight of the dry stucco.

### Claim 27 (depends on 20)

The light weight gypsum board of claim 20, wherein the gypsum composition is formed from a water to stucco weight ratio from about 0.7 to about 1.2.

### Claim 28 (depends on 20)

The light weight gypsum board of claim 20, wherein:
the set gypsum composition is further formed from at least foaming agent and accelerator;
the stucco is in an amount from about 700 lb/MSF to about 1300 lb/MSF;
the starch is in an amount from about 0.5% to about 6% by weight based on the weight of the stucco;
the dispersant is in an amount from about 0.2% to about 3.0% by weight based on the weight of the stucco;
the foaming agent has a major weight portion of unstable component and a minor weight portion of stable component, the amount of foaming agent and the weight ratio of said unstable component to stable component effective to form a void distribution within said gypsum composition, wherein the foaming agent is in an amount of 0.1% or less by weight based on the weight of the stucco;
the starch and the void distribution are effective to provide a board density of about 24 lb/ft3 to about 34 lb/ft3 and, at a board thickness of ½ inch, said core hardness of at least about 11 lb, a nail pull resistance of at least about 65 lb, and a flexural strength of at least about 36 lb in a machine direction and/or about 107 lb in a cross-machine direction, the nail pull resistance and the flexural strength determined according to ASTM standard C473; and
the board has a humidified bond load of at least about 15 lb after being (a) conditioned for about 6 hours in an environment sufficient to produce conditions of 90% relative humidity and 90° F. temperature, and (b) dried to constant weight.

### Claim 29 (depends on 28)

The light weight gypsum board of claim 28, wherein the foaming agent is in an amount from about 0.02% to about 0.03% by weight based on the weight of the stucco.

### Claim 30 (depends on 28)

The light weight gypsum board of claim 28, wherein:
the set gypsum composition is further formed from at least paper fiber and/or glass fiber;
the gypsum composition is formed from a water to stucco weight ratio from about 0.7 to about 1.2;
the starch comprises pregelatinized starch;
the dispersant comprises naphthalenesulfonate;
the phosphate comprises sodium trimetaphosphate;
the paper fiber and/or glass fiber is present in an amount from about 0.20% to 1.30% by weight based on the weight of the stucco;
the accelerator comprises heat resistant accelerator and is present in an amount from about 0.2% to about 0.9% by weight based on the weight of the stucco; and
the board has a humidified bond load of at least about 17 lb after being (a) conditioned for about 6 hours in an environment sufficient to produce conditions of 90% relative humidity and 90° F. temperature, and (b) dried to constant weight.