# US 2012/0251809 A1 · Biaxially oriented polypropylene film substrate free from primer coating and film free from primer coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251809 A1
- Document ID: US20120251809A1
- Status: Published application
- Kind: A1
- Application number: 13/516,388
- Filed: 2010-12-28
- Published: 2012-10-04
- Earliest claimed: 2009-12-29
- Assignees: Hainan Shiner Industrial Co., Ltd.
- Inventors: Tan Li; Hongcun Huang; Lianqin Hu
- Web page: https://patentgrep.com/patent/US20120251809A1

## CPC

- C09D 123/12: Polypropene
- B32B 27/08: of synthetic resin
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- C09D 4/06: {Organic non-macromolecular compounds having at least one polymerisable carbon-to-carbon unsaturated bond} in combination with a macromolecular compound other than an unsaturated polymer of groups C09D159/00 - C09D187/00
- C09D 133/02: Homopolymers or copolymers of acids; Metal or ammonium salts thereof
- C09D 133/08: Homopolymers or copolymers of acrylic acid esters
- Y10T 428/265: 1 mil or less
- Y10T 428/31667: Next to addition polymer from unsaturated monomers, or aldehyde or ketone condensation product
- Y10T 428/31801: Of wax or waxy material
- Y10T 428/31924: Including polyene monomers
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Disclosed is a biaxially oriented polypropylene film substrate free from primer coating, which comprises successively connected affinity layer, core layer and surface layer, said affinity layer comprises 10% to 80% by weight of polypropylene homopolymer, 10% to 80% by weight of polyolefin plastomer and 1% to 10% by weight of anti-adhesion agent; said core layer is polypropylene homopoiymer; said surface layer is the same as the affinity layer or a non-coated surface layer that comprises 90% to 99% by weight of polypropylene homopolymer and 1% to 10% by weight of anti-adhesion agent. A film free from primer coating and its preparing method are also provided. The coated film of this invention does not need the process of primer pre-coating which reduces the relevant equipment costs on one hand and avoids the safety risks when using and restoring solvent type primer on the other.

## Claims

### Claim 1

A biaxially oriented polypropylene film substrate which is free from primer, characterized in that it comprises successively connected affinity layer, core layer and surface layer, the affinity layer comprises 10% to 80% by weight of polypropylene homopolymer, 10% to 80% by weight of polyolefin plastomer and 1% to 10% by weight of anti-adhesion agent; the core layer is polypropylene homopolymer; the surface layer is the same as the affinity layer or a non-coated surface layer, said non-coated surface layer comprises 90% to 99% by weight of polypropylene homopolymer and 1% to 10% by weight of anti-adhesion agent.

### Claim 2 (depends on 1)

The biaxially oriented polypropylene film substrate according to claim 1, characterized in that the thickness of the affinity layer is 1 μm to 10 μm.

### Claim 3 (depends on 1)

The biaxially oriented polypropylene film substrate according to claim 1, characterized in that the thickness of the non-coated surface layer is 1 μm to 10 μm.

### Claim 4 (depends on 1)

The biaxially oriented polypropylene film substrate according to claim 1, characterized in that the total thickness of the biaxially oriented polypropylene film substrate free from primer is 10 μm to 60 μm.

### Claim 5 (depends on 1)

The biaxially oriented polypropylene film substrate according to claim 1, characterized in that the active ingredients content of the anti-adhesion agent is 500 PPM to 5000 PPM.

### Claim 6 (depends on 1)

A coated film free from primer, characterized in that: said film comprises the biaxially oriented polypropylene film substrate according to claim 1 5, and a coating layer placed on the surface of the substrate, said coating layer is polyvinylidene chloride coating, acrylic acid coating or modified polyvinyl alcohol coating;
the polyvinylidene chloride coating is formed by coating the substrate surface with the following ingredients followed by drying: 30% to 95% by weight of polyvinylidene chloride emulsion, 0 to 50% by weight of softened water, 1% to 12% by weight of slip agent and 0.05% to 5% by weight of anti-adhesion agent; said polyvinylidene chloride emulsion is formed by reaction of 85% to 95% by weight of polyvinylidene chloride, 0.5% to 10% by weight of methyl methacrylate, 0.5% to 3.5% by weight of methyl acrylate, 0.01% to 0.3% by weight of catalyst and 0.2% to 3.5% by weight of emulsifying agent;
the acrylic acid coating is formed by coating the substrate surface with the following ingredients followed by drying: 25% to 95% by weight of acrylic acid emulsion, 0 to 70% by weight of softened water, 2% to 15% by weight of slip agent and 0.1% to 5% by weight of anti-adhesion agent, said acrylic acid emulsion is formed by copolymerization of 10% to 80% by weight of acrylic acid and 20% to 90% by weight of methyl acrylate or ethyl acrylate;
the modified polyvinyl alcohol coating is formed by coating the substrate surface with the following ingredients followed by drying: 50% to 100% by weight of modified polyvinyl alcohol solution, 0 to 40% by weight of softened water, 0 to 10% by weight of slip agent and 0 to 4% by weight of anti-adhesion agent; said polyvinyl alcohol solution is formed by reaction of 5% to 15% by weight of polyvinyl alcohol, 82% to 92% by weight of softened water, 0.05% to 0.1% by weight of catalyst, 0.5% to 2% by weight of condensing agent, 0.1% to 0.5% by weight of antifoaming agent and 0.5% to 1.5% by weight of anti-adhesion agent.

### Claim 7 (depends on 6)

The coated film according to claim 6, characterized in that: the coating layer is placed on one surface or both surfaces of the substrate.

### Claim 8 (depends on 6)

The coated film according to claim 6, characterized in that the solid content of the polyvinylidene chloride coating is 20% to 60%, the solid content of slip agent is 10% to 30%, and the solid content of anti-adhesion agent is 5% to 20%.

### Claim 9 (depends on 6)

The coated film according to claim 6, characterized in that the solid content of the acrylic acid emulsion is 10% to 50%, the solid content of slip agent is 10% to 30%, and the solid content of anti-adhesion agent is 5% to 20%.

### Claim 10 (depends on 6)

The coated film according to claim 6, characterized in that the solid content of the modified polyvinyl alcohol solution is 5% to 20%, the solid content of slip agent is 10% to 30%, and the solid content of anti-adhesion agent is 5% to 20%.

### Claim 11 (depends on 6)

The coated film according to claim 6, characterized in that the thickness of the polyvinylidene chloride coating is: 0.3 μm to 6.0 μm; the thickness of the acrylic acid coating is: 0.3 μm to 3.5 μm; and the thickness of the modified polyvinyl alcohol is: 0.3 μm to 2.0 μm.

### Claim 12 (depends on 6)

The coated film according to claim 6, characterized in that the slip agent is palm wax.

### Claim 13 (depends on 6)

The coated film according to claim 6, characterized in that the anti-adhesion agent is silicon dioxide.

### Claim 14 (depends on 1)

A manufacturing method of a coated film, characterized in that said method comprises:
the biaxially oriented polypropylene film substrate according to claim 1 is subjected to corona treatment;
the polyvinylidene chloride coating, acrylic acid coating or modified polyvinyl alcohol coating is uniformly coated onto the corona surface of the biaxially oriented polypropylene film substrate, and the film is dried after the completion of coating to obtain coated film;
the polyvinylidene chloride coating is formed by coating the substrate surface with the following ingredients followed by drying: 30% to 95% by weight of polyvinylidene chloride emulsion, 0 to 50% by weight of softened water, 1% to 12% by weight of slip agent and 0.05% to 5% by weight of anti-adhesion agent; said polyvinylidene chloride emulsion is formed by reaction of 85% to 95% by weight of polyvinylidene chloride, 0.5% to 10% by weight of methyl methacrylate, 0.5% to 3.5% by weight of methyl acrylate, 0.01% to 0.3% by weight of catalyst and 0.2% to 3.5% by weight of emulsifying agent;
the acrylic acid coating is formed by coating the substrate surface with the following ingredients followed by drying: 25% to 95% by weight of acrylic acid emulsion, 0 to 70% by weight of softened water, 2% to 15% by weight of slip agent and 0.1% to 5% by weight of anti-adhesion agent, said acrylic acid emulsion is formed by copolymerization of 10% to 80% by weight of acrylic acid and 20% to 90% by weight of methyl acrylate or ethyl acrylate;
the modified polyvinyl alcohol coating is formed by coating the substrate surface with the following ingredients followed by drying: 50% to 100% by weight of modified polyvinyl alcohol solution, 0 to 40% by weight of softened water, 0 to 10% by weight of slip agent and 0 to 4% by weight of anti-adhesion agent; said polyvinyl alcohol solution is formed by reaction of 5% to 15% by weight of polyvinyl alcohol, 82% to 92% by weight of softened water, 0.05% to 0.1% by weight of catalyst, 0.5% to 2% by weight of condensing agent, 0.1% to 0.5% by weight of antifoaming agent and 0.5% to 1.5% by weight of anti-adhesion agent.

### Claim 15 (depends on 14)

The manufacturing method of the coated film free from primer according to claim 14, characterized in that: the coating weight of the polyvinylidene chloride coating is 0.4 g/m2-7.5 g/m2; the coating weight of the acrylic acid coating is 0.35 g/m2-4.0 g/m2; the coating weight of the modified polyvinyl alcohol coating is 0.25 g/m2-1.8 g/m2.

### Claim 16 (depends on 14)

The manufacturing method of the coated film free from primer according to claim 14, characterized in that: the coating speed is 100 m/min-250 m/min.

### Claim 17 (depends on 14)

The manufacturing method of the coated film free from primer according to claim 14, characterized in that: the drying mode is one of hot air drying and far infrared drying, or using both of them simultaneously; the drying temperature is 90° C.-140° C., and drying time is 5 seconds-20 seconds.

### Claim 18 (depends on 14)

The manufacturing method of the coated film free from primer according to claim 14, characterized in that: the coating is reverse roll-kiss coating.