# US 2012/0251769 A1 · Liquid crystalline polymer molded article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251769 A1
- Document ID: US20120251769A1
- Status: Published application
- Kind: A1
- Application number: 13/425,573
- Filed: 2012-03-21
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: Sumitomo Chemical Company, Limited
- Inventors: Hiroshi HARADA; Satoshi SEKIMURA
- Web page: https://patentgrep.com/patent/US20120251769A1

## CPC

- B29C 45/00: Injection moulding, i.e. forcing the required volume of moulding material through a nozzle into a closed mould; Apparatus therefor (injection blow-moulding B29C49/06)
- C09K 19/38: Polymers
- Y10T 428/24273: including aperture
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Provided is a liquid crystal polymer molding including an opening portion in which a weld portion has high strength and also surface properties are satisfactory. A liquid crystal polymer molding including an opening portion obtained by subjecting a liquid crystal polymer composition containing a spherical filler to injection molding, wherein the liquid crystal polymer molding includes a weld portion, formed by injection molding, which extends toward the outside from the opening portion, and the weld portion has a thickness in the opening portion of 2.5 mm or less, and also has a length, along a surface of the molding, of at least two times the thickness.

## Claims

### Claim 1

A liquid crystalline polymer molded article comprising an opening portion obtained by subjecting a liquid crystalline polymer composition containing a spherical filler to injection molding, wherein
the liquid crystalline polymer molded article includes a weld portion, formed by injection molding, which extends toward the outside from the opening portion, and
the weld portion has a thickness in the opening portion of 2.5 mm or less, and also has a length, along a surface of the molding, of at least two times the thickness.

### Claim 2 (depends on 1)

The liquid crystalline polymer molded article according to claim 1, wherein the liquid crystalline polymer is a liquid crystalline polyester.

### Claim 3 (depends on 2)

The liquid crystalline polymer molded article according to claim 2, wherein the liquid crystalline polyester includes a repeating unit derived from p-hydroxybenzoic acid in the proportion of 30 mol % or more based on the total amount of the whole repeating unit which constitutes the liquid crystalline polyester.

### Claim 4 (depends on 1)

The liquid crystalline polymer molded article according to claim 1, which is obtained by injection molding under the conditions that injection acceleration defined by dividing the maximum value of an injection rate by time required to reach the maximum value from initiation of the injection is from 1,000 to 25,000 mm/sec2, and also the maximum value of injection pressure in a mold inlet is from 5 to 150 MPa in one injection molding.

### Claim 5 (depends on 1)

The liquid crystalline polymer molded article according to claim 1, which is obtained by injection molding under the conditions that the temperature of the liquid crystalline polymer composition at the time of injection is [flow initiation temperature of the liquid crystalline polymer composition+20° C.] or higher and [flow temperature of the liquid crystalline polymer composition+80° C.] or lower.

### Claim 6 (depends on 1)

The liquid crystalline polymer molded article according to claim 1, which is obtained by injection molding under the conditions that the temperature of a mold at the time of injection molding is 80° C. or higher and [flow initiation temperature of the liquid crystalline polymer composition−100° C.] or lower.

### Claim 7 (depends on 1)