# US 2012/0251760 A1 · Glass substrate for magnetic disk and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251760 A1
- Document ID: US20120251760A1
- Status: Published application
- Kind: A1
- Application number: 13/245,252
- Filed: 2011-09-26
- Published: 2012-10-04
- Earliest claimed: 2008-12-02
- Assignees: Asahi Glass Company, Limited
- Inventors: Mizuho ISHIDA; Norihito Shida; Katsuhiro Matsumoto; Kazuo Mannami
- Web page: https://patentgrep.com/patent/US20120251760A1

## CPC

- G11B 5/8404: {manufacturing base layers}
- B24B 37/24: characterised by the composition or properties of the pad materials
- B24D 3/32: for porous or cellular structure
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)

## Abstract

A method for producing a glass substrate for a magnetic disk involving the use of a polishing pad having: a first resin foam layer which forms the polishing surface, includes a resin foam having pores with a pore diameter of more than 20 μm and has a thickness of 400 μm or less; and a second resin foam layer which is provided between a platen for fixing the polishing pad and the first resin foam layer, includes a resin foam having pores with a pore diameter of 20 μm or less and has a thickness of 50 to 250 μm, and in which a total thickness of the first resin foam layer and the second resin foam layer is 550 μm or less, and a international rubber hardness degree of the polishing pad measured by the M method according to JIS K6253 is 40 IRHD or more.

## Claims

### Claim 1

A method for producing a glass substrate for a magnetic disk, said method comprising a step of polishing a main surface of a circular glass plate while supplying a polishing slurry containing a polishing material,
wherein polishing is performed, after a polishing surface is subjected to dressing treatment, by using a polishing pad having: a first resin foam layer which forms the polishing surface, comprises a resin foam having pores with a pore diameter of more than 20 μm and has a thickness of 400 μm or less; and a second resin foam layer which is provided between a platen for fixing the polishing pad and the first resin foam layer, comprises a resin foam having pores with a pore diameter of 20 μm or less and has a thickness of 50 to 250 μm,
and wherein a total thickness of the first resin foam layer and the second resin foam layer is 550 μm or less, and a international rubber hardness degree of the polishing pad measured by the M method according to JIS K6253 is 40 IRHD or more.

### Claim 2 (depends on 1)

The method for producing a glass substrate for a magnetic disk according to claim 1, wherein the second resin foam layer has a compressibility at 200 μm of 3% or less.

### Claim 3 (depends on 1)

The method for producing a glass substrate for a magnetic disk according to claim 1, wherein an open pore area ratio of the polishing surface is adjusted to 8% or more, and an average circle equivalent diameter of open pores of the polishing surface is adjusted to 10 μm or more, by the dressing treatment.

### Claim 4 (depends on 1)

The method for producing a glass substrate for a magnetic disk according to claim 1, wherein after a surface layer of the polishing pad is cut off by the dressing treatment, brush cleaning is performed while supplying pure water.

### Claim 5 (depends on 1)

A glass substrate for a magnetic disk produced by the method for producing a glass substrate for a magnetic disk according to claim 1.

### Claim 6 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the first resin foam layer and the second resin foam layer are joined through a joining solution.

### Claim 7 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the polishing material is a colloidal silica or a fumed silica.

### Claim 8 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the first resin foam layer comprises polyurethane.

### Claim 9 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the international rubber hardness degree of the polishing pad measured by the M method according to JIS K6253 is 50 IRHD or less.

### Claim 10 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the first resin foam layer has a thickness of 100 to 400 μm.

### Claim 11 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the second resin foam layer comprises polyethylene terephthalate.

### Claim 12 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the total thickness of the first resin foam layer and the second resin foam layer is 500 μm or less.

### Claim 13 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the first resin foam layer has a thickness of 350 μm or less.

### Claim 14 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the second resin foam layer has a thickness of 100 to 250 μm.

### Claim 15 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the international rubber hardness degree of the polishing pad measured by the M method according to JIS K6253 is 42 IRHD or more.

### Claim 16 (depends on 1)

The method for producing a glass substrate for magnetic disk according to claim 1, wherein the international rubber hardness degree of the polishing pad measured by the M method according to JIS K6253 is 46-49 IRHD.