# US 2012/0251743 A1 · Durable glass housings/enclosures for electronic devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251743 A1
- Document ID: US20120251743A1
- Status: Published application
- Kind: A1
- Application number: 13/471,505
- Filed: 2012-05-15
- Published: 2012-10-04
- Earliest claimed: 2008-08-21
- Inventors: Jaymin Amin; Matthew John Dejneka; Linda Ruth Pinckney; Katherine Rose Rossington; Robert Sabia
- Web page: https://patentgrep.com/patent/US20120251743A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- Y10T 428/131: Glass, ceramic, or sintered, fused, fired, or calcined metal oxide or metal carbide containing [e.g., porcelain, brick, cement, etc.]
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- Y10T 428/265: 1 mil or less
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A housing/enclosure/cover can include an ion-exchanged glass exhibiting the following attributes (1) radio, and microwave frequency transparency, as defined by a loss tangent of less than 0.03 and at a frequency range of between 15 MHz to 3.0 GHz; (2) infrared transparency; (3) a fracture toughness of greater than 0.6 MPa·m1/2; (4) a 4-point bend strength of greater than 350 MPa; (5) a Vickers hardness of at least 450 kgf/mm2 and a Vickers median/radial crack initiation threshold of at least 5 kgf; (6) a Young's Modulus ranging between about 50 to 100 GPa;; (7) a thermal conductivity of less than 2.0 W/m° C., and (9) and at least one of the following attributes: (i) a compressive surface layer having a depth of layer (DOL) greater and a compressive stress greater than 400 MPa, or, (ii) a central tension of more than 20 MPa.

## Claims

### Claim 1

An article suitable for housing, enclosing, or covering the components of a portable electronic device, the article comprising:
an ion exchanged glass exhibiting:
radio and microwave frequency transparency, as defined by a loss tangent of less than 0.03 and at a frequency range of between 15 MHz to 3.0 GHz;
infrared transparency;
a fracture toughness of greater than 0.60 MPa·m1/2;
a 4-point bend strength of greater than 350 MPa
a Vickers hardness of at least 450 kgf/mm2;
a Vickers median/radial crack initiation threshold of at least 5 kgf;
a Young's Modulus ranging between 50 to 100 GPa;
a thermal conductivity of less than 2.0 W/m° C.; and
at least one of the following attributes:
(i) a compressive surface layer having a depth of layer (DOL) greater than or equal to 20 μm and a compressive stress greater than 400 MPa; or
(ii) a central tension of more than 20 MPa.

### Claim 2 (depends on 1)

The article of claim 1, wherein the glass exhibits a refractive index of greater than 1.47 at 633 nm.

### Claim 3 (depends on 1)

The article of claim 1, wherein the glass exhibits radio and microwave frequency transparency, as defined by a loss tangent of less than 0.015 at a frequency range of between 500 MHz to 3.0 GHz.

### Claim 4 (depends on 1)

The article of claim 1, wherein the glass exhibits a fracture toughness of greater than 0.75 MPa·m1/2.

### Claim 5 (depends on 1)

The article of claim 1, wherein the glass exhibits a Young's Modulus ranging between 50 and 75 GPa.

### Claim 6 (depends on 1)

The article of claim 1, wherein the glass exhibits an 4-point bend strength of greater than 475 MPa.

### Claim 7 (depends on 1)

The article of claim 1, wherein the glass exhibits a Vickers hardness of at least 500 kgf/mm2 and Vickers median/radial crack initiation threshold of greater than 10 kgf.

### Claim 8 (depends on 1)

The article of claim 1, wherein the glass exhibits a thermal conductivity of less than 1.5 W/m° C.

### Claim 9 (depends on 1)

The article of claim 1, wherein the glass article is transparent and exhibits at least one surface having a Ra roughness of less than 50 nm.

### Claim 10 (depends on 1)

The article of claim 1, wherein the glass article appears opaque and exhibits at least one surface having a Ra roughness of between 50 nm and 15 μm.

### Claim 11 (depends on 1)

The article of claim 1, wherein the glass exhibits a near-infrared transparency of greater than 80% at a wavelength ranging from 750 to 2000 nm.

### Claim 12 (depends on 1)

The article of claim 1, wherein the article exhibits an overall thickness of 1.2 mm and compressive layer exhibiting a DOL of ranging between 40 to 80 μm and the compressive layer exhibits a compressive stress of 525 MPa.

### Claim 13 (depends on 1)

The article of claim 1, wherein the glass is an alkali-aluminosilicate glass.

### Claim 14 (depends on 13)

The article of claim 13, wherein the alkali-aluminosilicate glass comprises in mole percent as oxides on a batched basis: 40-80% SiO2, 0-28% Al2O3, 0-8% B2O3, 0-18% Li2O, 0-10% Na2O, 0-11% K2O, 0-16% MgO, 0-18% CaO, 0-15% CaF2, 0-20% SrO, 0-12% BaO, 0-8% ZnO, 0-4% P2O5, 0-8% TiO2, 0-5% ZrO2, 0-1% SnO2, 0-1% Sb2O3, and 0-1% As2O3.

### Claim 15 (depends on 13)

The article of claim 13, wherein the alkali-aluminosilicate glass comprises in mole percent as oxides on a batched basis: 60-70% SiO2; 6-14% Al2O3; 0-15% B2O3; 0-15% Li2O; 0-20% Na2O; 0-10% K2O; 0-8% MgO; 0-10% CaO; 0-5% ZrO2; 0-1% SnO2; 0-1% CeO2; less than 50 ppm As2O3; and less than 50 ppm Sb2O3; wherein 12 mol %≦Li2O+Na2O+K2O≦20 mol % and 0 mol %≦MgO+CaO≦10 mol %.

### Claim 16 (depends on 13)

The article of claim 13, wherein the alkali-aluminosilicate glass comprises in mole percent as oxides on a batched basis: 61-75% SiO2, 7-15% Al2O3, 0-12% B2O3, 9-21% Na2O, 0-4% K2O, 0-7% MgO, and 0-3% CaO.

### Claim 17 (depends on 13)

The article of claim 13, wherein the alkali-aluminosilicate glass comprises in mole percent as oxides on a batched basis: 60-72% SiO2; 9-16% Al2O3; 5-12% B2O3; 8-16% Na2O;
and 0-4% K2O; wherein
Al
2

O
3


(
mol


%
)
+
B
2

O


(
mol


%
)
∑

alkali


metal


modifiers


(
mol


%
)
>
1.

### Claim 18

An article suitable for housing, enclosing, or covering the components of a portable electronic device, the article comprising:
an ion exchanged alkali-aluminosilicate glass exhibiting:
radio and microwave frequency transparency, as defined by a loss tangent of less than 0.03 and at a frequency range of between 15 MHz to 3.0 GHz;
infrared transparency;
a fracture toughness of greater than 0.60 MPa·m1/2;
a 4-point bend strength of greater than 350 MPa;
a Vickers hardness of at least 450 kgf/mm2;
a Vickers median/radial crack initiation threshold of at least 5 kgf;
a Young's Modulus ranging between 50 to 100 GPa;
a thermal conductivity of less than 2.0 W/m° C.; and
at least one of the following attributes:
(i) a compressive surface layer having a depth of layer (DOL) greater than or equal to 20 μm and a compressive stress greater than 400 MPa; or
(ii) a central tension of more than 20 MPa;
wherein the ion exchanged alkali-aluminosilicate glass comprises in mole percent as oxides on a batched basis: 61-75% SiO2, 7-15% Al2O3, 0-12% B2O3, 9-21% Na2O, 0-4% K2O, 0-7% MgO, and 0-3% CaO; and
wherein the glass article is transparent and exhibits at least one surface having a Ra roughness of less than 50 nm.

### Claim 19

An article suitable for housing, enclosing, or covering the components of a portable electronic device, the article comprising:
an ion exchanged alkali-aluminosilicate glass exhibiting:
radio and microwave frequency transparency, as defined by a loss tangent of less than 0.03 and at a frequency range of between 15 MHz to 3.0 GHz;
infrared transparency;
a fracture toughness of greater than 0.60 MPa·m1/2;
a 4-point bend strength of greater than 350 MPa;
a Vickers hardness of at least 450 kgf/mm2;
a Vickers median/radial crack initiation threshold of at least 5 kgf;
a Young's Modulus ranging between 50 to 100 GPa;
a thermal conductivity of less than 2.0 W/m° C.; and
at least one of the following attributes:
(i) a compressive surface layer having a depth of layer (DOL) greater than or equal to 20 μm and a compressive stress greater than 400 MPa; or
(ii) a central tension of more than 20 MPa;
wherein the alkali-aluminosilicate glass comprises in mole percent as oxides on a batched basis: 60-72% SiO2; 9-16% Al203; 5-12% B2O3; 8-16% Na2O; and 0-4% K2O; wherein
Al
2

O
3


(
mol


%
)
+
B
2

O


(
mol


%
)
∑

alkali


metal


modifiers


(
mol


%
)
>
1
;
and
wherein the glass article is transparent and exhibits at least one surface having a Ra roughness of less than 50 nm.