# US 2012/0251741 A1 · Method for adjusting the coolant consumption within actively cooled components, and component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251741 A1
- Document ID: US20120251741A1
- Status: Published application
- Kind: A1
- Application number: 13/351,259
- Filed: 2012-01-17
- Published: 2012-10-04
- Earliest claimed: 2011-01-18
- Assignees: Siemens Aktiengesellschaft
- Inventors: Fathi AHMAD; Knut HALBERSTADT; Christian LERNER
- Web page: https://patentgrep.com/patent/US20120251741A1

## CPC

- C23C 16/045: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- C23C 10/02: Pretreatment of the material to be coated (C23C10/04 takes precedence)
- C23C 10/04: Diffusion into selected surface areas, e.g. using masks
- C23C 10/48: Aluminising
- C23C 10/60: After-treatment
- F01D 5/288: {Protective coatings for blades}
- Y02T 50/60: Efficient propulsion technologies, e.g. for aircraft
- Y10T 428/13: Hollow or container type article [e.g., tube, vase, etc.]
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F01D: NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES (machines or engines for liquids F03; non-positive displacement pumps F04D)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for adjusting the coolant consumption within actively cooled components is produced. The components include an interior with at least one duct with different regions which have different cross sections of flow. A greater increase in the wall thickness is produced in the region having the smaller cross section of flow by a first diffusion process and a lesser increase in the wall thickness is produced in the region having the larger cross section of flow by a second diffusion process which is different from the first. By using different diffusion coatings in a component, it is possible to adjust the flow of coolant through a component in a controlled way.

## Claims

### Claim 1

A method for adjusting the flow of a medium within a hollow component which in the interior includes a duct with different regions which include different cross sections of flow, comprising:
producing a greater increase in a first wall thickness in a first region having a smaller cross section of flow than a second region by a first diffusion coating process; and
producing a lesser increase in a second wall thickness in the second region having a larger cross section of flow by a second diffusion coating process, which is different from the first diffusion coating process.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein aluminizing processes are used for the diffusion coatings processes.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein two different coating materials are used for the diffusion coating processes.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein two different coating materials are used for the diffusion coating processes.

### Claim 5 (depends on 3)

The method as claimed in claim 3, wherein Ni2Al3 is used as an aluminum source for the first diffusion coating process.

### Claim 6 (depends on 3)

The method as claimed in claim 3, wherein which NiAl is used as an aluminum source for the second diffusion coating process.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the first and second diffusion processes are carried out in succession.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the first and second diffusion processes are carried out simultaneously.

### Claim 9 (depends on 1)

The method as claimed in claim 1,
wherein different coating materials are used for the diffusion coating processes, and
wherein a first coating material is applied on top of a second coating material.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the region which was alitized first is alitized again.

### Claim 11 (depends on 3)

The method as claimed in claim 3,
wherein the coating materials have different activation energies, and
wherein firstly a lower temperature is used for one coating material and then a higher temperature is used for the other coating material.

### Claim 12 (depends on 1)

A hollow component, comprising:
a plurality of regions with different alitized layer thicknesses in the interior of the component,
wherein the hollow component is alitized in the interior, and
wherein the hollow component is produced by the method as claimed in claim 1.

### Claim 13 (depends on 12)

The component as claimed in claim 12,
wherein a first region including a larger cross section of flow includes a smaller alitized layer thickness.

### Claim 14 (depends on 13)

The component as claimed in claim 13, wherein the smaller alitized layer thickness is between 20 μm to 60 μm.

### Claim 15 (depends on 12)

The component as claimed in claim 12,
wherein a second region having the smaller cross section of flow includes a larger alitized layer thickness.

### Claim 16 (depends on 15)

The component as claimed in claim 15, wherein the larger alitized layer thickness is between 60 μm to 120 μm.

### Claim 17 (depends on 15)

The component as claimed in claim 15, wherein the larger alitized layer thickness is between 80 μm to 100 μm.