# US 2012/0251739 A1 · Optical film, polarizer, and image display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251739 A1
- Document ID: US20120251739A1
- Status: Published application
- Kind: A1
- Application number: 13/427,473
- Filed: 2012-03-22
- Published: 2012-10-04
- Earliest claimed: 2011-03-31
- Assignees: FUJIFILM Corporation
- Inventors: Yumi KATO; Kazuo KAMOHARA; Mamoru SAKURAZAWA
- Web page: https://patentgrep.com/patent/US20120251739A1

## CPC

- G02B 1/04: made of organic materials, e.g. plastics (G02B1/08 takes precedence)
- G02B 1/14: Protective coatings, e.g. hard coatings
- C09K 2323/035: Ester polymer, e.g. polycarbonate, polyacrylate or polyester
- Y10T 428/265: 1 mil or less
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.

## Claims

### Claim 1

An optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.

### Claim 2 (depends on 1)

The optical film according to claim 1, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is from 4.0 GPa to 5.5 GPa.

### Claim 3 (depends on 1)

The optical film according to claim 1, wherein the ratio of the TD tensile elastic modulus to the MD tensile elastic modulus of the cellulose ester film is less than 1.4.

### Claim 4 (depends on 3)

The optical film according to claim 3, wherein the ratio of the TD tensile elastic modulus to the MD tensile elastic modulus of the cellulose ester film is from 0.9 to 1.2.

### Claim 5 (depends on 1)

The optical film according to claim 1, wherein the cellulose ester film comprises at least one sugar ester.

### Claim 6 (depends on 5)

The optical film according to claim 5, wherein the cellulose ester film comprises the sugar ester in an amount of from 2% by mass to less than 25% by mass relative to the cellulose ester.

### Claim 7 (depends on 5)

The optical film according to claim 5, wherein the sugar ester is a mixture of multiple sugar ester compounds that are the same in point of the type of the ester substituent therein but differ in point of the degree of ester substitution therein.

### Claim 8 (depends on 7)

The optical film according to claim 7, wherein the mean ester substitution ratio of the multiple sugar ester compounds differing in point of the degree of ester substitution therein is from 62 to 94%.

### Claim 9 (depends on 5)

The optical film according to claim 5, wherein the sugar ester is a mixture of a sugar ester substituted with an ester group having an aromatic ring-comprising group and a sugar ester substituted with an ester group having an aliphatic acyl group.

### Claim 10 (depends on 9)

The optical film according to claim 9, wherein the mean ester substitution ratio of the sugar esters substituted with an ester group having an aromatic ring-containing group is from 62% to 94%.

### Claim 11 (depends on 9)

The optical film according to claim 9, wherein the blend ratio of the sugar ester substituted with an ester group having an aromatic ring-containing group to the sugar ester substituted with an ester group having an aliphatic acyl group is at least ⅓.

### Claim 12 (depends on 1)

The optical film according to claim 1, wherein the cellulose ester film is a stretched film.

### Claim 13 (depends on 1)

The optical film according to claim 1, wherein the cellulose ester is a cellulose acetate.

### Claim 14 (depends on 1)

The optical film according to claim 1, wherein the cellulose ester has a degree of acetyl substitution of from 2.70 to 2.95.

### Claim 15 (depends on 1)

The optical film according to claim 1, wherein the cellulose ester has a degree of acetyl substitution of from 2.82 to 2.87.

### Claim 16 (depends on 1)

The optical film according to claim 1, wherein the hard coat layer is a polyfunctional (meth)acrylate-base hard coat layer.

### Claim 17 (depends on 16)

The optical film according to claim 16, wherein the hard coat layer comprises a polymer derived from at least two kinds of polyfunctional monomers having at least three (meth)acryloyl groups in one molecule.

### Claim 18

An image display device having an optical film on the display surface of the panel thereof, wherein the optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.

### Claim 19

A polarizer having a polarizing element and an optical film, wherein the optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.

### Claim 20

A liquid-crystal display device at least having a polarizer having a polarizing element and an optical film, wherein the optical film comprising a cellulose ester film and, as formed on at least one surface thereof, a hard coat layer having a thickness of from 0.1 to 6 μm, wherein the tensile elastic modulus of the cellulose ester film both in the machine direction (MD) thereof and in the direction transverse to the machine direction (TD) thereof is at least 4.0 GPa.