# US 2012/0251732 A1 · Process of Applying Water-based Rubber Copolyer to Textile

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251732 A1
- Document ID: US20120251732A1
- Status: Published application
- Kind: A1
- Application number: 13/074,075
- Filed: 2011-03-29
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Inventors: Ching-Ming Jwo; Chin-Jen Jwo; Shih-Shang Lo; Ying-Tasi Kao
- Web page: https://patentgrep.com/patent/US20120251732A1

## CPC

- D06N 3/0088: {by directly applying the resin (D06N3/0045 takes precedence)}
- D06M 15/693: with natural or synthetic rubber, or derivatives thereof
- D06N 3/10: with styrene-butadiene copolymerisation products {or other synthetic rubbers or elastomers except polyurethanes}
- D06N 3/106: {Elastomers}
- D06N 3/14: with polyurethanes
- D06N: WALL, FLOOR, OR LIKE COVERING MATERIALS, e.g. LINOLEUM, OILCLOTH, ARTIFICIAL LEATHER, ROOFING FELT, CONSISTING OF A FIBROUS WEB COATED WITH A LAYER OF MACROMOLECULAR MATERIAL; FLEXIBLE SHEET MATERIAL NOT OTHERWISE PROVIDED FOR
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

A process of making a textile comprising dropping a predetermined amount of rubber copolymer in a reactor filled with a solvent including 90-100 wt % of toluene, 0-10 wt % of acetone, and 0-10 wt % of ethanol; adjusting conditions of the reactor to a predetermined range of temperature and a predetermined atmospheric pressure so as to reduce sizes of molecules of the rubber copolymer; adding water to the reactor to disperse the rubber copolymer in the solvent to make an aqueous solution with dispersing rubber copolymer; and penetrating the water-based rubber copolymer through fibers of the textile for permanently attaching thereto.

## Claims

### Claim 1

A process of making a textile, comprising the steps of:
dropping a predetermined amount of rubber copolymer in a reactor filled with a solvent including 90-100 wt % of toluene, 0-10 wt % of acetone, and 0-10 wt % of ethanol;
adjusting conditions of the reactor to a predetermined range of temperature and a predetermined atmospheric pressure so as to reduce sizes of molecules of the rubber copolymer;
adding water to the reactor to disperse the rubber copolymer in the solvent to make an aqueous solution with dispersing rubber copolymer; and
penetrating the dispersing rubber copolymer through fibers of the textile for permanently attaching thereto.

### Claim 2 (depends on 1)

The process of claim 1, wherein the penetration comprises applying the solution to the textile so as to penetrate the dispersing rubber copolymer through the fibers of the textile for permanently attaching thereto.

### Claim 3 (depends on 1)

The process of claim 1, wherein the penetration comprises submerging the textile in the solution so as to penetrate the dispersing rubber copolymer through the fibers of the textile for permanently attaching thereto.

### Claim 4 (depends on 2)

The process of claim 2, wherein the application comprises applying the solution to the textile in a weight of 20-200 g/m2.

### Claim 5 (depends on 1)

The process of claim 1, further comprising adding thickening agents to the solution to increase viscosity of the solution.

### Claim 6 (depends on 5)

The process of claim 5, wherein the viscosity of the solution is 150-30,000 cps.

### Claim 7 (depends on 1)

The process of claim 1, wherein the predetermined range of temperature is between 10-100° C. and the predetermined atmospheric pressure is 1 atmospheric pressure.

### Claim 8 (depends on 1)

The process of claim 1, wherein the predetermined range of temperature is between 20-35° C.

### Claim 9 (depends on 1)

The process of claim 1, wherein the rubber copolymer is rubber emulsion copolymer.

### Claim 10 (depends on 1)

The process of claim 1, wherein the rubber copolymer is a rubber copolymer having a grain size of 5-40 μm.

### Claim 11 (depends on 1)

The process of claim 1, wherein the addition comprises adding water to the solution with a weight ratio of the solution and the water is 2 to 1 to make an aqueous solution with dispersing rubber copolymer.