# US 2012/0251727 A1 · Process for producing rigid open-cell foam

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251727 A1
- Document ID: US20120251727A1
- Status: Published application
- Kind: A1
- Application number: 13/526,162
- Filed: 2012-06-18
- Published: 2012-10-04
- Earliest claimed: 2009-12-18
- Assignees: Asahi Glass Company, Limited
- Inventors: Katsuhiko Shimizu; Hiroshi Wada; Yoshinori Toyota
- Web page: https://patentgrep.com/patent/US20120251727A1

## CPC

- C08G 18/482: {Mixtures of polyethers containing at least one polyether containing nitrogen}
- C08G 18/1825: {having hydroxy or primary amino groups}
- C08G 18/1833: {having ether, acetal, or orthoester groups}
- C08G 18/3206: {aliphatic}
- C08G 18/4816: {mixtures of two or more polyetherpolyols having at least three hydroxy groups}
- C08G 18/4829: {Polyethers containing at least three hydroxy groups (C08G18/4833 - C08G18/5096 take precedence)}
- C08G 18/4833: {Polyethers containing oxyethylene units}
- C08G 18/4837: {and other oxyalkylene units}
- C08G 18/4841: {containing oxyethylene end groups}
- C08G 18/5021: {having nitrogen}
- C08G 18/6674: {with compounds of group C08G18/3203}
- C08G 18/7664: {containing alkylene polyphenyl groups}
- C08G 2110/0025: rigid
- C08G 2110/005: < 50kg/m3
- C08G 2110/0083: prepared using water as the sole blowing agent
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

To provide a process capable of producing a light-weight rigid open-cell foam by a spraying method using mainly or solely water as a blowing agent, wherein a polyol system liquid is excellent in storage stability even when the blowing agent is used in a large amount, and the foam is excellent in dimensional stability without sagging and capable of forming a uniform thermal insulation layer having an excellent appearance for the purpose of constructing a whole constructions.

## Claims

### Claim 1

A process for producing a rigid open-cell foam, which comprises mixing and spraying onto a substrate, by a spraying method, a liquid component (X) which comprises a polyol (P), a blowing agent, a surfactant and a catalyst, and a liquid component (Y) which comprises a polyisocyanate compound, and subjecting the mixture on the substrate to foaming and a reaction for curing, wherein
the polyol (P) comprises the following polyols (A), (B) and (C), and based on the entire amount of the polyol (P), the content of the polyol (A) is from 45 to 80 mass %, the content of the polyol (B) is from 10 to 40 mass %, the content of the polyol (C) is from 5 to 30 mass %, and the total content of the polyols (A), (B) and (C) is from 90 to 100 mass %, and
as the blowing agent, water is used,
polyol (A): a polyol that has a hydroxy value of from 100 to 900 mgKOH/g, obtainable by ring-opening addition of an alkylene oxide to an initiator (S1) that contains no nitrogen atom and has from 2 to 8 functionality, or a polyhydric alcohol that contains no nitrogen atom and has from 2 to 8 functionality and a hydroxy value of from 100 to 900 mgKOH/g,
polyol (B): a polyol that has a hydroxy value of from 20 to 56 mgKOH/g and a terminal oxyethylene group content of from 5 to 15 mass %, obtainable by ring-opening addition of an alkylene oxide other than ethylene oxide, to an initiator (S2) that contains no nitrogen atom and has from 2 to 8 functionality, followed by ring-opening addition of ethylene oxide,
polyol (C): a polyol that has a hydroxy value of from 50 to 350 mgKOH/g, obtainable by ring-opening addition of ethylene oxide and an alkylene oxide other than ethylene oxide, to an initiator (S3) that contains nitrogen atom(s) and has from 3 to 5 functionality, wherein the amount of ethylene oxide based on the entire amount of the alkylene oxide is from 30 to 80 mass %.

### Claim 2 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the liquid components (X) and (Y) are mixed in such a ratio that the isocyanate index becomes from 20 to 100.

### Claim 3 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the liquid component (X) further contains a flame retardant.

### Claim 4 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the amount of the water is from 15 to 30 parts by mass per 100 parts by mass of the polyol (P).

### Claim 5 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein as the blowing agent, only water is used.

### Claim 6 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the initiator (S3) is a compound that contains at least two nitrogen atoms.

### Claim 7 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the initiator (S3) is an amine compound.

### Claim 8 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the polyol (C) is a polyol obtainable by ring-opening addition of ethylene oxide to the initiator (S3), followed by ring-opening addition of an alkylene oxide other than ethylene oxide.

### Claim 9 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the polyol (A) has an oxyethylene group content of from 0 to 5 mass %.

### Claim 10 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the alkylene oxide other than ethylene oxide to be used in the production of the polyols (A), (B) and (C) is propylene oxide for each polyol.

### Claim 11 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the closed-cell percentage of the rigid foam is at most 10%.

### Claim 12 (depends on 1)

The process for producing a rigid open-cell foam according to claim 1, wherein the substrate is a building or a building material.