# US 2012/0251713 A1 · Method for restoring antimicrobial hydrophilic coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251713 A1
- Document ID: US20120251713A1
- Status: Published application
- Kind: A1
- Application number: 13/074,612
- Filed: 2011-03-29
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Assignees: Hamilton Sundstrand Space Systems International, Inc.
- Inventors: Peter W. Keilich; Mark E. Caron
- Web page: https://patentgrep.com/patent/US20120251713A1

## CPC

- C09D 5/14: Paints containing biocides, e.g. fungicides, insecticides or pesticides (C09D5/16 takes precedence)
- B01D 53/261: {by adsorption}
- B01D 2259/4575: in aeroplanes or space ships
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

A method for restoring a silver oxide-containing hydrophilic coating includes heating the coating to a temperature between about 260° C. and about 540° C. and maintaining the coating at a temperature between about 260° C. and about 540° C. in an environment containing oxygen and ozone for less than 24 hours.

## Claims

### Claim 1

A method for restoring a silver oxide-containing hydrophilic coating, the method comprising:
heating the coating to a temperature between about 260° C. and about 540° C.; and
maintaining the coating at a temperature between about 260° C. and about 540° C. in an environment containing oxygen and ozone for less than 24 hours.

### Claim 2 (depends on 1)

The method of claim 1, wherein the coating is heated to a temperature between about 370° C. and about 510° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the coating is exposed to an environment consisting of oxygen and ozone when the coating is heated to a temperature above about 370° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the coating is maintained at a temperature between about 260° C. and about 540° C. for between about 1 hour and about 4 hours.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step of maintaining the coating at a temperature between about 260° C. and about 540° C. in the environment containing oxygen and ozone comprises:
maintaining the coating at a first temperature between about 260° C. and about 540° C. for between about 1 hour and about 4 hours;
reducing the temperature of the coating to a second temperature lower than the first temperature; and
maintaining the coating at the second temperature for between about 15 minutes and about 4 hours.

### Claim 6 (depends on 1)

The method of claim 1, wherein the environment contains ozone at a concentration equal to or greater than a stoichiometric amount for the following reaction:
2Ag+O3→Ag2O+O2.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
cooling the component to ambient temperature; and
eliminating exposure of the coating to ozone once the coating is at a temperature below about 150° C.

### Claim 8 (depends on 7)

The method of claim 7, wherein exposure of the coating to ozone is eliminated once the coating is at a temperature below about 200° C.

### Claim 9

A method for preparing a component having a silver oxide-containing hydrophilic coating, the method comprising:
heating the component to a first temperature between about 370° C. and about 540° C.;
maintaining the component at the first temperature for between about 1 hour and about 4 hours in an environment containing oxygen and ozone to eliminate contaminants from the coating;
reducing the temperature of the component to a second temperature between about 260° C. and about 510° C.; and
maintaining the component at the second temperature for between about 15 minutes and about 4 hours in the environment containing oxygen and ozone.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first temperature is between about 400° C. and about 510° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein the second temperature is between about 370° C. and about 425° C.

### Claim 12 (depends on 9)

The method of claim 9, wherein the coating is exposed to an environment consisting of oxygen and ozone while the component is at a temperature above about 370° C.

### Claim 13 (depends on 9)

The method of claim 9, further comprising:
reducing the temperature of the component after maintaining the component at the second temperature, wherein the coating is exposed to an environment consisting of oxygen once the component is at a temperature below about 200° C.

### Claim 14 (depends on 9)

The method of claim 9, wherein the environment contains ozone at a concentration equal to or greater than a stoichiometric amount for the following reaction:
2Ag+O3→Ag2O+O2.

### Claim 15

A method for restoring a condensing heat exchanger having an antimicrobial hydrophilic coating, the method comprising:
heating the heat exchanger to a first temperature between about 370° C. and about 540° C.;
maintaining the heat exchanger at the first temperature for less than about 24 hours in an environment containing oxygen and ozone to eliminate contaminants from the coating;
reducing the temperature of the heat exchanger to a second temperature between about 260° C. and about 510° C.; and
maintaining the heat exchanger at the second temperature for between about 15 minutes and about 4 hours in the environment containing oxygen and ozone to reform silver oxide.

### Claim 16 (depends on 15)

The method of claim 15, wherein the first temperature is between about 400° C. and about 510° C.

### Claim 17 (depends on 15)

The method of claim 15, wherein the second temperature is between about 370° C. and about 425° C.

### Claim 18 (depends on 15)

The method of claim 15, wherein the coating is exposed to an environment consisting of oxygen and ozone while the component is at a temperature above about 370° C.

### Claim 19 (depends on 15)

The method of claim 15, further comprising:
reducing the temperature of the component after maintaining the component at the second temperature, wherein the coating is exposed to an environment consisting of oxygen once the component is at a temperature below about 200° C.

### Claim 20 (depends on 15)

The method of claim 15, wherein the environment contains ozone at a concentration equal to or greater than a stoichiometric amount for the following reaction:
2Ag+O3→Ag2O+O2.