# US 2012/0251706 A1 · Method of manufacturing an anti-fingerprint paint and use of the anti-fingerprint paint

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251706 A1
- Document ID: US20120251706A1
- Status: Published application
- Kind: A1
- Application number: 13/074,000
- Filed: 2011-03-28
- Published: 2012-10-04
- Earliest claimed: 2011-03-28
- Inventors: Chih-Hao Huang
- Web page: https://patentgrep.com/patent/US20120251706A1

## CPC

- B05D 5/083: {involving the use of fluoropolymers}
- B05D 1/18: performed by dipping
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B05D 3/0236: {with ovens (B05D3/0227 takes precedence)}
- B05D 3/0413: {Heating with air}
- B05D 2202/00: Metallic substrate
- C08K 3/04: Carbon
- C08K 3/22: of metals
- C08K 2201/011: Nanostructured additives
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A method of manufacturing the anti-fingerprint paint is described hereinafter. Firstly, blend fluorinated polymer with fluorocarbon solvents to form fluorocarbon polymer paint. Secondly, blend nano-particles with the fluorocarbon solvents, then add the fluorine-couplant into the fluorocarbon solvents with the nano-particles therein, and further mix up the above-mentioned solvents to get a nano-particle solvent. Lastly, blend the fluorocarbon polymer paint with the nano-particle solvents and further mix up the mixture of the fluorocarbon polymer paint and the nano-particle solvents under a room temperature for 12 to 24 hours to form the anti-fingerprint paint. The method of forming the anti-fingerprint coating onto the surface of the substrate is described hereinafter. Firstly, coat the anti-fingerprint paint onto a surface of the substrate. Secondly, heat the anti-fingerprint paint coated on the surface of the substrate to form the anti-fingerprint coating on the surface of the substrate.

## Claims

### Claim 1

A method of manufacturing an anti-fingerprint paint, comprising the steps of:
blending fluorinated polymer with fluorocarbon solvents to form fluorocarbon polymer paint;
blending nano-particles with the fluorocarbon solvents, then adding fluorine-couplant into the fluorocarbon solvents with the nano-particles therein, and further mixing up the above-mentioned solvents to get a nano-particle solvent with an outside surface of each of the nano-particles dressed up by a layer of fluorinated molecules; and
blending the fluorocarbon polymer paint with the nano-particle solvents, and further mixing up the mixture of the fluorocarbon polymer paint and the nano-particle solvents under a room temperature for 12 to 24 hours to form the anti-fingerprint paint.

### Claim 2 (depends on 1)

The method of manufacturing the anti-fingerprint paint as claimed in claim 1, wherein the nano-particle has a diameter of 5 to 20 nanometers.

### Claim 3 (depends on 1)

The method of manufacturing the anti-fingerprint paint as claimed in claim 1, wherein the nano-particle is a metallic oxide.

### Claim 4 (depends on 1)

The method of manufacturing the anti-fingerprint paint as claimed in claim 1, wherein the nano-particle is a metal.

### Claim 5 (depends on 1)

The method of manufacturing the anti-fingerprint paint as claimed in claim 1, wherein the nano-particle is a polymer material.

### Claim 6 (depends on 1)

The method of manufacturing the anti-fingerprint paint as claimed in claim 1, wherein the nano-particle is a carbon capsule.

### Claim 7 (depends on 1)

A method of forming an anti-fingerprint coating onto a surface of a substrate, comprising the steps of:
coating the anti-fingerprint paint of claim 1 onto the surface of the substrate; and
heating the anti-fingerprint paint coated on the surface of the substrate under 80 to 120 centigrade degrees for 0.5 to 2 hours, or air drying the anti-fingerprint paint coated on the surface of the substrate for 24 to 48 hours, to make a functional base of fluorine-couplant in the anti-fingerprinted paint and a surface material of the substrate realize a chemical bonding so as to form the anti-fingerprint coating on the surface of the substrate.

### Claim 8 (depends on 7)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 7, wherein the anti-fingerprint coating contains nano-particles dressed up by fluorinated molecules and the fluorine-couplant.

### Claim 9 (depends on 8)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 8, wherein the nano-particle has a diameter of 5 to 20 nanometers.

### Claim 10 (depends on 8)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 8, wherein the nano-particle is a metallic oxide, a metal, a polymer material or a carbon capsule.

### Claim 11 (depends on 7)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 7, wherein the anti-fingerprint paint is coated on the surface of the substrate by means of dipping.

### Claim 12 (depends on 7)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 7, wherein the substrate is made of glass, metal, ceramic material or polymer.

### Claim 13 (depends on 7)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 7, wherein the substrate is a shell or a touching screen of an electronic apparatus.

### Claim 14 (depends on 7)

The method of forming the anti-fingerprint coating onto the surface of the substrate as claimed in claim 7, wherein the anti-fingerprint coating has a thickness of 10 nm to 50 nm.