# US 2012/0251626 A1 · Process for manufacturing biocompatible material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251626 A1
- Document ID: US20120251626A1
- Status: Published application
- Kind: A1
- Application number: 13/447,832
- Filed: 2012-04-16
- Published: 2012-10-04
- Earliest claimed: 2007-10-26
- Assignees: RBS Co., Ltd.
- Inventors: Yoshiaki Okada
- Web page: https://patentgrep.com/patent/US20120251626A1

## CPC

- A61K 38/39: Connective tissue peptides, e.g. collagen, elastin, laminin, fibronectin, vitronectin, cold insoluble globulin [CIG]
- A61K 33/42: Phosphorus; Compounds thereof
- A61P 3/02: Nutrients, e.g. vitamins, minerals
- A61P 3/14: for calcium homeostasis (vitamin D A61P3/02; parathyroid hormones A61P5/18; calcitonin A61P5/22; osteoporosis A61P19/10; bone metastasis A61P35/04)
- A61P 19/00: Drugs for skeletal disorders
- A61P 19/08: for bone diseases, e.g. rachitism, Paget's disease
- A61P 19/10: for osteoporosis
- A61K: PREPARATIONS FOR MEDICAL, DENTAL OR TOILETRY PURPOSES (devices or methods specially adapted for bringing pharmaceutical products into particular physical or administering forms A61J3/00; chemical aspects of, or use of materials for deodorisation of air, for disinfection or sterilisation, or for bandages, dressings, absorbent pads or surgical articles A61L; soap compositions C11D)
- A61P: SPECIFIC THERAPEUTIC ACTIVITY OF CHEMICAL COMPOUNDS OR MEDICINAL PREPARATIONS

## Abstract

A process for producing a biocompatible material includes the steps of mixing an extract of a fish scale-derived hydroxyapatite (with water content of 70 to 75% by weight) and of a fish scale-derived collagen (with water content of 40 to 60% by weight) in the weight percent ratio of about 8:2, stirring the mixture and drying the mixture by a hot blast in order to obtain a composite.

## Claims

### Claim 1

A process for producing a biocompatible material, comprising the steps of: mixing an extract of a fish scale-derived hydroxyapatite with water content of 70 to 75% by weight and an extract of a fish scale-derived collagen with water content of 40 to 60% by weight, in a weight percent ratio of about 8:2 to form a mixture; stirring the mixture; and drying the mixture using a hot blast in order to obtain a composite.

### Claim 2 (depends on 1)

The process for producing the biocompatible material according to claim 1, wherein a production of the composite is incorporated in a process for producing the fish scale-derived hydroxyapatite.

### Claim 3 (depends on 1)