# US 2012/0251431 A1 · Method for producing nitride crystal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251431 A1
- Document ID: US20120251431A1
- Status: Published application
- Kind: A1
- Application number: 13/427,058
- Filed: 2012-03-22
- Published: 2012-10-04
- Earliest claimed: 2011-03-22
- Assignees: Mitsubishi Chemical Corporation
- Inventors: Hideo FUJISAWA; Yutaka Mikawa; Kazunori Kamada
- Web page: https://patentgrep.com/patent/US20120251431A1

## CPC

- C30B 7/10: by application of pressure, e.g. hydrothermal processes
- C30B 7/105: {using ammonia as solvent, i.e. ammonothermal processes}
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 29/403: {AIII-nitrides}
- C30B 29/406: {Gallium nitride}
- Y02P 20/54: using solvents, e.g. supercritical solvents or ionic liquids
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing a nitride crystal, comprising growing a nitride crystal on the surface of a seed crystal put in a reactor while the temperature and the pressure inside the reactor that contains, as put thereinto, a seed crystal having a hexagonal-system crystal structure, a nitrogen-containing solvent, a starting material, and a mineralizing agent containing fluorine and at least one halogen element selected from chlorine, bromine and iodine are so controlled that the solvent therein could be in a supercritical state and/or a subcritical state to thereby grow a nitride crystal on the surface of the seed crystal in the reactor.

## Claims

### Claim 1

A method for producing a nitride crystal, comprising growing a nitride crystal on the surface of a seed crystal put in a reactor while the temperature and the pressure inside the reactor that contains, as put thereinto, a seed crystal having a hexagonal-system crystal structure, a nitrogen-containing solvent, a starting material, and a mineralizing agent containing fluorine and at least one halogen element selected from chlorine, bromine and iodine are so controlled that the solvent therein could be in a supercritical state and/or a subcritical state to thereby grow a nitride crystal on the surface of the seed crystal in the reactor.

### Claim 2 (depends on 1)

The method for producing a nitride crystal of claim 1, wherein the mineralizing agent contains chlorine and fluorine.

### Claim 3 (depends on 2)

The method for producing a nitride crystal of claim 2, wherein the chlorine concentration in the mineralizing agent is from 1 to 200 molar times the fluorine concentration therein.

### Claim 4 (depends on 1, 2, 3)

The method for producing a nitride crystal of any one of claims 1 to 3, wherein the mineralizing agent contains bromine and fluorine.

### Claim 5 (depends on 4)

The method for producing a nitride crystal of claim 4, wherein the bromine concentration in the mineralizing agent is from 0.1 to 100 molar times the fluorine concentration therein.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The method for producing a nitride crystal of any one of claims 1 to 5, wherein the mineralizing agent contains iodine and fluorine.

### Claim 7 (depends on 6)

The method for producing a nitride crystal of claim 6, wherein the iodine concentration in the mineralizing agent is from 0.1 to 100 molar times the fluorine concentration therein.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

The method for producing a nitride crystal of any one of claims 1 to 7, wherein the total molar amount of the halogen elements contained in the mineralizing agent is from 0.1 to 30 mol % of the molar amount of the nitrogen-containing solvent.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The method for producing a nitride crystal of any one of claims 1 to 8, wherein the temperature of the region in which the starting material is melted inside the reactor is higher than the temperature of the region in which the nitride crystal is grown on the surface of the seed crystal.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

The method for producing a nitride crystal of any one of claims 1 to 9, wherein the temperature inside the reactor in the growing of the nitride crystal is from 500 to 650° C.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The method for producing a nitride crystal of any one of claims 1 to 10, wherein the pressure under which the nitride crystal is grown is from 120 to 350 MPa.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

The method for producing a nitride crystal of any one of claims 1 to 11, wherein the nitride crystal is a crystal of a nitride of a Group 13 metal in the Periodic Table.

### Claim 13 (depends on 12)

The method for producing a nitride crystal of claim 12, wherein the growth rate of the M-plane is at least 3 times the growth rate of the Periodic Table Group 13 metal plane.

### Claim 14 (depends on 12, 13)

The method for producing a nitride crystal of claim 12 or 13, wherein the growth rate of the M-plane is at least 0.4 times the growth rate of the C-plane.

### Claim 15 (depends on 12, 13, 14)

The method for producing a nitride crystal of any one of claims 12 to 14, wherein the growth rate of the A-plane is at least 0.6 times the growth rate of the C-plane.

### Claim 16 (depends on 12, 13, 14)

The method for producing a nitride crystal of any one of claims 12 to 14, wherein the growth rate of the A-plane is at least 1.5 times the growth rate of the C-plane.

### Claim 17 (depends on 12, 13, 14, 15, 16)

The method for producing a nitride crystal of any one of claims 12 to 16, wherein the growth rate of the Periodic Table Group 13 metal plane is from 10 to 150 μm/day.

### Claim 18 (depends on 12, 13, 14, 15, 16, 17)

The method for producing a nitride crystal of any one of claims 12 to 17, wherein the growth rate of the M-plane is from 100 to 500 μm/day.

### Claim 19 (depends on 12, 13, 14, 15, 16, 17, 18)

The method for producing a nitride crystal of any one of claims 12 to 18, wherein the growth rate of the A-plane is from 100 to 2500 μm/day.

### Claim 20 (depends on 12, 13, 14, 15, 16, 17, 18, 19)

The method for producing a nitride crystal of any one of claims 12 to 19, wherein the growth rate of the N-plane is from 100 to 1000 μm/day.

### Claim 21 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20)

A nitride crystal produced according to the production method of any one of claims 1 to 20.

### Claim 22 (depends on 21)

The nitride crystal of claim 21, wherein the fluorine concentration is from 5×1015 to 1×1018 atoms/cm−3.

### Claim 23 (depends on 21, 22)

The nitride crystal of claim 21 or 22, wherein the total concentration of chlorine, bromine and iodine is at most 1×1018 atoms/cm−3.

### Claim 24 (depends on 21, 22, 23)

The nitride crystal of any one of claims 21 to 23, which is a Periodic Table Group 13 metal nitride crystal.

### Claim 25 (depends on 24)

The nitride crystal of claim 24, wherein the major plane is the C-plane and the X-ray diffractiometry half-value width in reflection on the (0002) plane is at most 150 arcsec.

### Claim 26 (depends on 24)

The nitride crystal of claim 24, wherein the major plane is the M-plane and the X-ray diffractiometry half-value width in reflection on the (10-10) plane is at most 150 arcsec.