# US 2012/0251426 A1 · Polycrystalline Silicon For Solar Cell And Preparation Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251426 A1
- Document ID: US20120251426A1
- Status: Published application
- Kind: A1
- Application number: 13/515,426
- Filed: 2010-10-20
- Published: 2012-10-04
- Earliest claimed: 2009-12-14
- Assignees: JX Nippon Mining & Metals Corporation; Jnc Corporation; Toho Titanium Co., Ltd.
- Inventors: Kenji Sato
- Web page: https://patentgrep.com/patent/US20120251426A1

## CPC

- B22D 25/02: by its peculiarity of shape; of works of art {(cylinders, pistons B22D15/02)}
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

The present invention provides a process for preparing a polycrystalline silicon having the surface layer in which the areas having a short carrier lifetime due to Fe has been substantially eliminated. A preparation method of polycrystalline silicon comprising preparing a mold evenly applied with a mold release agent produced by mixing a binder and a solvent with a silicon nitride powder and then solidifying a molten silicon in said mold, wherein x≦5.0, 20≦y≦100 and x×y≦100 are satisfied given that x represents a concentration of Fe (atomic ppm) contained as impurity in the silicon nitride powder and y represents a thickness of the mold release agent (μm) applied to the mold.

## Claims

### Claim 1

A preparation method of a polycrystalline silicon comprising preparing a mold applied with a mold release agent produced by mixing a binder and a solvent with a silicon nitride powder and then solidifying a molten silicon in said mold, wherein x≦5.0, 20≦y≦100 and x×y≦100 are satisfied given that x represents a concentration of Fe (atomic ppm) contained as impurity in the silicon nitride powder and y represents a thickness of the mold release agent (μm) applied to the mold.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein the concentration of Fe in the silicon nitride powder has been reduced through a process in which hydrochloric acid or aqua regia is contacted with the silicon nitride powder, said process being performed in ultrasonic waves and/or in a grinder using grinding medium made of other than Fe.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein x≦1.0.

### Claim 4 (depends on 1)

The preparation method according to any one of claims 1, wherein 30≦y≦80.

### Claim 5 (depends on 1)

The preparation method according to any one of claims 1, wherein x×y≦30.

### Claim 6 (depends on 2)

The preparation method according to any one of claims 2, wherein the temperature of hydrochloric acid or aqua regia is 60-100° C.

### Claim 7

A polycrystalline silicon having a carrier lifetime of 5 μsec or more at a crystal surface contacted with a mold release agent.