# US 2012/0251416 A1 · Process for recycling of tungsten carbide alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251416 A1
- Document ID: US20120251416A1
- Status: Published application
- Kind: A1
- Application number: 13/516,458
- Filed: 2010-12-07
- Published: 2012-10-04
- Earliest claimed: 2010-01-08
- Inventors: Jayakannan Arumugavelu
- Web page: https://patentgrep.com/patent/US20120251416A1

## CPC

- C22B 7/001: {Dry processes}
- C01B 32/949: Tungsten or molybdenum carbides
- C22B 34/36: Obtaining tungsten
- C22C 29/08: based on tungsten carbide
- B22F 2009/001: {from scrap particles}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure is a process for the recycling of tungsten carbide alloy. Tungsten carbide alloy scrap is heated in an oxidizing atmosphere and the oxidized material is pulverized by grinding. The powder material is treated with a carburizing mixture for reducing and carburizing the powdered tungsten oxides and other metal oxides. The method is cost effective and environment friendly.

## Claims

### Claim 1

A process for the recycling of tungsten carbide alloy comprising acts of:
a) oxidizing the tungsten carbide alloy to obtain tungsten oxides and other metallic oxides;
b) grinding the tungsten oxides and other metallic oxides to obtain a powder; and
c) treating the powder with a carburizing mixture for reducing and carburizing the powdered tungsten oxides and other metallic oxides to obtain the purified tungsten carbide alloy powder.

### Claim 2 (depends on 1)

The process as claimed in claim 1, wherein the oxidation is carried out in an oxidation furnace at a temperature ranging from about 400° C. to about 1000° C., preferably at about 950° C.

### Claim 3 (depends on 1)

The process as claimed in claim 1, wherein the oxidation is carried out using oxidizing agent selected from a group comprising air and oxygen, preferably air.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the grinding is carried out by a method selected from a group comprising ball mill, Attritor Mill, High Speed Intensive mill; preferably ball mill.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein the grinding is carried out for a period ranging from about 0.5 h to about 10 h, preferably for about 2 h.

### Claim 6 (depends on 1)

The process as claimed in claim 1, wherein the carburizing mixture is selected from a group comprising air, hydrogen, nitrogen, carbon monoxide, methane, carbon dioxide, compressed natural gas (CNG), liquefied petroleum gas (LPG) and mixtures thereof.

### Claim 7 (depends on 6)

The process as claimed in claim 6, wherein the carburizing mixture is a combination of about 10% liquefied petroleum gas and about 90% nitrogen.

### Claim 8 (depends on 1)

The process as claimed in claim 1, wherein the treatment with the carburizing mixture is carried out for a period ranging from about 1 h to about 15 h, preferably 3 h.

### Claim 9 (depends on 8)

The process as claimed in claim 8, wherein the treatment with the carburizing mixture to obtain the purified tungsten carbide alloy powder is carried out in a reduction furnace at a temperature ranging from about 800° C. to about 1400° C., preferably at about 1050° C.

### Claim 10 (depends on 9)

The process as claimed in claim 9, wherein the purified tungsten carbide alloy powder is cooled to a temperature ranging from about 300° C. to about 200° C. preferably about 200° C. in nitrogen, and then to about 40° C. to about 20° C., preferably about 25° C. in air.