# US 2012/0251381 A1 · Articles containing copper nanoparticles and methods for production and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251381 A1
- Document ID: US20120251381A1
- Status: Published application
- Kind: A1
- Application number: 13/079,757
- Filed: 2011-04-04
- Published: 2012-10-04
- Earliest claimed: 2011-04-04
- Assignees: Lockheed Martin Corporation
- Inventors: Peter V. Bedworth; Alfred A. Zinn
- Web page: https://patentgrep.com/patent/US20120251381A1

## CPC

- C09K 5/14: Solid materials, e.g. powdery or granular
- B22F 1/054: Nanosized particles
- B22F 3/02: Compacting only
- B22F 3/20: by extruding
- C09K 5/00: Heat-transfer, heat-exchange or heat-storage materials, e.g. refrigerants; Materials for the production of heat or cold by chemical reactions other than by combustion
- C22C 9/00: Alloys based on copper
- H01B 1/16: the conductive material comprising metals or alloys
- H01B 1/22: the conductive material comprising metals or alloys
- H10W 72/30: Die-attach connectors
- H10W 72/07331: {Connecting techniques}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Articles containing a matrix material and plurality of copper nanoparticles in the matrix material that have been at least partially fused together are described. The copper nanoparticles are less than about 20 nm in size. Copper nanoparticles of this size become fused together at temperatures and pressures that are much lower than that of bulk copper. In general, the fusion temperatures decrease with increasing applied pressure and lowering of the size of the copper nanoparticles. The size of the copper nanoparticles can be varied by adjusting reaction conditions including, for example, surfactant systems, addition rates, and temperatures. Copper nanoparticles that have been at least partially fused together can form a thermally conductive percolation pathway in the matrix material.

## Claims

### Claim 1

An article comprising:
a matrix material; and
a plurality of copper nanoparticles in the matrix material that have been at least partially fused together;
wherein the plurality of copper nanoparticles are less than about 20 nm in size.

### Claim 2 (depends on 1)

The article of claim 1, wherein the plurality of copper nanoparticles further comprise a surfactant system.

### Claim 3 (depends on 2)

The article of claim 2, wherein the surfactant system comprises a bidentate diamine and one or more C6-C18 alkylamines.

### Claim 4 (depends on 1)

The article of claim 1, wherein the plurality of copper nanoparticles range between about 1 nm and about 10 nm in size.

### Claim 5 (depends on 1)

The article of claim 1, wherein the plurality of copper nanoparticles range between about 1 nm and about 5 nm in size.

### Claim 6 (depends on 1)

The article of claim 1, wherein the plurality of copper nanoparticles become at least partially fused together in the matrix material by applying at least one of heat or pressure to the article.

### Claim 7 (depends on 6)

The article of claim 6, wherein the article is heated at a temperature of at most about 200° C. to at least partially fuse the plurality of copper nanoparticles together.

### Claim 8 (depends on 6)

The article of claim 6, wherein the article is heated at a temperature of at most about 100° C. to at least partially fuse the plurality of copper nanoparticles together.

### Claim 9 (depends on 1)

The article of claim 1, further comprising:
a filler material.

### Claim 10 (depends on 9)

The article of claim 9, wherein the filler material is selected from the group consisting of flame retardants, UV protective agents, antioxidants, graphite, graphite oxide, graphene, carbon nanotubes, fiber materials, ceramic materials, and combinations thereof.

### Claim 11 (depends on 1)

The article of claim 1, wherein the article comprises about 10% to about 99.9% copper nanoparticles.

### Claim 12 (depends on 1)

The article of claim 1, wherein the plurality of copper nanoparticles comprise a thermally conductive percolation pathway in the matrix material.

### Claim 13 (depends on 1)

The article of claim 1, wherein the article has a thermal conductivity ranging between about 50 watts/m·K and about 400 watts/m·K.

### Claim 14 (depends on 1)

The article of claim 1, wherein the matrix material is selected from the group consisting of a polymer matrix, a rubber matrix, a glass matrix, a ceramic matrix and a metal matrix.

### Claim 15

A method comprising:
providing a plurality of copper nanoparticles;
wherein the plurality of copper nanoparticles are less than about 20 nm in size;
mixing the plurality of copper nanoparticles with a matrix material; and
applying at least one of heat or pressure to at least partially fuse the plurality of copper nanoparticles together.

### Claim 16 (depends on 15)

The method of claim 15, wherein the plurality of copper nanoparticles further comprise a surfactant system.

### Claim 17 (depends on 16)

The method of claim 16, wherein the surfactant system comprises a bidentate diamine and one or more C6-C18 alkylamines.

### Claim 18 (depends on 15)

The method of claim 15, wherein the plurality of copper nanoparticles range between about 1 nm and about 10 nm in size.

### Claim 19 (depends on 15)

The method of claim 15, wherein the plurality of copper nanoparticles range between about 1 nm and about 5 nm in size.

### Claim 20 (depends on 15)

The method of claim 15, further comprising:
curing the matrix material.

### Claim 21 (depends on 15)

The method of claim 15, wherein the plurality of copper nanoparticles are at least partially fused together by heating at a temperature of at most about 200° C.

### Claim 22 (depends on 15)

The method of claim 15, wherein the plurality of copper nanoparticles are at least partially fused together by heating at a temperature of at most about 100° C.

### Claim 23 (depends on 15)

The method of claim 15, further comprising:
removing the matrix material to leave behind a network of at least partially fused copper nanoparticles.

### Claim 24 (depends on 15)

The method of claim 15, wherein applying pressure comprises extruding the mixture of copper nanoparticles and the matrix material.

### Claim 25 (depends on 15)

The method of claim 15, wherein the matrix material is selected from the group consisting of a polymer matrix, a rubber matrix, a glass matrix, a ceramic matrix and a metal matrix.

### Claim 26

A method comprising:
providing an article comprising:
a matrix material; and
a plurality of copper nanoparticles that have been at least partially fused together in the matrix material;
wherein the plurality of copper nanoparticles are less than about 20 nm in size; and
placing the article in thermal contact with a heat source.

### Claim 27 (depends on 26)

The method of claim 26, further comprising:
placing the article in thermal contact with a heat sink.

### Claim 28 (depends on 26)

The method of claim 26, wherein the plurality of copper nanoparticles further comprise a surfactant system comprising a bidentate diamine and one or more C6-C18 alkylamines.

### Claim 29 (depends on 26)

The method of claim 26, wherein the plurality of copper nanoparticles comprise a thermally conductive percolation pathway in the matrix material.

### Claim 30 (depends on 26)

The method of claim 26, wherein the article has a thermal conductivity ranging between about 50 watts/m·K and about 400 watts/m·K.

### Claim 31

A composition comprising:
a plurality of copper nanoparticles that are less than about 20 nm in size that further comprise a surfactant system comprising a bidentate diamine and one or more C6-C18 alkylamines; and
a matrix material selected from the group consisting of a polymer matrix, a rubber matrix, a ceramic matrix, a metal matrix, and a glass matrix.

### Claim 32

A method comprising:
providing a plurality of copper nanoparticles that are mixed with a matrix material to form a paste;
wherein the plurality of copper nanoparticles are less than about 20 nm in size and further comprise a surfactant system comprising a bidentate diamine and one or more C6-C18 alkylamines;
placing the paste in a joint between a first member and a second member; and
joining the first member to the second member by at least partially fusing the plurality of copper nanoparticles together.

### Claim 33 (depends on 32)

The method of claim 32, wherein the plurality of copper nanoparticles are sufficiently porous to allow for rework of the joint after being at least partially fused together.

### Claim 34 (depends on 33)

The method of claim 33, wherein the plurality of copper nanoparticles are up to about 25% porous after being at least partially fused together.

### Claim 35 (depends on 32)