# US 2012/0251377 A1 · Method for enhancing strength and hardness of powder metallurgy stainless steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251377 A1
- Document ID: US20120251377A1
- Status: Published application
- Kind: A1
- Application number: 13/074,652
- Filed: 2011-03-29
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Inventors: Kuen-Shyang Hwang; Li-Hui Cheng; Yung-Chung Lu
- Web page: https://patentgrep.com/patent/US20120251377A1

## CPC

- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 3/16: in successive or repeated steps
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/44: with molybdenum or tungsten
- C22C 38/48: with niobium or tantalum
- C22C 38/58: with more than 1.5% by weight of manganese
- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/22: of ferrous surfaces
- B22F 2201/30: Carburising atmosphere
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method for enhancing strength and hardness of powder metallurgy stainless steels comprises steps of fabricating a stainless steel powder into a green compact; placing the green compact in a reducing environment and maintaining the green compact at a sintering temperature to form a sintered body; and placing the sintered body in a carbon-bearing atmosphere and maintaining the sintered body at a carburizing temperature below 600° C. to implant carbon atoms into the sintered body and form carburized regions in the sintered body. Thereby, the strength and hardness of powder metallurgy stainless steels can be improved. As the carburizing temperature is lower than 600° C., chromium would not react with carbon. Therefore, the strength and hardness of powder metallurgy stainless steels can be enhanced and the superior corrosion resistance is still preserved.

## Claims

### Claim 1

A method for enhancing strength and hardness of powder metallurgy stainless steels, comprising steps of:
fabricating a stainless steel powder into a green compact;
placing the green compact in a reducing environment and maintaining the green compact at a sintering temperature to form a sintered body; and
placing the sintered body in a carbon-bearing atmosphere and maintaining the sintered body at a carburizing temperature below 600° C. to implant carbon atoms into the sintered body and form carburized regions in the sintered body.

### Claim 2 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the reducing environment is vacuum or hydrogen-bearing atmosphere.

### Claim 3 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the sintering temperature ranges from 1,050 to 1,400° C.

### Claim 4 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the carburizing temperature ranges from 400 to 580° C.

### Claim 5 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the sintered body has a relative density of greater than 30%.

### Claim 6 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the green compact is fabricated with an Metal Injection Molding method.

### Claim 7 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steel according to claim 1, wherein the green compact is fabricated with a powder-compaction method.

### Claim 8 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the carbon-bearing atmosphere is an atmosphere containing carbon monoxide, methane, or propane.

### Claim 9 (depends on 1)

The method for enhancing strength and hardness of powder metallurgy stainless steels according to claim 1, wherein the stainless steel powder is an iron-based material containing less than 2.0 wt % carbon, less than 1.0 wt % silicon, less than 2.0 wt % manganese, 12.0-19.0 wt % chromium, less than 15.0 wt % nickel, less than 6.0 wt % molybdenum, and less than 6.0 wt % copper.