# US 2012/0251376 A1 · Process for producing improved grain refining aluminium-titanium-boron master alloys for aluminum foundry alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251376 A1
- Document ID: US20120251376A1
- Status: Published application
- Kind: A1
- Application number: 13/203,538
- Filed: 2009-02-27
- Published: 2012-10-04
- Earliest claimed: 2009-02-27
- Assignees: Tubitak
- Inventors: Yucel Birol
- Web page: https://patentgrep.com/patent/US20120251376A1

## CPC

- C22C 1/1036: {starting from a melt}
- C22C 1/03: using master alloys
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A process is provided for producing aluminium-titanium-boron grain refining master alloys containing soluble titanium aluminide and insoluble aluminium boride particles, the process comprising mixing aluminium-boron alloy powder and K2TiF6 salt to obtain a blended mixture, heat treating the mixed powder blend thus obtained in an inert gas furnace just below the melting point of aluminium, at approximately 650 degrees Celcius sufficiently long and compacting the heated powder blend in the form of tablets. The cast grain size of an aluminium-7 wt % silicon foundry alloy after inoculation with this master alloy at an addition level of 0.02% Ti was less than 200 microns for contact times of upto 15 minutes.

## Claims

### Claim 1

1) A method to produce Al—Ti—B grain refiner master alloys with Al3Ti particles and AlB2 particles dispersed in an aluminium matrix, comprising;
a. thoroughly mixing Al—B alloy powder and K2TiF6 salt to obtain a blended mixture,
b. heating the mixed powder blend under flowing argon to between 600 Centigrade and 650 Centigrade, more specifically to 650 Centigrade,
c. holding the mixed powder blend at this temperature for ½ hours,
d. pressing the heat treated powder blend into pellets

### Claim 2 (depends on 1)

2) A method according to claim 1, wherein the boron content of the Al—B alloy is between 1 to 10 wt %.

### Claim 3 (depends on 1)

3) A method according to claim 1, wherein the Al—B alloy powder is prepared by
a. adding KBF4 salt into molten aluminium to facilitate a salt reaction to form the AlB2 particles dispersed in an aluminium matrix,
b. pulverizing the alloy thus produced into powder form by mechanical means

### Claim 4 (depends on 1)

4) A method according to claim 1, wherein the titanium to boron ratio by weight of the resultant alloy is preferably equal to or less than 1 and the titanium and boron contents are between 1 to 5% Ti and 1 to 5% B, respectively, the balance being aluminium, potassium and fluorine.

### Claim 5 (depends on 1)

5) A method according to claim 1, wherein the resultant alloy contains Al3Ti particles smaller than 20 microns.