# US 2012/0251023 A1 · Method for producing a plain bearing element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251023 A1
- Document ID: US20120251023A1
- Status: Published application
- Kind: A1
- Application number: 13/508,096
- Filed: 2010-11-05
- Published: 2012-10-04
- Earliest claimed: 2009-11-05
- Assignees: Miba Gleitlager GmbH
- Inventors: Walter Gaertner
- Web page: https://patentgrep.com/patent/US20120251023A1

## CPC

- C23C 14/046: {Coating cavities or hollow spaces, e.g. interior of tubes; Infiltration of porous substrates}
- F16C 33/12: Structural composition; Use of special materials or surface treatments, e.g. for rust-proofing
- F16C 33/14: Special methods of manufacture; Running-in
- F16C 2204/20: Alloys based on aluminium
- F16C 2223/60: by vapour deposition, e.g. PVD, CVD
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS

## Abstract

The invention relates to a method for producing a plain bearing element (1) by means of coating a surface (5) of a substrate with a tribologically effective sliding layer (6) by means of cathode sputtering in a gas atmosphere and using at least one metal target (16), with a substrate having a cylindrical cavity (3) being used, and the target (16) being arranged at least partially in the cavity (3) and furthermore the discharge for sputtering the target (16) is supported or maintained by means of a third electrode (26).

## Claims

### Claim 1

Method for producing a plain bearing element (1) by coating a surface (5) of a substrate with a tribologically effective sliding layer (6) by means of cathode sputtering in a gas atmosphere and using at least one metal target (16), wherein a substrate is used, which has a cylindrical cavity (3) and the target (16) being arranged at least partially in the cavity (3) and furthermore the discharge for sputtering the target (16) is supported or maintained by means of a third electrode (26).

### Claim 2 (depends on 1)

Method according to claim 1, wherein a glowing cathode is used as third electrode (26).

### Claim 3 (depends on 1)

Method according to claim 1, wherein an alloy, which starts melting at a temperature of 200° C. or melts at this temperature is used as a target (16).

### Claim 4 (depends on 1)

Method according to claim 1, wherein an element selected from a group comprising Al, Cu, Ag, Sn, Bi, Sb as main alloy element is used as target (16).

### Claim 5 (depends on 1)

Method according to claim 1, wherein a target (16) is used having a maximum diameter selected from a range of 5 mm to 55 mm.

### Claim 6 (depends on 1)

Method according to claim 1, wherein the distance between the surface of the substrate to be coated and the surface of the target is at least 5 mm.

### Claim 7 (depends on 1)

Method according to claim 1, wherein before the tribologically effective layer is produced on the surface (5) of the substrate, this surface (5) is cleaned by inverse cathode sputtering by using an inert gas.

### Claim 8 (depends on 7)

Method according to claim 7, wherein during the cleaning of the surface, a voltage between −300 V and −1400 V is applied to the substrate.

### Claim 9 (depends on 1)

Method according to claim 1, wherein during the coating, a bias voltage, selected from a range having a lower limit of −200 V and an upper limit of −10 V, is applied to the substrate.

### Claim 10 (depends on 1)

Method according to claim 1, wherein a temperature of the substrate is open loop controlled and/or closed loop controlled during the coating.

### Claim 11

Metal plain bearing element (1) with a bearing element body (9) having a support element (4) with a cylindrical cavity (3) having an inner diameter (7), with a metal sliding layer (6) being disposed at the interior surface (5), wherein the inner diameter of the bearing element body is not larger than 70 mm and the sliding layer (6) is produced through cathode sputtering.

### Claim 12 (depends on 11)

Plain bearing element (1) according to claim 11, wherein the bearing element body (9) in axial direction has a length (8) that is larger than the inner diameter (7).

### Claim 13 (depends on 11)

Plain bearing element (1) according to claim 11, wherein the bearing element body (9) is embodied in a seamless way.

### Claim 14 (depends on 11)

Plain bearing element (1) according to claim 11, wherein the sliding layer (6) is made of an alloy having a base element which forms the main ingredient and which is selected from a group comprising Al, Cu, Ag, Sn, Pb, Bi, Sb.

### Claim 15 (depends on 11)

Plain bearing element (1) according to claim 11, wherein the sliding layer (6) has a structure which is free of a texture in axial direction.