# US 2012/0250186 A1 · Method for manufacturing magnetic recording medium, and magnetic recording/reproducing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0250186 A1
- Document ID: US20120250186A1
- Status: Published application
- Kind: A1
- Application number: 13/432,931
- Filed: 2012-03-28
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: Showa Denko K.K.
- Inventors: Toshikazu IRISAWA; Atsushi HASHIMOTO
- Web page: https://patentgrep.com/patent/US20120250186A1

## CPC

- C23C 14/0036: {Reactive sputtering}
- C23C 14/0042: {Controlling partial pressure or flow rate of reactive or inert gases with feedback of measurements}
- C23C 14/165: {by cathodic sputtering}
- C30B 23/002: {Controlling or regulating}
- C30B 23/025: {characterised by the substrate}
- C30B 29/52: Alloys
- G11B 5/672: {having different compositions in a plurality of magnetic layers, e.g. layer compositions having differing elemental components or differing proportions of elements}
- G11B 5/7369: {Two or more non-magnetic underlayers, e.g. seed layers or barrier layers}
- G11B 5/7373: {Non-magnetic single underlayer comprising chromium}
- G11B 5/7377: {Physical structure of underlayer, e.g. texture}
- G11B 5/851: Coating a support with a magnetic layer by sputtering
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)

## Abstract

A method for manufacturing a magnetic recording medium including at least a non-magnetic substrate, a soft magnetic underlayer, an orientation control layer that controls an orientation of an immediate upper layer, and a perpendicular magnetic layer in which a magnetization easy axis is mainly perpendicularly oriented with respect to the non-magnetic substrate so as to be laminated one another on the non-magnetic substrate. The perpendicular magnetic layer includes two or more magnetic layers, and each layer is subjected to a crystal growth such that each crystal grain composing each magnetic layer forms a columnar crystal continuous in a thickness direction together with the crystal grains composing the orientation control layer. The orientation control layer, formed of a Co—Cr alloy, is formed by the reactive sputtering using a mixture of a sputtering gas and nitrogen.

## Claims

### Claim 1

A method for manufacturing a magnetic recording medium comprising at least a non-magnetic substrate, a soft magnetic underlayer, an orientation control layer that controls an orientation of an immediate upper layer, and a perpendicular magnetic layer in which a magnetization easy axis is mainly perpendicularly oriented with respect to the non-magnetic substrate so as to be laminated one another on the non-magnetic substrate, characterized in that:
the perpendicular magnetic layer includes two or more magnetic layers, and each layer is subjected to a crystal growth such that each crystal grain composing each magnetic layer forms a columnar crystal continuous in a thickness direction together with the crystal grains composing the orientation control layer, wherein
the orientation control layer, formed of a Co—Cr alloy, is formed by reactive sputtering using a mixture of a sputtering gas and nitrogen, thereby causing the Co—Cr alloy to be doped with the nitrogen within a range from 3 atomic % to 15 atomic %.

### Claim 2 (depends on 1)

The method for manufacturing the magnetic recording medium according to claim 1, wherein the Co—Cr alloy contains Co within a range from 50 atomic % to 80 atomic % and Cr within a range from 20 atomic % to 50 atomic %.

### Claim 3 (depends on 1)

The method for manufacturing the magnetic recording medium according to claim 1, wherein the Co—Cr alloy contains at least one or more elements selected from Pt, B, Ta, Mo, Cu, Nd, W, Nb, Sm, Tb, Ru, and Re within a range from 1 atomic % to 10 atomic %.

### Claim 4 (depends on 1)

The method for manufacturing the magnetic recording medium according to claim 1, wherein, in a corrugated surface in which a top part of each columnar crystal composing the orientation control layer is formed into a convex, a height from the topmost part of each columnar crystal to a boundary with the next columnar crystal is set to a value of an outer diameter or less of the columnar crystal.

### Claim 5 (depends on 1)

The method for manufacturing the magnetic recording medium according to claim 1, wherein the crystal grains composing the orientation control layer are set to have a grain diameter of 5 nm or less.

### Claim 6 (depends on 1)

The method for manufacturing the magnetic recording medium according to claim 1, wherein a Ru layer or a second orientation control layer containing Ru as a main component is formed on the orientation control layer.

### Claim 7 (depends on 1)

The method for manufacturing the magnetic recording medium according to claim 1, wherein the magnetic layer or the non-magnetic layer has a granular structure.

### Claim 8 (depends on 1)

A magnetic recording/reproducing apparatus, comprising:
a magnetic recording medium manufactured by the manufacturing method according to claim 1, and
a magnetic head for performing recording and reproducing of information with respect to the magnetic recording medium.