# US 2012/0247005 A1 · METHOD AND REACTOR FOR PROCESSING BULK MATERIAL CONTAINING Li

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0247005 A1
- Document ID: US20120247005A1
- Status: Published application
- Kind: A1
- Application number: 13/501,478
- Filed: 2010-10-15
- Published: 2012-10-04
- Earliest claimed: 2009-10-14
- Inventors: Hubert Jaeger; Johann Daimer
- Web page: https://patentgrep.com/patent/US20120247005A1

## CPC

- C22B 26/12: Obtaining lithium
- C01D 15/02: Oxides; Hydroxides
- C22B 7/001: {Dry processes}
- F27D 99/0001: {Heating elements or systems}
- H01M 10/4242: {Regeneration of electrolyte or reactants}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The invention relates to a method for recovering lithium from a starting material comprising lithium. According to the invention, the starting material is heated with carbon in a reactor by carrying out direct inductive heating of the carbon.

## Claims

### Claim at position 1

-26. (canceled)

### Claim 27

A method of reclaiming lithium from a starting material containing lithium, comprising the step of heating the starting material with carbon in a reactor in which the carbon is directly inductively heated.

### Claim 28 (depends on 27)

The method in accordance with claim 27, wherein the starting material contains carbon which is suitable to be directly inductively heated.

### Claim 29 (depends on 27)

The method in accordance with claim 27, wherein the carbon, which is suitable to be directly inductively heated, is added to and/or is to be added to the starting material.

### Claim 30 (depends on 27)

The method in accordance with claim 27, wherein the starting material and/or the bulk material contain(s) waste from batteries containing lithium ions.

### Claim 31 (depends on 27)

The method in accordance with claim 27, wherein bulk material is used of which more than 50% by weight has a grain size of more than 30 mm.

### Claim 32 (depends on 27)

The method in accordance with claim 27, wherein bulk material is used of which more than 50% by weight has a grain size of between 50 and 150 mm.

### Claim 33 (depends on 27)

The method in accordance with claim 27, wherein the step of heating is carried out inductively at frequencies between 1 and 50 kHz.

### Claim 34 (depends on 27)

The method in accordance with claim 27, wherein maximum temperatures are set in the reactor between 1100° C. and 3000° C.

### Claim 35 (depends on 27)

The method in accordance with claim 27, wherein lithium converted into a gaseous phase is precipitated with a liquid.

### Claim 36 (depends on 27)

The method in accordance with claim 27, wherein water and/or water vapor is introduced in at least one zone of the reactor.

### Claim 37

A reactor for carrying out a method of reclaiming lithium from a starting material containing lithium, wherein the reactor comprises induction coils which are suitable to heat the carbon directly inductively.

### Claim 38 (depends on 37)

The reactor in accordance with claim 37, wherein the induction coils are suitable to heat the starting material with a radial temperature gradient which is less than 100 K/m.

### Claim 39 (depends on 37)

The reactor in accordance with claim 37, wherein the reactor further comprises a high temperature resistant inner wall into which the induction fields generated by the induction coils at the frequencies used for heating the bulk material do not couple or at least hardly do not couple.

### Claim 40 (depends on 37)

The reactor in accordance with claim 37, wherein the inner wall has a lining which contains at least one material from the group comprising carbon, oxidic refractory materials, non-oxidic refractory materials and chamotte.

### Claim 41 (depends on 40)

The reactor in accordance with claim 40, wherein the lining comprises clay-bound graphite.

### Claim 42 (depends on 37)

The reactor in accordance with claim 37, wherein the reactor has a reactor space which has an upper zone, a middle zone and a lower zone in the axial direction, with the middle zone being provided with the induction coils extending at least partly around the reactor and purified bulk material accumulating in the lower zone and wherein the purified bulk material can be removed from it.

### Claim 43 (depends on 37)

The reactor in accordance with claim 37, wherein the reactor has a diameter in the region of the induction coils of more than 50 cm.

### Claim 44 (depends on 37)

The reactor in accordance with claim 37, wherein the reactor further comprises a loading lock via which the reactor can be supplied with starting material, with the loading lock being suitable to prevent an uncontrolled escape of gases from the reactor.

### Claim 45 (depends on 37)

The reactor in accordance with claim 37, wherein a gas scrubber connected to the reactor space is provided which is suitable to precipitate lithium transferred into a gaseous phase with a liquid.

### Claim 46 (depends on 37)

The reactor in accordance with claim 37, wherein at least one injection apparatus is provided which is suitable to introduce water and/or water vapor into the reactor space in at least one of the upper, middle and lower zones.

### Claim 47

A bulk material containing carbon purified using a method of reclaiming lithium from a starting material containing lithium, said method comprising the step of heating the starting material with carbon in a reactor, in which the carbon is directly inductively heated, as a fuel or as a resource.