# US 2012/0241053 A1 · Use of intermediate piece for connecting molded articles of manganese steel with carbon steel, and method for connecting austenitic manganese steel casting pieces with standard rails

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0241053 A1
- Document ID: US20120241053A1
- Status: Published application
- Kind: A1
- Application number: 13/489,991
- Filed: 2012-06-06
- Published: 2012-09-27
- Earliest claimed: 2007-10-05
- Assignees: VAE GmbH; VAE Eisenbahnsysteme GmbH
- Inventors: Johannes BLUMAUER
- Web page: https://patentgrep.com/patent/US20120241053A1

## CPC

- B23K 35/004: {at least one of the workpieces being of a metal of the iron group}
- C21D 6/004: {containing Cr and Ni}
- C21D 9/04: for rails
- C22C 38/001: {containing N}
- C22C 38/44: with molybdenum or tungsten
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

In an intermediate piece for connecting molded articles of manganese steel with carbon steel, in particular austenitic manganese steel casting frogs with standard rails, the intermediate piece is comprised of steel from the group of austenitic-ferritic duplex steels having a ferrite portion of <60 wt %. The method for connecting austenitic manganese steel castings with standard rails is characterized in that an austenitic-ferritic intermediate piece made of duplex steel comprising <60% ferrite is welded with the manganese steel casting and the standard rail.

## Claims

### Claim 1

Use of an intermediate piece for connecting a molded article of manganese steel with a standard rail made of carbon steel, wherein said intermediate piece is comprised of steel from the group of austenitic-ferritic duplex steels having a ferrite portion of less than 60 weight percent.

### Claim 2 (depends on 1)

Use of an intermediate piece according to claim 1, wherein said intermediate piece is comprised of steel having a directional analysis of:
C max 0.03 weight %;
Cr 21-23 weight %;
Ni 4.5-6.5 weight %;
Mo 2.5-3.5 weight %; and
N 0.1-2.22 weight %.

### Claim 3 (depends on 1)

Use of an intermediate piece according to claim 1, wherein the intermediate piece is solution-annealed and subsequently quenched.

### Claim 4 (depends on 1)

Use of an intermediate piece according to claim 1, wherein the intermediate piece is solution-annealed at 900° C. to 1100° C., and subsequently quenched with water, and further quenched by air.

### Claim 5 (depends on 1)

Use of an intermediate piece according to claim 1, wherein the molded article of manganese steel is an austenitic manganese steel casting frog.

### Claim 6 (depends on 2)

Use of an intermediate piece according to claim 2, wherein the intermediate piece is solution-annealed and subsequently quenched.

### Claim 7 (depends on 2)

Use of an intermediate piece according to claim 2, wherein the intermediate piece is solution-annealed at 900° C. to 1100° C., and subsequently quenched with water, and further quenched by air.

### Claim 8

A method for connecting an austenitic manganese steel casting with a standard rail made of carbon steel, comprising the step of welding an austenitic-ferritic intermediate piece comprised of duplex steel comprising less than 60 percent ferrite with the manganese steel casting and the standard rail.

### Claim 9 (depends on 8)

A method according to claim 8, wherein the intermediate piece has a directional analysis of:
C max 0.03 weight %;
Cr 21-23 weight %;
Ni 4.5-6.5 weight %;
Mo 2.5-3.5 weight %; and
N 0.1-2.22 weight %;
and wherein the intermediate piece is initially welded with the standard rail and subsequently welded with the austenitic manganese steel casting.

### Claim 10 (depends on 8)

A method according to claim 8, wherein the intermediate piece is cooled with compressed air during the welding step.

### Claim 11 (depends on 8)

A method according to claim 8, wherein, before the welding step, the intermediate piece is solution-annealed at 900° C. to 1100° C. and is subsequently quenched with water and further quenched by air.

### Claim 12 (depends on 8)

A method according to claim 8, wherein, after the welding step, the welded connection with the standard rail is cooled and then is annealed at 200° C. to 600° C. for tempering.

### Claim 13 (depends on 8)

A method according to claim 8, wherein, after the welding step, the welded connection with the manganese steel casting is cooled and then is annealed at 200° C. to 600° C. for tempering.

### Claim 14 (depends on 8)

A method according to claim 8, wherein the intermediate piece is subjected to a hardening treatment prior to or after the welding step.

### Claim 15 (depends on 9)

A method according to claim 9, wherein the intermediate piece is cooled with compressed air during welding.

### Claim 16 (depends on 9)

A method according to claim 9, wherein, before welding, the intermediate piece is solution-annealed at 900° C. to 1100° C. and is subsequently quenched with water and further quenched by air.

### Claim 17 (depends on 10)

A method according to claim 10, wherein, before the welding step, the intermediate piece is solution-annealed at 900° C. to 1100° C. and is subsequently quenched with water and further quenched by air.

### Claim 18 (depends on 9)

A method according to claim 9, wherein the welded connection with the standard rail is cooled and then is annealed at 200° C. to 600° C. for tempering.

### Claim 19 (depends on 9)

A method according to claim 9, wherein the welded connection with the manganese steel casting is cooled and then is annealed at 200° C. to 600° C. for tempering.

### Claim 20 (depends on 9)

A method according to claim 9, wherein the intermediate piece is subjected to a hardening treatment prior to or after welding.