# US 2012/0237823 A1 · Porous three dimensional copper, tin, copper-tin, copper-tin-cobalt, and copper-tin-cobalt-titanium electrodes for batteries and ultra capacitors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0237823 A1
- Document ID: US20120237823A1
- Status: Published application
- Kind: A1
- Application number: 13/486,202
- Filed: 2012-06-01
- Published: 2012-09-20
- Earliest claimed: 2009-02-04
- Assignees: Applied Materials, Inc.
- Inventors: SERGEY D. LOPATIN; Dmitri A. BREVNOV; Robert Z. BACHRACH
- Web page: https://patentgrep.com/patent/US20120237823A1

## CPC

- C25D 3/38: of copper
- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 5/48: After-treatment of electroplated surfaces
- C25D 5/605: {Surface topography of the layers, e.g. rough, dendritic or nodular layers}
- C25D 5/623: {Porosity of the layers}
- C25D 17/00: Constructional parts, or assemblies thereof, of cells for electrolytic coating
- H01M 4/0438: {by electrochemical processing (electroless electrochemical plating C23C18/54)}
- H01M 4/366: {as layered products}
- H01M 4/38: of elements or alloys
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- Y02E 60/10: Energy storage using batteries
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method and apparatus for forming a reliable and cost efficient battery or electrochemical capacitor electrode structure that has an improved lifetime, lower production costs, and improved process performance are provided. In one embodiment a method for forming a three dimensional porous electrode for a battery or an electrochemical cell is provided. The method comprises depositing a columnar metal layer over a substrate at a first current density by a diffusion limited deposition process and depositing three dimensional metal porous dendritic structures over the columnar metal layer at a second current density greater than the first current density.

## Claims

### Claim 1

A substrate processing system for processing a vertically oriented flexible conductive substrate, comprising:
a first plating chamber configured to plate a conductive microstructure comprising a first conductive material over a portion of the vertically oriented flexible conductive substrate;
a first rinse chamber configured to rinse and remove any residual plating solution from the portion of the vertically oriented flexible conductive substrate with a rinsing fluid;
a second plating chamber configured to deposit a second conductive material over the conductive microstrutures;
a second rinse chamber configured to rinse and remove any residual plating solution from the portion of the vertically oriented flexible conductive substrate.
a substrate transfer mechanism configured to transfer the vertically oriented flexible conductive substrate among the chambers, wherein each of the chambers comprises:
a processing volume;
a feed roll disposed outside the processing volume and configured to retain a portion of the vertically oriented flexible conductive substrate; and
a take up roll disposed out side the processing volume and configured to retain a portion of the vertically oriented flexible conductive substrate, wherein the substrate transfer mechanism is configured to activate the feed rolls and the take up rolls to move the vertically oriented flexible conductive substrate in and out of each chamber, and hold the vertically oriented flexible conductive substrate in the processing volume of each chamber.

### Claim 2 (depends on 1)

The substrate processing system of claim 1, further comprising:
a spray coating chamber configured to deposit lithium containing particles over the vertically oriented flexible conductive substrate.

### Claim 3 (depends on 1)

The substrate processing chamber of claim 1, wherein the conductive microstructure comprises a columnar metal layer with a three dimensional metal porous dendritic structure deposited over the columnar metal layer.

### Claim 4 (depends on 3)

The substrate processing system of claim 3, wherein the first conductive material comprises copper and the second conductive material comprises tin.

### Claim 5 (depends on 1)

The substrate processing chamber of claim 1, wherein first plating chamber, the first rinse chamber, second plating chamber, and the second rinse chamber are each configured to simultaneously process opposite sides of the portion of the vertically oriented flexible conductive substrate.

### Claim 6

An electrochemical capacitor, comprising:
a flexible conductive current collector;
a porous electrode comprising:
a columnar metal layer formed on the flexible conductive current collector; and
a three-dimensional metal macro-porous dendrictic structure formed over the columnar metal layer, wherein the three dimensional metal macro-porous dendritic structure has pores of about 100 microns or less; and
a separator formed over the three dimensional metal macro-porous dendritic structure.

### Claim 7 (depends on 6)

The electrochemical capacitor of claim 6, wherein the three-dimensional metal macro-porous dendritic structure has pores between about 2 nanometers and about 50 nanometers.

### Claim 8 (depends on 7)

The electrochemical capacitor of claim 7, wherein the three-dimensional metal macro-porous dendritic structure comprises a copper-tin alloy.

### Claim 9 (depends on 7)

The electrochemical capacitor of claim 7, further comprising a tin layer formed on the three-dimensional metal macro-porous dendritic structure, wherein the three-dimensional metal macro-porous dendritic structure comprises copper.

### Claim 10 (depends on 6)

The electrochemical capacitor of claim 6, further comprising a passivation layer formed on the three-dimensional metal macro-porous dendritic structure.

### Claim 11 (depends on 10)

The electrochemical capacitor of claim 10, wherein the passivation layer is selected from the group consisting of: lithium-copper-phosphorous-oxynitride (P—O—N), lithium-copper-boron-oxynitride (B—O—N), lithium-copper-oxides, lithium-copper-silicon oxides, lithium-copper-nickel oxides, lithium-copper-tin oxides, lithium-copper-cobalt oxides, lithium-copper-cobalt-tin-titanium oxides, lithium-copper-cobalt-nickel-aluminum oxides, lithium-copper-titanium oxides, lithium-aluminum-silicon, lithium-copper-manganese oxides, and lithium-copper-iron-phosphides.

### Claim 12 (depends on 6)

The electrochemical capacitor of claim 6, wherein the separator is a porous separator.

### Claim 13 (depends on 12)

The electrochemical capacitor of claim 12, wherein the separator comprises a material selected from the group comprising: polyolefin, polypropylene, polyethylene, and combinations thereof.

### Claim 14 (depends on 13)

The electrochemical capacitor of claim 13, wherein the separator further comprises inorganic particles selected from the group comprising aluminum oxide, silica, ceramic particles, and combinations thereof embedded in the separator.

### Claim 15

A battery, comprising:
a flexible conductive current collector;
a porous electrode comprising:
a columnar metal layer formed on the flexible conductive current collector; and
a three-dimensional metal macro-porous dendrictic structure formed over the columnar metal layer, wherein the three dimensional metal macro-porous dendritic structure has pores of about 100 microns or less; and
a separator formed over the three dimensional metal macro-porous dendritic structure.

### Claim 16 (depends on 15)

The electrochemical capacitor of claim 15, wherein the three-dimensional metal macro-porous dendritic structure has pores between about 2 nanometers and about 50 nanometers.

### Claim 17 (depends on 16)

The electrochemical capacitor of claim 16, wherein the three-dimensional metal macro-porous dendritic structure comprises a copper-tin alloy.

### Claim 18 (depends on 16)

The electrochemical capacitor of claim 16, further comprising a tin layer formed on the three-dimensional metal macro-porous dendritic structure, wherein the three-dimensional metal macro-porous dendritic structure comprises copper.

### Claim 19 (depends on 15)

The electrochemical capacitor of claim 15, further comprising a passivation layer formed on the three-dimensional metal macro-porous dendritic structure.

### Claim 20 (depends on 19)

The electrochemical capacitor of claim 19, wherein the passivation layer is selected from the group consisting of: lithium-copper-phosphorous-oxynitride (P—O—N), lithium-copper-boron-oxynitride (B—O—N), lithium-copper-oxides, lithium-copper-silicon oxides, lithium-copper-nickel oxides, lithium-copper-tin oxides, lithium-copper-cobalt oxides, lithium-copper-cobalt-tin-titanium oxides, lithium-copper-cobalt-nickel-aluminum oxides, lithium-copper-titanium oxides, lithium-aluminum-silicon, lithium-copper-manganese oxides, and lithium-copper-iron-phosphides.