# US 2012/0237822 A1 · Lithium ion secondary battery and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0237822 A1
- Document ID: US20120237822A1
- Status: Published application
- Kind: A1
- Application number: 13/419,639
- Filed: 2012-03-14
- Published: 2012-09-20
- Earliest claimed: 2011-03-18
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Tomoya Futamura; Tamae Moriwaka; Takahiro Kawakami; Junpei Momo; Nobuhiro Inoue
- Web page: https://patentgrep.com/patent/US20120237822A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/362: {Composites}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/665: {Composites}
- H01M 4/668: {Composites of electroconductive material and synthetic resins}
- C30B 1/00: Single-crystal growth directly from the solid state (unidirectional demixing of eutectoid materials C30B3/00; under a protective fluid C30B27/00)
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A lithium ion secondary battery includes a positive electrode, a negative electrode, and an electrolyte provided between the positive electrode and the negative electrode. The positive electrode includes a positive electrode current collector and a positive electrode active material layer over the positive electrode current collector. The positive electrode active material layer includes a plurality of lithium-containing composite oxides each of which is expressed by LiMPO4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) that is a general formula. The lithium-containing composite oxide is a flat single crystal particle in which the length in the b-axis direction is shorter than each of the lengths in the a-axis direction and the c-axis direction. The lithium-containing composite oxide is provided over the positive electrode current collector so that the b-axis of the single crystal particle intersects with the surface of the positive electrode current collector.

## Claims

### Claim 1

A lithium ion secondary battery comprising:
a positive electrode comprising:
a positive electrode current collector; and
a positive electrode active material layer over the positive electrode current collector, the positive electrode active material layer comprising a plurality of single crystal particles;
a negative electrode; and
an electrolyte provided between the positive electrode and the negative electrode,
wherein each of the single crystal particles is a lithium-containing composite oxide,
wherein in each of the single crystal particles, a length in a b-axis direction is shorter than each of lengths in an a-axis direction and a c-axis direction, and
wherein each of the single crystal particles is provided over the positive electrode current collector so that a b-axis of each of the single crystal particles intersects with a surface of the positive electrode current collector.

### Claim 2 (depends on 1)

The lithium ion secondary battery according to claim 1, wherein each length in the b-axis direction of the single crystal particles is greater than or equal to 5 nm and less than or equal to 50 nm.

### Claim 3 (depends on 1)

The lithium ion secondary battery according to claim 1, wherein a b-axis of each of the single crystal particles intersects with the surface of the positive electrode current collector at an angle greater than or equal to 60 degrees and less than or equal to 90 degrees.

### Claim 4 (depends on 1)

The lithium ion secondary battery according to claim 1, wherein at least one of the single crystal particles is overlapped with at least another one of the single crystal particles.

### Claim 5 (depends on 1)

The lithium ion secondary battery according to claim 1, wherein the lithium-containing composite oxide has an olivine structure.

### Claim 6 (depends on 1)

The lithium ion secondary battery according to claim 1, wherein the lithium-containing composite oxide is expressed by LiMPO4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) that is a general formula.

### Claim 7 (depends on 1)

The lithium ion secondary battery according to claim 1, wherein each of the single crystal particles is a flat single crystal particle.

### Claim 8

A method for manufacturing a lithium ion secondary battery, comprising the steps of:
applying a slurry including a plurality of single crystal particles to an upper surface of a positive electrode current collector, wherein each of the single crystal particles is a lithium-containing composite oxide, and wherein in each of the single crystal particles, a length in a b-axis direction is shorter than each of lengths in an a-axis direction and a c-axis direction; and
exerting pressure on the slurry so that a b-axis of each of the single crystal particles intersects with the upper surface of the positive electrode current collector.

### Claim 9 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein each length in the b-axis direction of the single crystal particles is greater than or equal to 5 nm and less than or equal to 50 nm.

### Claim 10 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein a b-axis of each of the single crystal particles intersects with the upper surface of the positive electrode current collector at an angle greater than or equal to 60 degrees and less than or equal to 90 degrees.

### Claim 11 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein at least one of the single crystal particles is overlapped with at least another one of the single crystal particles.

### Claim 12 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein the lithium-containing composite oxide has an olivine structure.

### Claim 13 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein the lithium-containing composite oxide is expressed by LiMPO4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) that is a general formula.

### Claim 14 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein each of the single crystal particles is a flat single crystal particle.

### Claim 15 (depends on 8)

The method for manufacturing a lithium ion secondary battery, according to claim 8, wherein the step of exerting pressure on the slurry is a step of moving a roller over the slurry.

### Claim 16

A method for manufacturing a lithium ion secondary battery, comprising the steps of:
applying a slurry including a plurality of single crystal particles to an upper surface of a positive electrode current collector, wherein each of the single crystal particles is a lithium-containing composite oxide, and wherein in each of the single crystal particles, a length in a b-axis direction is shorter than each of lengths in an a-axis direction and a c-axis direction; and
transmitting vibration to the slurry so that a b-axis of each of the single crystal particles intersects with the upper surface of the positive electrode current collector.

### Claim 17 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein each length in the b-axis direction of the single crystal particles is greater than or equal to 5 nm and less than or equal to 50 nm.

### Claim 18 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein a b-axis of each of the single crystal particles intersects with the upper surface of the positive electrode current collector at an angle greater than or equal to 60 degrees and less than or equal to 90 degrees.

### Claim 19 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein at least one of the single crystal particles is overlapped with at least another one of the single crystal particles.

### Claim 20 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein the lithium-containing composite oxide has an olivine structure.

### Claim 21 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein the lithium-containing composite oxide is expressed by LiMPO4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) that is a general formula.

### Claim 22 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein each of the single crystal particles is a flat single crystal particle.

### Claim 23 (depends on 16)

The method for manufacturing a lithium ion secondary battery, according to claim 16, wherein the step of transmitting vibration to the slurry is a step of transmitting ultrasonic vibration to the slurry.

### Claim 24

A positive electrode comprising:
a positive electrode current collector; and
a positive electrode active material layer over the positive electrode current collector, the positive electrode active material layer comprising a plurality of single crystal particles,
wherein each of the single crystal particles is a lithium-containing composite oxide,
wherein in each of the single crystal particles, a length in a b-axis direction is shorter than each of lengths in an d-axis direction and a c-axis direction, and
wherein each of the single crystal particles is provided over the positive electrode current collector so that a b-axis of each of the single crystal particles intersects with a surface of the positive electrode current collector.