# US 2012/0237728 A1 · Molded ferrite sheet, sintered ferrite substrate and antenna module

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0237728 A1
- Document ID: US20120237728A1
- Status: Published application
- Kind: A1
- Application number: 13/482,100
- Filed: 2012-05-29
- Published: 2012-09-20
- Earliest claimed: 2007-03-07
- Assignees: Toda Kogyo Corporation
- Inventors: Tetsuya KIMURA; Tomohiro Dote; Kazumi Yamamoto; Takanori Doi; Yoji Okano
- Web page: https://patentgrep.com/patent/US20120237728A1

## CPC

- C04B 35/62218: {obtaining ceramic films, e.g. by using temporary supports}
- C04B 35/265: {Compositions containing one or more ferrites of the group comprising manganese or zinc and one or more ferrites of the group comprising nickel, copper or cobalt}
- C04B 35/63408: {Polyalkenes}
- H01F 1/344: {Ferrites, e.g. having a cubic spinel structure (X2+O)(Y23+O3), e.g. magnetite Fe3O4}
- H01F 41/16: the magnetic material being applied in the form of particles, e.g. by serigraphy {, to form thick magnetic films or precursors therefor} (H01F41/18 {-H01F41/24} take precedence)
- H01Q 17/00: Devices for absorbing waves radiated from an antenna; Combinations of such devices with active antenna elements or systems
- C04B 2235/3234: Titanates, not containing zirconia
- C04B 2235/3279: Nickel oxides, nickalates, or oxide-forming salts thereof
- C04B 2235/3281: Copper oxides, cuprates or oxide-forming salts thereof, e.g. CuO or Cu2O
- C04B 2235/3284: Zinc oxides, zincates, cadmium oxides, cadmiates, mercury oxides, mercurates or oxide forming salts thereof
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/602: Making the green bodies or pre-forms by moulding
- C04B 2235/6025: Tape casting, e.g. with a doctor blade
- C04B 2235/77: Density
- C04B 2235/945: Products containing grooves, cuts, recesses or protusions
- C04B 2235/963: Surface properties, e.g. surface roughness
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- Y10T 428/31609: Particulate metal or metal compound-containing
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H01Q: ANTENNAS, i.e. RADIO AERIALS (radiators or antennas for microwave heating H05B6/72)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a molded ferrite sheet having opposing surfaces and a thickness in a range of 30 μm to 430 μm, at least one surface of said opposing surfaces having the following surface roughness characteristics (a) to (c): (a) a center line average roughness is in a range of 170 nm to 800 nm, (b) a maximum height is in a range of 3 μm to 10 μm, and (c) an area occupancy rate of cross-sectional area taken along a horizontal plane at a depth of 50% of the maximum height in a square of side 100 μm is in a range of 10 to 80%.

## Claims

### Claim at position 1

-18. (canceled)

### Claim 19

A method of preparing molded ferrite sheet having opposing surfaces and a thickness in a range of 30 μm to 430 μm, comprising subjecting at least one surface to sandblasting with a polishing material thereby roughening said surface, wherein
at least one surface of said opposing surfaces having the following surface roughness characteristics (a) to (c):
(a) a center line average roughness is in the range of 170 nm to 800 nm,
(b) a maximum height is in a range of 3 μm to 10 μm, and
(c) an area occupancy rate of cross-sectional area taken along a horizontal plane at a depth of 50% of the maximum height in a square of said 100 μm is in a range of 10 to 80%.

### Claim 20

A method of preparing molded ferrite sheet having opposing surfaces and a thickness in a range of 30 μm to 430 μm, comprising subjecting at least one surface to roughening said surface, wherein
at least one surface of said opposing surfaces having the following surface roughness characteristics (a) to (c):
(a) a center line average roughness is in the range of 170 nm to 800 nm,
(b) a maximum height is in a range of 3 μm to 10 μm, and
(c) an area occupancy rate of cross-sectional area taken along a horizontal plane at a depth of 50% of the maximum height in a square of said 100 μm is in a range of 10 to 80%,
comprising preparing said molded ferrite sheet by molding under pressure using a mold or calender roll having a roughened surface so that the roughness of the roughened surface of said mold or calender roll is transferred to a surface of said molded ferrite sheet in contact with the roughened surface of said mold or calender roll.

### Claim 21

A method of preparing molded ferrite sheet having opposing surfaces and a thickness in a range of 30 μm to 430 μm, comprising subjecting at least one surface to roughening said surface, wherein
at least one surface of said opposing surfaces having the following surface roughness characteristics (a) to (c):
(a) a center line average roughness is in the range of 170 nm to 800 nm,
(b) a maximum height is in a range of 3 μm to 10 μm, and
(c) an area occupancy rate of cross-sectional area taken along a horizontal plane at a depth of 50% of the maximum height in a square of said 100 μm is in a range of 10 to 80%,
comprising preparing said molded ferrite sheet by applying a coating of a ferrite-dispersed coating liquid to a surface of a plastic film, and drying the applied coating, and wherein said surface of said plastic film has been roughened by sandblasting so that the roughness of said plastic film is transferred to a surface of the dried coating in contact with the roughened surface of said plastic film.

### Claim 22

A method of preparing molded ferrite sheet having opposing surfaces and a thickness in a range of 30 μm to 430 μm, comprising subjecting at least one surface to roughening said surface, wherein
at least one surface of said opposing surfaces having the following surface roughness characteristics (a) to (c):
(a) a center line average roughness is in the range of 170 nm to 800 nm,
(b) a maximum height is in a range of 3 μm to 10 μm, and
(c) an area occupancy rate of cross-sectional area taken along a horizontal plane at a depth of 50% of the maximum height in a square of said 100 μm is in a range of 10 to 80%,
comprising preparing said molded ferrite sheet by applying a coating of a ferrite-dispersed coating liquid to a support and drying the applied coating, wherein the ferrite has been obtained by adjusting a particle size of a ferrite powder having an average particle diameter of 0.1 to 10 μm so that the surface roughness characteristics are imparted to a surface of the dried coating in contact with said support.

### Claim 23 (depends on 19)

The molded ferrite sheet prepared by the process of claim 19, wherein the ferrite is Ni—Zn—Cu-based spinel ferrite or Mg—Zn—Cu-based spinel ferrite.

### Claim 24 (depends on 20)

The molded ferrite sheet prepared by the process of claim 20, wherein the ferrite is Ni—Zn—Cu-based spinel ferrite or Mg—Zn—Cu-based spinel ferrite.

### Claim 25 (depends on 21)

The molded ferrite sheet prepared by the process of claim 21, wherein the ferrite is Ni—Zn—Cu-based spinel ferrite or Mg—Zn—Cu-based spinel ferrite.

### Claim 26 (depends on 22)

The molded ferrite sheet prepared by the process of claim 22, wherein the ferrite is Ni—Zn—Cu-based spinel ferrite or Mg—Zn—Cu-based spinel ferrite.