# US 2012/0237699 A1 · Printable and printed articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0237699 A1
- Document ID: US20120237699A1
- Status: Published application
- Kind: A1
- Application number: 13/046,976
- Filed: 2011-03-14
- Published: 2012-09-20
- Earliest claimed: 2011-03-14
- Assignees: Hewlett-Packard Development Company, L.P.
- Inventors: Dheya M. Alfekri; Ronald J. Selensky
- Web page: https://patentgrep.com/patent/US20120237699A1

## CPC

- D06P 5/30: Ink jet printing
- B32B 27/10: of paper or cardboard
- B32B 27/12: next to a fibrous or filamentary layer
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B41M 5/506: {Intermediate layers}
- B41M 5/52: Macromolecular coatings
- B41M 5/5218: {characterised by inorganic additives, e.g. pigments, clays}
- B41M 5/5254: {characterised by the use of polymers obtained by reactions only involving carbon-to-carbon unsaturated bonds, e.g. vinyl polymers}
- B32B 2255/10: on synthetic resin layer or on natural or synthetic rubber layer
- B32B 2307/75: Printability
- B32B 2451/00: Decorative or ornamental articles
- B41M 5/5236: {characterised by the use of natural gums, of proteins, e.g. gelatins, or of macromolecular carbohydrates, e.g. cellulose}
- B41M 5/5245: {characterised by the use of polymers containing cationic or anionic groups, e.g. mordants}
- B41M 5/5272: {Polyesters; Polycarbonates}
- B41M 5/5281: {Polyurethanes or polyureas}
- B41M 7/0036: {using protective coatings or layers dried without curing}
- Y10T 428/24802: Discontinuous or differential coating, impregnation or bond [e.g., artwork, printing, retouched photograph, etc.]
- D06P: DYEING OR PRINTING TEXTILES; DYEING LEATHER, FURS OR SOLID MACROMOLECULAR SUBSTANCES IN ANY FORM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Printable articles including a substrate, an image receiving layer over the substrate, and a barrier layer between the substrate and the image receiving layer are useful in the production of fine art reproductions. The image receiving layer comprises at least one pigment and two or more binders, wherein at least one of the two or more binders has a glass transition temperature (Tg) at least 20° C. less than a Tg of at least one other of the two or more binders. Printed articles including a printable article with marking material contained in the image receiving layer may exhibit a textured cracking pattern after application and drying of the marking material or a liquid laminate.

## Claims

### Claim 1

A printable article, comprising:
a substrate;
an image receiving layer over the substrate; and
a barrier layer between the substrate and the image receiving layer;
wherein the image receiving layer comprises at least one pigment and two or more binders; and
wherein at least one of the two or more binders has a glass transition temperature (Tg) at least 20° C. less than a Tg of at least one other of the two or more binders.

### Claim 2 (depends on 1)

The printable article of claim 1, further comprising:
wherein the at least one of the two or more binders has a Tg of less than 25° C.; and wherein the at least one other of the two or more binders has a Tg of greater than 25° C.

### Claim 3 (depends on 1)

The printable article of claim 1, wherein the at least one of the two or more binders has a Tg at least 30° C. less than the at least one other of the two or more binders.

### Claim 4 (depends on 1)

The printable article of claim 1, wherein the at least one of the two or more binders has a Tg of less than 10° C.

### Claim 5 (depends on 1)

The printable article of claim 1, wherein the at least one of the two or more binders has a Tg of less than 0° C.

### Claim 6 (depends on 1)

The printable article of claim 1, wherein the two or more binders comprise dried acrylic polymer emulsions.

### Claim 7 (depends on 1)

The printable article of claim 1, wherein image receiving layer comprises 20-60 dry weight % of the two or more binders.

### Claim 8 (depends on 1)

The printable article of claim 1, wherein image receiving layer comprises 40-80 dry weight % of the at least one pigment.

### Claim 9 (depends on 1)

The printable article of claim 1, wherein the image receiving layer has a coating weight of 10-70 gsm.

### Claim 10 (depends on 1)

The printable article of claim 1, wherein the substrate is a fibrous substrate.

### Claim 11 (depends on 1)

The printable article of claim 1, wherein the at least one pigment comprises at least one hollow polymer pigment.

### Claim 12 (depends on 11)

The printable article of claim 11, wherein the at least one hollow polymer pigment comprises a dried acrylic or styrene acrylic polymer emulsion.

### Claim 13 (depends on 1)

The printable article of claim 1, wherein the barrier layer is impervious to a liquid coating used to form the image receiving layer.

### Claim 14 (depends on 1)

The printable article of claim 1, wherein the image receiving layer further comprises microporous and/or mesoporous inorganic particles.

### Claim 15

A printable article, comprising:
a fibrous substrate;
an image receiving layer over the fibrous substrate; and
a barrier layer between the fibrous substrate and the image receiving layer;
wherein the image receiving layer comprises at least one polymer pigment and two or more polymer binders; and
wherein at least one of the two or more polymer binders has a glass transition temperature (Tg) at least 20° C. less than a Tg of at least one other of the two or more polymer binders; and
wherein at least one of the two or more polymer binders has a glass transition temperature (Tg) of less than 10° C.

### Claim 16 (depends on 15)

The printable article of claim 15, wherein image receiving layer comprises at least 40 dry weight % of the two or more polymer binders.

### Claim 17 (depends on 15)

The printable article of claim 15, wherein image receiving layer comprises at least 50 dry weight % of the at least one polymer pigment.

### Claim 18 (depends on 15)

The printable article of claim 15, wherein the at least one polymer pigment comprises hollow beads.

### Claim 19

A printed article, comprising:
a substrate;
an image receiving layer over the substrate;
a barrier layer between the substrate and the image receiving layer; and
marking material contained in the image receiving layer, thereby forming an image layer comprising the image receiving layer and the marking material;
wherein the image receiving layer comprises at least one pigment and two or more binders;
wherein at least one of the two or more binders has a glass transition temperature (Tg) at least 20° C. less than a Tg of at least one other of the two or more binders; and
wherein the printed article exhibits a textured cracking pattern in the image layer.

### Claim 20 (depends on 19)

The printed article of claim 19, further comprising a liquid laminate over the image layer.