# US 2012/0234686 A1 · Method and system for preparation of highly porous and preferentially-oriented platinum nanowires and thin films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0234686 A1
- Document ID: US20120234686A1
- Status: Published application
- Kind: A1
- Application number: 13/421,706
- Filed: 2012-03-15
- Published: 2012-09-20
- Earliest claimed: 2011-03-15
- Assignees: Institut National de la Recherche Scientifique (INRS)
- Inventors: Erwan BERTIN; Sébastien GARBARINO; Daniel GUAY; Manuel MARTIN; Alexandre PONROUCH
- Web page: https://patentgrep.com/patent/US20120234686A1

## CPC

- C25D 3/50: of platinum group metals
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C25D 5/605: {Surface topography of the layers, e.g. rough, dendritic or nodular layers}
- C25D 5/617: {Crystalline layers}
- C25D 5/623: {Porosity of the layers}
- Y02E 60/50: Fuel cells
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparation of highly porous and preferentially-oriented {100} platinum on a substrate by electrodeposition in a deposition bath, comprising using a deposition potential Edep lower than ERHE+150 mV and an acidified platinum salt solution having a Pt salt concentration less than 5.0 mmole L−1 or, in presence of hydrogen, comprising limiting the concentration of Pt salts in the electrolyte to less than 5.0 mmole L−1 and controlling the temperature of the electrolyte. Preferentially-oriented {100} platinum nanowires and thin films, comprising Pt{100} in a range between about 20 and about 60% and having a roughness factor of at least 50 are produced.

## Claims

### Claim 1

A method for preparation of highly porous and preferentially-oriented {100} platinum on a substrate by electrodeposition in a deposition bath, comprising using a deposition potential Edep lower than ERHE+150 mV and an acidified platinum salt solution having a Pt salt concentration less than 5.0 mmole L−1.

### Claim 2 (depends on 1)

The method of claim 1, wherein the deposition potential Edep is about ERHE+150 mV.

### Claim 3 (depends on 1)

The method of claim 1, wherein the deposition potential Edep is about ERHE−50 mV.

### Claim 4 (depends on 1)

The method of claim 1, wherein the platinum salt concentration is less than 0.5 mmole L−1.

### Claim 5 (depends on 1)

The method of claim 1, wherein the platinum salt concentration is less than 0.25 mmole L−1.

### Claim 6 (depends on 1)

The method of claim 1, wherein the temperature of the deposition bath is less than 70° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the temperature of the deposition bath is less than 25° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate is one of Ti and carbon substrates.

### Claim 9 (depends on 1)

The method of claim 1, independent of the nature and geometry of the substrate.

### Claim 10 (depends on 1)

The method of claim 1, comprising deposition in a confined volume.

### Claim 11 (depends on 1)

The method of claim 1, comprising using a nanoporous membrane.

### Claim 12 (depends on 1)

The method of claim 1, comprising retrieving the substrate from the deposition bath after the deposition period.

### Claim 13 (depends on 1)

The method of claim 1, using KCl as supporting electrolyte.

### Claim 14 (depends on 1)

The method of claim 1, using an halide as supporting electrolyte.

### Claim 15 (depends on 1)

The method of claim 1, wherein the roughness factor of the preferentially-oriented {100} platinum is at least 50.

### Claim 16 (depends on 1)

The method of claim 1, wherein the roughness factor of the preferentially-oriented {100} platinum is comprised in a range between about 50 and about 700 for Pt{100} thin films and about 50 and about 1000 for Pt{100} nanowires.

### Claim 17 (depends on 1)

The method of claim 1, wherein the ratio I(200)/I(220) of the deposits is comprised in a range between about 1.7 and about 2.2.

### Claim 18 (depends on 1)

The method of claim 1, wherein the ratio h2/h1 of the deposits is comprised in a range between about 0.85 and about 2.2.

### Claim 19 (depends on 1)

The method of claim 1, wherein the deposits comprise Pt{100} in a range between about 20 and about 60%.

### Claim 20 (depends on 1)

The method of claim 1, wherein the rugosity of the deposits ranges from about 8 to about 420.

### Claim 21 (depends on 1)

The method of claim 1, further comprising modifying the Pt(100) surface by deposition of at least a second element.

### Claim 22 (depends on 1)

The method of claim 1, further comprising modifying the Pt(100) surface by deposition of gold.

### Claim 23

A method for preparation of highly porous and preferentially-oriented {100} platinum on a substrate by electrodeposition in presence of hydrogen, comprising limiting the concentration of Pt salts in the electrolyte to less than 5.0 mmole L−1 and controlling the temperature of the electrolyte.

### Claim 24 (depends on 23)

The method of claim 23, comprising controlling the temperature of the electrolyte to less than 70° C.

### Claim 25 (depends on 23)

The method of claim 23, comprising controlling the temperature of the electrolyte to less than 25° C.

### Claim 26 (depends on 23)

The method of claim 23, comprising limiting the concentration of Pt salts in the electrolyte to less than 0.5 mmole L−1.

### Claim 27 (depends on 23)

The method of claim 23, comprising limiting the concentration of Pt salts in the electrolyte to less than 0.25 mmole L−1.

### Claim at position 28

Preferentially-oriented {100} platinum nanowires and thin films, comprising Pt{100} in a range between about 20 and about 60% and having a roughness factor of at least 50.

### Claim 29 (depends on 28)

Preferentially-oriented {100} platinum nanowires and thin films of claim 28, having a roughness factor comprised between about 50 and about 700 for Pt{100} thin films and between about 50 and about 1000 for Pt{100} nanowires.

### Claim 30 (depends on 28)

Preferentially-oriented {100} platinum nanowires and thin films of claim 28, having a rugosity in a range comprised between about 8 and about 420.