# US 2012/0234138 A1 · Method of recovering gold from dilute gold solution

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0234138 A1
- Document ID: US20120234138A1
- Status: Published application
- Kind: A1
- Application number: 13/422,505
- Filed: 2012-03-16
- Published: 2012-09-20
- Earliest claimed: 2011-03-18
- Assignees: JX Nippon Mining & Metals Corporation
- Inventors: Kazuhiro HATANO; Yoshifumi ABE; Eiki ONO; Koji KATSUKAWA
- Web page: https://patentgrep.com/patent/US20120234138A1

## CPC

- C22B 3/302: {Ethers or epoxides}
- C22B 3/262: {using alcohols or phenols}
- C22B 11/04: {by wet processes (extraction of metal compounds by leaching in organic solutions C22B3/16; treatment or purification of solutions by liquid-liquid extraction C22B3/26)}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method of recovering gold from an aqueous solution having a gold concentration of 10 mg/L or lower, using a plurality of extraction apparatuses for bringing the aqueous solution into contact with an extraction agent, arranged to configure a multi-stage extraction process, the method allowing the aqueous solution to continuously flow from the first-stage extraction process to the next-stage extraction process, while recycling the extraction medium used in each stage twice or more times for the extraction process of the same stage, without back extraction and reduction.

## Claims

### Claim 1

A method of recovering gold from an aqueous solution having a gold concentration of 10 mg/L or lower, employing a plurality of extraction apparatuses for bringing the aqueous solution into contact with an extraction agent arranged to configure a multi-stage extraction process,
Wherein the method allows the aqueous solution to continuously flow from the first-stage extraction process to the next-stage extraction process, while recycling the extraction agent used in each stage twice or more times for the extraction process of the same stage, without back extraction and reduction; and
wherein in the first-stage extraction process the used extraction agent is repeatedly used until the concentration of gold in the extraction agent reaches to 1 g/L or above to extract gold, and wherein in the final-stage extraction process gold is extracted so that the concentration of gold in a post extraction liquid reaches to 0.5 mg/L or below.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein the extraction medium used in the second-stage process or thereafter is recycled, and then a part and/or the whole of which is fed back to the extraction apparatus in the previous stage.

### Claim 3 (depends on 1)

The method according to claim 1,
implementing a reduction process for reducing a part of, or the whole of the extraction medium after being recycled in the first-stage extraction process.

### Claim 4 (depends on 3)

The method according to claim 3,
wherein the reduction process is implemented until the gold concentration in the extraction medium decreases down to 0.5 g/L or below.

### Claim 5 (depends on 1)

The method according to claim 1,
wherein the volume ratio (O/A) of the extraction medium (Or) and the aqueous solution (Aq) in the first-stage extraction process is ⅕ or smaller.

### Claim 6 (depends on 1)

The method according to claim 1,
wherein the aqueous solution is a post-extraction liquid obtained after leaching of ore or concentrate which contains sulfide of copper.

### Claim 7 (depends on 1)

The method according to claim 1,
wherein supplementation of the extraction medium for use in each stage of extraction is implemented by using one of, or two or more media selected from the extraction medium in the succeeding stage, the extraction medium from which gold was deposited in the reduction process, and a fresh extraction medium.

### Claim 8 (depends on 1)

The method according to claim 1,
wherein the extraction medium is dibutyl carbitol (DBC).

### Claim 9 (depends on 1)

The method according to claim 1,
wherein the aqueous solution is a post-extraction liquid of copper concentrate which contains 120 to 200 g/L of chlorine, 0.1 to 30 g/L of copper, 0.01 to 10 g/L of iron, and has a pH value of 2.5 or lower.

### Claim 10 (depends on 1)

The method according to claim 1,
removing a solid matter from the aqueous solution before the aqueous solution is brought into contact with the extraction medium.