# US 2012/0231589 A1 · Thin-film transistor array device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0231589 A1
- Document ID: US20120231589A1
- Status: Published application
- Kind: A1
- Application number: 13/476,460
- Filed: 2012-05-21
- Published: 2012-09-13
- Earliest claimed: 2011-03-08
- Assignees: Panasonic Corporation
- Inventors: Toru SAITO
- Web page: https://patentgrep.com/patent/US20120231589A1

## CPC

- H10D 86/0229: {characterised by control of the annealing or irradiation parameters}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/381: {Beam shaping, e.g. using a mask}
- H10P 14/3814: {Continuous wave laser beam}
- H10P 14/382: {Scanning of a beam}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The following processes are included: preparing a substrate; forming a first gate electrode above the substrate; forming a second gate electrode above the substrate and adjacent to the first gate electrode; forming a gate insulating film on the first gate electrode and the second gate electrode; forming, on the gate insulating film, a noncrystalline semiconductor film at least in a first region above the first gate electrode and a second region above the second gate electrode; irradiating the noncrystalline semiconductor film a laser beam having continuous convex light intensity distributions; and forming a first source electrode and a first drain electrode above the first region, and a second source electrode and a second drain electrode above the second region. In the irradiating, when irradiating the first region with an inner region of the laser beam, the second region is irradiated with an outer region of the laser beam.

## Claims

### Claim 1

A thin-film transistor array device manufacturing method comprising:
preparing a substrate;
forming a first gate electrode above the substrate;
forming a second gate electrode above the substrate and adjacent to the first gate electrode;
forming a gate insulating film on the first gate electrode and the second gate electrode;
forming, on the gate insulating film, a noncrystalline semiconductor film at least in a first region above the first gate electrode and a second region above the second gate electrode;
irradiating the noncrystalline semiconductor film formed in the first region and the second region with a laser beam having continuous convex light intensity distributions in both a short-axis direction and a long-axis direction; and
forming a first source electrode and a first drain electrode above the first region, and a second source electrode and a second drain electrode above the second region,
wherein, in the irradiating, when irradiating the first region of the noncrystalline semiconductor film with an inner region of the laser beam, the second region is irradiated with an outer region of the laser beam which is a region outside of the inner region, continuous from the inner region, and with a light intensity lower than the light intensity of the inner region.

### Claim 2 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the first region is irradiated with the inner region of the laser beam such that the noncrystalline semiconductor film in the first region is heated to a temperature equal to or above a melting point of a crystalline semiconductor film obtained by crystallizing the noncrystalline semiconductor film, and
the second region is irradiated with the outer region of the laser beam such that the noncrystalline semiconductor film in the second region is heated to a temperature below the melting point of the crystalline semiconductor film.

### Claim 3 (depends on 2)

The thin-film transistor array device manufacturing method according to claim 2,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the second region is irradiated with the outer region of the laser beam such that the noncrystalline semiconductor film in the second region is heated to a temperature equal to or above the melting point of the noncrystalline semiconductor film.

### Claim 4 (depends on 2)

The thin-film transistor array device manufacturing method according to claim 2,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the second region is irradiated with the outer region of the laser beam such that the noncrystalline semiconductor film in the second region is heated to a temperature below a melting point of the noncrystalline semiconductor film and equal to or above a crystal growth temperature of the noncrystalline semiconductor film.

### Claim 5 (depends on 2)

The thin-film transistor array device manufacturing method according to claim 2,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the second region is irradiated with the outer region of the laser beam such that the noncrystalline semiconductor film in the second region is heated to a temperature equal to or below a crystal growth temperature of the noncrystalline semiconductor film.

### Claim 6 (depends on 2)

The thin-film transistor array device manufacturing method according to claim 2,
wherein the irradiating includes
crystallizing the noncrystalline semiconductor film by cooling the noncrystalline semiconductor film in the first region after heating the noncrystalline semiconductor film.

### Claim 7 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the noncrystalline semiconductor film formed in the first region is crystallized into a first crystalline semiconductor film having crystal grains of a first average crystal grain size, and
the noncrystalline semiconductor film formed in the second region is crystallized into a second crystalline semiconductor film having crystal grains of a second average crystal grain size smaller than the first average crystal grain size.

### Claim 8 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein, when maximum light intensity in at least one of the light intensity distributions of the laser beam is 100%,
the inner region is a region of light intensity from 77% to 100%.

### Claim 9 (depends on 7)

The thin-film transistor array device manufacturing method according to claim 7,
wherein the first average crystal grain size is from 60 nm to 1 μm.

### Claim 10 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein, when maximum light intensity in at least one of the light intensity distributions of the laser beam is 100%,
the outer region is a region of light intensity from 61% to 77%.

### Claim 11 (depends on 3)

The thin-film transistor array device manufacturing method according to claim 3,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the noncrystalline semiconductor film formed in the second region is crystallized into a second crystalline semiconductor film having an average crystal grain size from 40 nm to 60 nm.

### Claim 12 (depends on 3)

The thin-film transistor array device manufacturing method according to claim 3,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the second region is irradiated with the outer region of the laser beam such that the noncrystalline semiconductor film in the second region is heated to a temperature equal to or above 1100° C. and below 1414° C., and the noncrystalline semiconductor film in the second region is crystallized after a supercooled liquid state.

### Claim 13 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein, when maximum light intensity in at least one of the light intensity distributions of the laser beam is 100%,
the outer region is a region of light intensity from 44% to 61%.

### Claim 14 (depends on 4)

The thin-film transistor array device manufacturing method according to claim 4,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the noncrystalline semiconductor film formed in the second region is crystallized into a second crystalline semiconductor film having an average crystal grain size from 25 nm to 35 nm.

### Claim 15 (depends on 4)

The thin-film transistor array device manufacturing method according to claim 4,
wherein, when irradiating the noncrystalline semiconductor film with the laser beam,
the second region is irradiated with the outer region of the laser beam such that the temperature of the noncrystalline semiconductor film is equal to or above 600° C. and below 1100° C., and crystals grow by solid-phase growth in the noncrystalline semiconductor film in the second region.

### Claim 16 (depends on 7)

The thin-film transistor array device manufacturing method according to claim 7,
wherein the first crystalline semiconductor film and the second crystalline semiconductor film are spaced apart.

### Claim 17 (depends on 16)

The thin-film transistor array device manufacturing method according to claim 16,
wherein a boundary portion between the first crystalline semiconductor film and the second crystalline semiconductor film is removed by patterning.

### Claim 18 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein the continuous convex light intensity distributions are Gaussian distributions.

### Claim 19 (depends on 1)

The thin-film transistor array device manufacturing method according to claim 1,
wherein the laser irradiation is performed on the noncrystalline semiconductor film in an order of microseconds.