# US 2012/0231580 A1 · Method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0231580 A1
- Document ID: US20120231580A1
- Status: Published application
- Kind: A1
- Application number: 13/413,684
- Filed: 2012-03-07
- Published: 2012-09-13
- Earliest claimed: 2011-03-11
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Shunpei YAMAZAKI; Yuhei SATO; Keiji SATO; Tetsunori MARUYAMA; Junichi KOEZUKA
- Web page: https://patentgrep.com/patent/US20120231580A1

## CPC

- H10P 95/50: {Alloying conductive materials with semiconductor bodies}
- H10D 30/031: {of thin-film transistors [TFT]}
- H10D 30/6755: {Oxide semiconductors, e.g. zinc oxide, copper aluminium oxide or cadmium stannate}
- H10D 86/423: {comprising semiconductor materials not belonging to the Group IV, e.g. InGaZnO}
- H10D 86/60: wherein the TFTs are in active matrices
- H10D 99/00: Subject matter not provided for in other groups of this subclass
- H10P 14/27: {using selective deposition, e.g. simultaneous growth of monocrystalline and non-monocrystalline semiconductor materials}
- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10P 14/38: {characterised by treatments done after the formation of the materials}
- H10P 14/6319: {Formation by plasma treatments, e.g. plasma oxidation of the substrate}
- H10P 14/6939: {characterised by the metal}
- H10P 32/12: between a solid phase and a gaseous phase
- H10P 32/17: {characterised by the semiconductor material}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D 30/0312: {characterised by the gate electrodes}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In a manufacturing process of a transistor including an oxide semiconductor film, oxygen doping treatment is performed on the oxide semiconductor film, and then heat treatment is performed on the oxide semiconductor film and an aluminum oxide film provided over the oxide semiconductor film. Consequently, an oxide semiconductor film which includes a region containing more oxygen than a stoichiometric composition is formed. The transistor formed using the oxide semiconductor film can have high reliability because the amount of change in the threshold voltage of the transistor by a bias-temperature stress test (BT test) is reduced.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising the steps of:
forming an oxide film;
forming an oxide semiconductor film on the oxide film;
forming an aluminum oxide film over the oxide semiconductor film so that the aluminum oxide film is in contact with part of the oxide semiconductor film; and
performing heat treatment on the oxide semiconductor film and the aluminum oxide film.

### Claim 2 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the oxide film is a silicon oxide film.

### Claim 3 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the oxide semiconductor film comprises indium, gallium, and zinc.

### Claim 4 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the heat treatment is performed at a temperature of higher than or equal to 350° C. and lower than or equal to 650° C.

### Claim 5 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the oxide film and the oxide semiconductor film are successively formed without exposure to air.

### Claim 6 (depends on 1)

The method of manufacturing a semiconductor device according to claim 1, wherein the oxide semiconductor film comprises a crystalline region.

### Claim 7

A method of manufacturing a semiconductor device, the method comprising the steps of:
forming an oxide film;
forming an oxide semiconductor film on the oxide film;
forming an aluminum oxide film over the oxide semiconductor film so that the aluminum oxide film is in contact with part of the oxide semiconductor film;
adding oxygen into the oxide semiconductor film so that a region of the oxide semiconductor film comprises more oxygen than a stoichiometric composition; and
performing heat treatment on the oxide semiconductor film and the aluminum oxide film after adding the oxygen.

### Claim 8 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein the oxide film is a silicon oxide film.

### Claim 9 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein the oxide semiconductor film comprises indium, gallium, and zinc.

### Claim 10 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein the heat treatment is performed at a temperature of higher than or equal to 350° C. and lower than or equal to 650° C.

### Claim 11 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein the oxide film and the oxide semiconductor film are successively formed without exposure to air.

### Claim 12 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein a peak of a concentration of oxygen in the oxide semiconductor film into which the oxygen is added is higher than or equal to 1×1018/cm3 and lower than or equal to 3×1021/cm3.

### Claim 13 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein the oxide semiconductor film comprises a crystalline region.

### Claim 14

A method of manufacturing a semiconductor device, the method comprising the steps of:
forming an oxide film;
forming an oxide semiconductor film on the oxide film;
performing first heat treatment on the oxide semiconductor film to remove a hydrogen atom from the oxide semiconductor film;
forming an aluminum oxide film over the oxide semiconductor film after performing the first heat treatment so that the aluminum oxide film is in contact with part of the oxide semiconductor film;
adding oxygen into the oxide semiconductor film after performing the first heat treatment so that a region of the oxide semiconductor film comprises more oxygen than a stoichiometric composition; and
performing second heat treatment on the oxide semiconductor film and the aluminum oxide film after adding the oxygen.

### Claim 15 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the oxide film is a silicon oxide film.

### Claim 16 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the oxide semiconductor film comprises indium, gallium, and zinc.

### Claim 17 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the first heat treatment is performed at a temperature of higher than or equal to 250° C. and lower than or equal to 700° C.

### Claim 18 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the second heat treatment is performed at a temperature of higher than or equal to 350° C. and lower than or equal to 650° C.

### Claim 19 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the oxide film and the oxide semiconductor film are successively formed without exposure to air.

### Claim 20 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein a peak of a concentration of oxygen in the oxide semiconductor film into which the oxygen is added is higher than or equal to 1×1018/cm3 and lower than or equal to 3×1021/cm3.

### Claim 21 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the oxide semiconductor film comprises a crystalline region.