# US 2012/0231569 A1 · Optoelectronic component with three-dimension quantum well structure and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0231569 A1
- Document ID: US20120231569A1
- Status: Published application
- Kind: A1
- Application number: 13/473,924
- Filed: 2012-05-17
- Published: 2012-09-13
- Earliest claimed: 2010-02-01
- Assignees: Hermes-Epitek Corporation
- Inventors: BENSON CHAO; CHUNG-HUA FU; SHIH-CHIEH JANG
- Web page: https://patentgrep.com/patent/US20120231569A1

## CPC

- H10P 50/00: Etching of wafers, substrates or parts of devices
- H10H 20/80: Constructional details
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An optoelectronic component with three-dimension quantum well structure and a method for producing the same are provided, wherein the optoelectronic component comprises a substrate, a first semiconductor layer, a transition layer, and a quantum well structure. The first semiconductor layer is disposed on the substrate. The transition layer is grown on the first semiconductor layer, contains a first nitride compound semiconductor material, and has at least a texture, wherein the texture has at least a first protrusion with at least an inclined facet, at least a first trench with at least an inclined facet and at least a shoulder facet connected between the inclined facets. The quantum well structure is grown on the texture and shaped by the protrusion, the trench and the shoulder facet.

## Claims

### Claim 1

A method for producing an optoelectronic component with three-dimension quantum well structure, comprising:
A. growing a transition layer on a first semiconductor layer disposed on a substrate, wherein said transition layer contains a first nitride compound semiconductor material and has at least a texture, said texture has at least a protrusion with at least an inclined facet, at least a trench with at least an inclined facet and at least a shoulder facet connected between said inclined facets;
B. growing a quantum well structure on at least one of said inclined facets; and
C. growing a second semiconductor layer on said quantum well structure, wherein said second semiconductor layer contains a second nitride compound semiconductor material with opposite conduction type to said first nitride compound semiconductor material.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein said step A comprises:
A1. applying a first mask layer to said first semiconductor layer, wherein said first mask layer has at least a first opening exposing a part of said first semiconductor layer;
A2. growing a semiconductor material layer on said part of said first semiconductor layer, wherein said semiconductor material layer has said trench with one of said inclined facets;
A3. removing said first mask layer to expose remaining said semiconductor layer;
A4. applying a second mask layer to previous said semiconductor material layer, wherein said second mask layer has at least a second opening exposing a part of previous said semiconductor material layer;
A5. growing another semiconductor material layer having said protrusion with another one of said inclined facets on said part of previous said semiconductor material layer; and
A6. removing said second mask layer to expose previous said semiconductor material layer, so as to form said shoulder facet.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein said steps A4 to A6 are repeated in sequence more than one time to form more than two said semiconductor material layers respectively having said protrusion or said trench stacked to one another.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein said step A comprises:
A1. growing a semiconductor material layer on said first semiconductor layer;
A2. applying a first mask layer to said semiconductor material layer, wherein said first mask layer has at least a first opening exposing a part of said semiconductor material layer;
A3. etching said part of said semiconductor material layer to form said trench with one of said inclined facets;
A4. removing said first mask layer to expose remaining said semiconductor material layer;
A5. applying a second mask layer to previous said semiconductor material layer, wherein said second mask layer has at least a second opening exposing a part of previous said semiconductor material layer;
A6. growing another semiconductor material layer having said protrusion with another one of said inclined facets on said part of previous said semiconductor material layer; and
A7. removing said second mask layer to expose previous said semiconductor material layer, so as to form said shoulder facet.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein said steps A5 to A7 are repeated in sequence more than one time to form more than two said semiconductor material layers respectively having said protrusion or said trench stacked to one another.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein a slope of each of said inclined facets is adjusted by a growth speed of corresponding said semiconductor material layer.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein said inclined facets are parallel to one another.

### Claim 8

A method for producing an optoelectronic component with three-dimension quantum well structure, comprising:
A. growing a transition layer on a buffer layer disposed on a substrate;
B. applying a first mask layer to said transition layer, wherein said first mask layer has at least a first opening exposing a part of said transition layer;
C. etching said transition layer from said first opening to form a trench;
D. removing said first mask layer;
E. applying a second mask layer to said transition layer, wherein said second mask layer has at least a second opening exposing a different part of said transition layer adjacent to said trench;
F. growing a protrusion over said second opening;
G. removing said second mask layer to expose said trench and said protrusion; and
H. forming at least a pair of quantum well structures on said trench and said protrusion.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein said protrusion is away from said trench at a distance.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein a shoulder facet is connected between an inclined facet of said protrusion and an inclined facet of said trench when said first mask layer and said second layer are removed.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein a slope of said inclined facet of said protrusion is adjusted by a growth speed of said protrusion.

### Claim 12 (depends on 10)

The method as claimed in claim 10, wherein said inclined facets are parallel to one another.

### Claim 13 (depends on 8)

The method as claimed in claim 8, further comprising growing a semiconductor layer on said pair of quantum well structures, wherein said transition layer contains a first nitride compound semiconductor material and said second semiconductor layer contains a second nitride compound semiconductor material with opposite conduction type to said first nitride compound semiconductor material.

### Claim 14 (depends on 8)

The method as claimed in claim 8, further comprising processing the following steps in sequence at least one time between the steps G and H:
applying a third mask layer to said transition layer and said protrusion, wherein said third mask layer has at least a third opening exposing a part of said protrusion;
growing another protrusion over said third opening; and
removing said third mask layer to expose said trench and said protrusions.