# US 2012/0231365 A1 · Method for mechanically stabilizing nitrogen-containing polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0231365 A1
- Document ID: US20120231365A1
- Status: Published application
- Kind: A1
- Application number: 13/509,432
- Filed: 2010-11-12
- Published: 2012-09-13
- Earliest claimed: 2009-11-14
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Oliver Gronwald; Jörg Belack; Jochen Baurmeister; Thomas Justus Schmidt; Seongwoo Choi; Jung Ock Park; Woo Sung Jeon; Jung Seok Yi
- Web page: https://patentgrep.com/patent/US20120231365A1

## CPC

- H01M 8/0289: Means for holding the electrolyte (solid polymer electrolytes H01M8/1018)
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for the production of mechanically stabilized polyazole polymers, comprising the following steps: a) providing a membrane comprising i.) polyazoles with at least one amino group in a repeating unit except the ones obtainable by reacting aromatic and/or heteroaromatic diaminocarboxylic acids, ii.) at least one strong acid and iii.) at least one stabilizing reagent, the total content of stabilizing reagents in the membrane being within the range of from 0.01 to 30% by weight, b) performing the stabilization reaction in the membrane, immediately or in a subsequent processing step of the membrane, c) if appropriate, additionally doping the membrane obtained in accordance with step b) with a strong acid or concentrating the present strong acid further by removal of present water, wherein the stabilizing agent comprises at least one oxazine-based compound. The polyazole polymer membranes thus obtainable are in particular characterized by a high conductivity and a very good mechanical stability. Therefore, they are in particular suited for applications in fuel cells.

## Claims

### Claim at position 1

1-20. (canceled)

### Claim 21

A method for the production of mechanically stabilized polyazole polymers, comprising the following steps:
a) providing a membrane comprising
i.) polyazoles with at least one amino group in a repeating unit except the ones obtainable by reacting aromatic and/or heteroaromatic diaminocarboxylic acids,
ii.) at least one strong acid and
iii.) at least one stabilizing reagent, the total content of stabilizing reagents in the membrane being within the range of from 0.01 to 30% by weight,
b) performing the stabilization reaction in the membrane, immediately or in a subsequent processing step of the membrane,
c) optionally, additionally doping the membrane obtained in accordance with step b) with a strong acid or concentrating the present strong acid further by removal of present water,
wherein the stabilizing agent comprises at least one oxazine-based compound.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the method comprises the steps of:
a1-a) producing a film comprising polyazoles with at least one amino group in a repeating unit,
a1-b) treating the film from step a) with a solution comprising (i) at least one strong acid and (ii) at least one stabilizing reagent, the total content of stabilizing reagents in the solution being within the range of from 0.01 to 30% by weight.

### Claim 23 (depends on 21)

The method according to claim 21, wherein the method comprises the steps of:
a2-a) producing a solution comprising
i.) polyazoles with at least one amino group in a repeating unit,
ii.) at least one strong acid and
iii.) at least one stabilizing reagent, the total content of stabilizing reagents in the membrane being within the range of from 0.01 to 30% by weight,
a2-b) producing a membrane using the solution of step a-1).

### Claim 24 (depends on 21)

The method according to claim 21, wherein the polyazole has a molecular weight (measured as the intrinsic viscosity) of at least 1.8 dl/g.

### Claim 25 (depends on 21)

The method according to claim 21, wherein at least one strong, protic acid.

### Claim 26 (depends on 25)

The method according to claim 25, wherein at least one strong, protic acid, is based on phosphoric acid and/or sulphuric acid.

### Claim 27 (depends on 26)

The method according to claim 26, wherein, the phosphoric acid comprises polyphosphoric acid, phosphonic acid (H3PO3), orthophosphoric acid (H3PO4), pyrophosphoric acid (H4P2O7), triphosphoric acid (H5P3O10), metaphosphoric acid.

### Claim 28 (depends on 26)

The method according to claim 26, wherein, the phosphoric acid comprises polyphosphoric acid, phosphonic acid (H3PO3), orthophosphoric acid (H3PO4), pyrophosphoric acid (H4P2O7), triphosphoric acid (H5P3O10), metaphosphoric acid, cyclic organophosphoric acids and their derivatives.

### Claim 29 (depends on 21)

The method according to claim 21, wherein a first benzoxazine-based monomer represented by Formula 1 and/or a second benzoxazine-based monomer represented by Formula 2 and/or a polymer thereof is used
wherein
R1 to R4 are each independently hydrogen, a substituted or unsubstituted C1-C20 alkyl group, a substituted or unsubstituted C1-C20 alkoxy group, a substituted or unsubstituted C2-C20 alkenyl group, a substituted or unsubstituted C2-C20 alkynyl group, a substituted or unsubstituted C6-C20 aryl group, a substituted or unsubstituted C6-C20 aryloxy group, a substituted or unsubstituted C2-C20 heteroaryl group, a substituted or unsubstituted C2-C20 heteroaryloxy group, a substituted or unsubstituted C4-C20 cycloalkyl group, a substituted or unsubstituted C4-C20 cycloalkyloxy group, a substituted or unsubstituted C2-C20 heterocycle group, a halogen atom, a hydroxyl group, or a cyano group;
R5 is a halogenated C1-C20 alkyl group, a halogenated C1-C20 alkoxy group, a halogenated C2-C20 alkenyl group, a halogenated C2-C20 alkynyl group, a halogenated C6-C20 aryl group, a halogenated C6-C20 aryloxy group, a halogenated C7-C20 arylalkyl group, a halogenated C2-C20 heteroaryl group, a halogenated C2-C20 heteroaryloxy group, a halogenated C2-C20 heteroarylalkyl group, a halogenated C4-C20 carbocycle group, a halogenated C4-C20 carbocyclicalkyl group, a halogenated C2-C20 heterocycle group, or a halogenated C2-C20 heterocyclicalkyl group;
R5′ is a substituted or unsubstituted C1-C20 alkyl group, a substituted or unsubstituted C1-C20 alkoxy group, a substituted or unsubstituted C2-C20 alkenyl group, a substituted or unsubstituted C2-C20 alkynyl group, a substituted or unsubstituted C6-C20 aryl group, a substituted or unsubstituted C6-C20 aryloxy group, a substituted or unsubstituted C7-C20 arylalkyl group, a substituted or unsubstituted C2-C20 heteroaryl group, a substituted or unsubstituted C2-C20 heteroaryloxy group, a substituted or unsubstituted C2-C20 heteroarylalkyl group, a substituted or unsubstituted C4-C20 carbocycle group, a substituted or unsubstituted C4-C20 carbocyclicalkyl group, a substituted or unsubstituted C2-C20 heterocycle group, or a substituted or unsubstituted C2-C20 heterocyclicalkyl group; R6 is selected from the group consisting of a substituted or unsubstituted C1-C20 alkylene group, a substituted or unsubstituted C2-C20 alkenylene group, a substituted or unsubstituted C2-C20 alkynylene group, a substituted or unsubstituted C6-C20 arylene group, a substituted or unsubstituted C2-C20 heteroarylene group, —C(═O)—, and —SO2—.

### Claim 30 (depends on 21)

The method according to claim 21, wherein a first benzoxazine-based monomer represented by Formula 1 below and/or a second benzoxazine-based monomer represented by Formula 2 below and/or a polymer thereof are used
where, R1 is a hydrogen atom, a substituted or unsubstituted C1-C20 alkyl group, a substituted or unsubstituted C2-C20 alkenyl group, a substituted or unsubstituted C2-C20 alkynyl group, a substituted or unsubstituted C6-C20 aryl group, a substituted or unsubstituted C2-C20 heteroaryl group, a substituted or unsubstituted C4-C20 cycloalkyl group or a substituted or unsubstituted C2-C20 heterocyclic group, a halogen atom, a hydroxy group, or a cyano group;
R2 is a substituted or unsubstituted C1-C20 alkyl group, a substituted or unsubstituted C2-C20 alkenyl group, a substituted or unsubstituted C2-C20 alkynyl group, a substituted or unsubstituted C6-C20 aryl group, a substituted or unsubstituted C7-C20 arylalkyl group, a substituted or unsubstituted C2-C20 heteroaryl group, a substituted or unsubstituted C3-C20 heteroarylalkyl group, a substituted or unsubstituted C4-C20 carbocyclic group, a substituted or unsubstituted C5-C20 carbocyclic alkyl group, a substituted or unsubstituted C2-C20 heterocyclic group, or a substituted or unsubstituted C3-C20 heterocyclic alkyl group;
R3, is a substituted or unsubstituted C1-C20 alkylene group, a substituted or unsubstituted C2-C20 alkenylene group, a substituted or unsubstituted C2-C20 alkynylene group, a substituted or unsubstituted C6-C20 arylene group, a substituted or unsubstituted C2-C20 heteroarylene group, —C(═O)—, or —SO2—.

### Claim 31 (depends on 21)

The method according to claim 21, wherein a benzoxazine-based compound represented by Formula 1 and/or a polymer thereof is used
wherein R1 and R2 are each independently a C1-C20 alkyl group, a C1-C20 alkoxy group, a C6-C20 aryl group, a C6-C20 aryloxy group or a group represented by the formula below,
wherein R3 is a hydrogen atom, a C1-C20 alkyl group, a C1-C20 alkoxy group, a C6-C20 aryl group, a C6-C20 aryloxy group, a halogenated C6-C20 aryl group, a halogenated C6-C20 aryloxy group, a C1-C20 heteroaryl group, a C1-C20 heteroaryloxy group, a halogenated C1-C20 heteroaryl group, a halogenated C1-C20 heteroaryloxy group, a C4-C20 cycloalkyl group, a halogenated C4-C20 cycloalkyl group, a C1-C20 heterocyclic group or a halogenated C1-C20 heterocyclic group.

### Claim 32 (depends on 21)

The method according to claim 21, wherein a benzoxazine-based monomer represented by Formula 1 and/or a polymer thereof is used
wherein
A, B, C, D and E are carbon, or one or two of A, B, C, D and E is nitrogen and the others are carbon, and
R1 and R2 are connected to each other to form a ring, wherein the ring is a C6-C10 cycloalkyl group, a C3-C10 heteroaryl group, a fused C3-C10 heteroaryl group, a C3-C10 heterocyclic group or a fused C3-C10 heterocyclic group.

### Claim 33 (depends on 21)

The method according to claim 21, wherein a phosphorous containing monomer represented by Formula 1 and/or a polymer thereof is used
wherein A is a substituted or unsubstituted C1-C20 heterocycle group, a substituted or unsubstituted C4-C20 cycloalkyl group, or a substituted or unsubstituted C1-C20 alkyl group, and
R2 and R3 are each independently hydrogen, a C1-C20 alkyl group, a C1-C20 alkoxy group, a C6-C20 aryl group, a C6-C20 aryloxy group, a C1-C20 heteroaryl group, a C1-C20 heteroaryloxy group, a C4-C20 cycloalkyl group, a C1-C20 heterocycle group, a halogen atom, a cyano group, or a hydroxyl group,
the monomer comprises at least one oxazine-based moiety.

### Claim 34 (depends on 21)

The method according to claim 21, wherein a naphthoxazine benzoxazine-based monomer represented by Formula 1 below and/or a polymer thereof is used
wherein R2 and R3 or R3 and R4 are linked to each other to form a group represented by Formula 2 below,
R5 and R6 or R6 and R7 are linked to each other to form a group represented by Formula 2 below, and
wherein R1 is a substituted or unsubstituted C1-C20 alkyl group, a substituted or unsubstituted C1-C20 alkoxy group, a substituted or unsubstituted C2-C20 alkenyl group, a substituted or unsubstituted C2-C20 alkynyl group, a substituted or unsubstituted C6-C20 aryl group, a substituted or unsubstituted C6-C20 aryloxy group, a substituted or unsubstituted C7-C20 arylalkyl group, a substituted or unsubstituted C2-C20 heteroaryl group, a substituted or unsubstituted C2-C20 heteroaryloxy group, a substituted or unsubstituted C2-C20 heteroarylalkyl group, a substituted or unsubstituted C4-C20 carbocycle group, a substituted or unsubstituted C4-C20 carbocyclic alkyl group, a substituted or unsubstituted C2-C20 heterocycle group, or a substituted or unsubstituted C2-C20 heterocyclic alkyl group.

### Claim 35 (depends on 21)

The method according to claim 21, wherein a benzoxazine-based monomer represented by Formula 1 and/or a polymer thereof is used
wherein
at least one of R1, R1′, R1″, and R2 is a halogen atom, a halogenated C1-C20 alkyl group, a halogenated C1-C20 alkoxy group, a halogenated C2-C20 alkenyl group, a halogenated C2-C20 alkynyl group, a halogenated C6-C20 aryl group, a halogenated C6-C20 aryloxy group, a halogenated C2-C20 heteroaryl group, a halogenated C2-C20 heteroaryloxy group, a halogenated C4-C20 cycloalkyl group, or a halogenated C2-C20 heterocyclic group;
another one of R1, R1′, R1″, and R2 is a substituted or unsubstituted non-halogenated C2-C20 heterocyclic group;
and any remaining ones of R1, R1′, R1″, and R2 are hydrogen.

### Claim 36 (depends on 21)

The method according to claim 21, wherein this has a modulus of elasticity of at least 3 MPa.

### Claim 37 (depends on 21)

A membrane, obtained in accordance with the method according to claim 21.

### Claim 38 (depends on 37)

The membrane according to claim 37, wherein it has a solubility of less than 0.5% by weight of polyazole polymer in 99% phosphoric acid over a temperature range of from 85° C. to 120° C.

### Claim 39 (depends on 37)

A membrane electrode assembly, comprising at least one membrane according to claim 37.

### Claim 40 (depends on 39)

A fuel cell comprising at least one membrane electrode assembly according to claim 39.