# US 2012/0231173 A1 · Ceramic Coating Deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0231173 A1
- Document ID: US20120231173A1
- Status: Published application
- Kind: A1
- Application number: 13/043,948
- Filed: 2011-03-09
- Published: 2012-09-13
- Earliest claimed: 2011-03-09
- Assignees: United Technologies Corporation
- Inventors: Igor V. Belousov; Yuriy G. Kononenko; Anatoly Kuzmichev; Leonid Shaginyan; Michael J. Maloney; John F. Mullooly, JR.
- Web page: https://patentgrep.com/patent/US20120231173A1

## CPC

- C23C 14/30: by electron bombardment
- C23C 14/086: {of zinc, germanium, cadmium, indium, tin, thallium or bismuth}
- C23C 14/32: by explosion; by evaporation and subsequent ionisation of the vapours {, e.g. ion-plating}(C23C14/34 - C23C14/48 take precedence)
- C23C 14/54: Controlling or regulating the coating process
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A material is applied to a part. The part is placed in a deposition chamber and a first electric potential is applied to the part. Components are evaporated for forming the material. The evaporated components are ionized. The first electric potential is modulated so as to draw the ionized component to the part. The modulation comprises a plurality of first steps for PA-PVD. Each of the first steps comprises a series of pulses of negative potential. The modulation further comprises a plurality of second steps for PVD alternating with the first steps.

## Claims

### Claim 1

A method for applying a material to a part, the method comprising:
placing the part in a deposition chamber;
applying a first electric potential to the part;
evaporating components for forming the material;
ionizing the evaporated components; and
modulating the first electric potential so as to draw the ionized components to the part,
wherein the modulating comprises:
a plurality of first steps for PA-PVD, each comprising a series of pulses of negative potential; and
a plurality of second steps for PVD alternating with the first steps.

### Claim 2 (depends on 1)

The method of claim 1 wherein:
a pulse width τi is ≦10−3s;
a duty cycle D of the pulses is 0.1≦D≦0.99;
a pause between the pulses τp≧0.5×10−6s;
a duration T1 of each first step is 10≦T1≦1000 s; and
a duration T2 of each second step is 10≦T2>1000 s.

### Claim 3 (depends on 1)

The method of claim 1 wherein in at least one of the first steps:
a nominal voltage of the negative pulses is 0.5-10 kV; and
a pulse repetition frequency of the pulses is 0.05-1000 kHz.

### Claim 4 (depends on 3)

The method of claim 3 wherein in said at least one of the first steps:
the nominal voltage is 3-5 kV for a majority of the pulses;
the pulse repetition frequency is 0.5-5 kHz for a majority of the pulses; and
a duty cycle is 0.8-0.9 for a majority of the pulses.

### Claim 5 (depends on 1)

The method of claim 1 wherein the modulating comprises a stage in which:
a magnitude of the pulses increases across several of the first stages

### Claim 6 (depends on 5)

The method of claim 5 wherein:
the magnitude increases by 50-500% relative to the first pulse of the first stage.

### Claim 7 (depends on 1)

The method of claim 1 wherein the modulating comprises a stage in which:
a magnitude of the pulses increases progressively within at least one of the first stages.

### Claim 8 (depends on 7)

The method of claim 7 wherein:
the magnitude increases by 50-500% relative to the first pulse of the first stage.

### Claim 9 (depends on 1)

The method of claim 1 wherein the modulating comprises a stage in which:
a duty cycle of the pulses increases progressively within at least one of the first stages.

### Claim 10 (depends on 9)

The method of claim 9 wherein:
the duty cycle increases by 50-900%.

### Claim 11 (depends on 1)

The method of claim 1 wherein:
the part is a superalloy turbine part and the material is YSZ.

### Claim 12 (depends on 1)

The method of claim 1 wherein:
the ionizing is modulated.

### Claim 13 (depends on 1)

The method of claim 1 wherein the material is applied to a thickness of at least 0.05-1.0 mm.

### Claim 14

A method for applying a material to a part, the method comprising:
placing the part in a deposition chamber;
applying a first electric potential to the part;
evaporating components for forming a TBC material;
ionizing the evaporated components and the reactive gas; and
modulating the first electric potential so as to draw the ionized components to the part,
wherein the modulating comprises:
a plurality of first intervals, each comprising a series of pulses of negative potential; and
a plurality of second intervals alternating with the first intervals and each comprising the first potential being essentially zero voltage.

### Claim 15

An apparatus for depositing material on a workpiece comprising:
a deposition chamber;
deposition material at least partially within the deposition chamber;
a first electron beam source, positioned to direct a first electron beam to vaporize a portion of the deposition material;
an ionizing system positioned to ionize the vaporized material and the reactive gas;
a bias voltage source connected to apply an electric potential to the workpiece; and
a control apparatus coupled to the bias voltage source and configured to apply said electric potential in:
a plurality of first steps for PAPVD, each comprising a series of pulses of negative potential; and
a plurality of second steps for PVD alternating with the first steps.

### Claim 16 (depends on 15)

The apparatus of claim 15 wherein:
the control apparatus is configured to progressively increase a magnitude of the pulses within at least one of the first steps.

### Claim 17 (depends on 15)

The apparatus of claim 15 further comprising:
a crucible containing the deposition material; and
an inductor over the crucible.

### Claim 18 (depends on 15)

The apparatus of claim 15 further comprising:
a plasma generator having electrodes and plasma generating oxygen gas source having an outlet directing the plasma-generating oxygen gas toward the substrate.

### Claim 19 (depends on 15)

The apparatus of claim 15 further comprising:
an arc discharge plasma generator having electrodes formed from the deposition material.

### Claim 20

The apparatus of 19 further comprising an arc discharge plasma generator having:
a ceramic electrode (286); and
a heater (290) for heating the ceramic electrode up to temperature of ceramic electrical conductivity appearance.