# US 2012/0231152 A1 · Methods for preparing a coating solution for producing a transparent conductive film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0231152 A1
- Document ID: US20120231152A1
- Status: Published application
- Kind: A1
- Application number: 13/281,182
- Filed: 2011-10-25
- Published: 2012-09-13
- Earliest claimed: 2011-03-07
- Inventors: Jyung-Dong LIN; Cho-Liang Chung; Ming-Wuu Hsu; Yi-Hsuan Ho
- Web page: https://patentgrep.com/patent/US20120231152A1

## CPC

- H01B 1/22: the conductive material comprising metals or alloys
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

A method for preparing a coating solution for producing a transparent conductive film includes dissolving a zinc precursor and a metal salt with a solvent to form a first solution containing the zinc precursor and a second solution containing the metal salt. The first solution is mixed with the second solution. At least one stabilizer is added into a mixture of the first and second solutions to form a coating solution precursor. The coating solution precursor is heated and stirred until even dissolution of the zinc precursor and the metal salt. The heated and stirred coating solution precursor is placed steadily in an environment having a temperature lower than a room temperature to undergo crystal growth, obtaining a raw coating solution. The raw coating solution is then filtered to obtain a coating solution.

## Claims

### Claim 1

A method for preparing a coating solution for producing a transparent conductive film, comprising:
a preparing step including: dissolving a zinc precursor and a metal salt with a solvent to form a first solution containing the zinc precursor and a second solution containing the metal salt, mixing the first solution with the second solution, and adding at least one stabilizer into a mixture of the first and second solutions to form a coating solution precursor;
a crystal growing step including: heating and stirring the coating solution precursor until even dissolution of the zinc precursor and the metal salt, and steadily placing the heated and stirred coating solution precursor in an environment having a temperature lower than a room temperature to undergo crystal growth, obtaining a raw coating solution; and
a filtering step including: filtering the raw coating solution to obtain a coating solution.

### Claim 2 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, further comprising a treating step after the filtering step, with the treating step including: submerging a substrate in the coating solution and pulling the substrate out of the coating solution after a surface of the substrate is coated with the coating solution.

### Claim 3 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, wherein the temperature of the environment is in a range of 5-23° C.

### Claim 4 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, wherein the coating solution precursor is steadily placed in the environment for 3-30 days in the crystal growing step.

### Claim 5 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, wherein the raw coating solution is filtered with a 0.5 μm mesh in the filtering step to remove crystalline grains having diameters larger than 0.5 μm from the raw coating solution.

### Claim 6 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, with the concentration of zinc precursor in the first solution being 0.1-1M, with the concentration of metal salt in the second solution being 0.1-10 wt %, with a final concentration of said at least one stabilizer in the coating solution precursor being 0.1-2M.

### Claim 7 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, with said at least one stabilizer is selected from the group consisting of monoethanolamine, diethanolamine, triethanolamine, and combinations thereof.

### Claim 8 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, wherein the zinc precursor is zinc acetate dehydrate or zinc acetate anhydrous.

### Claim 9 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, wherein the metal salt is aluminum nitrate or gallium nitrate.

### Claim 10 (depends on 1)

The method for preparing a coating solution for producing a transparent conductive film as claimed in claim 1, wherein the solvent is 2-propanol.