# US 2012/0225959 A1 · Proton-conductive membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0225959 A1
- Document ID: US20120225959A1
- Status: Published application
- Kind: A1
- Application number: 13/039,796
- Filed: 2011-03-03
- Published: 2012-09-06
- Earliest claimed: 2011-03-03
- Assignees: Excellatron Solid State, LLC
- Inventors: James R. Muller; John Scott Flanagan; Timothy Schriefer; Lazbourne A. Allie; Lonnie G. Johnson
- Web page: https://patentgrep.com/patent/US20120225959A1

## CPC

- C08J 5/2275: {Heterogeneous membranes}
- C08K 3/32: Phosphorus-containing compounds
- H01M 8/103: having nitrogen, e.g. sulfonated polybenzimidazoles [S-PBI], polybenzimidazoles with phosphoric acid, sulfonated polyamides [S-PA] or sulfonated polyphosphazenes [S-PPh]
- H01M 8/1048: Ion-conducting additives, e.g. ion-conducting particles, heteropolyacids, metal phosphate or polybenzimidazole with phosphoric acid
- C08J 2379/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- H01M 2008/1095: {Fuel cells with polymeric electrolytes}
- Y02E 60/50: Fuel cells
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An anhydrous, proton-conductive medium comprises a poly(amic acid)-based polyimide and at least one phosphorus compound from the group consisting of phosphorus oxides and phosphoric acids. The precursor solution for the polyimide is a mixture of a phosphorus oxide and a poly(amic acid). A suitable phosphorus oxide has the formula P4O10. A process for forming an anhydrous, proton-conductive membrane comprises mixing a phosphorus oxide in a poly(amic acid) solution to form a mixture, dispensing the mixture upon a support structure, and substantially drying the mixture. The mixture may then be cured.

## Claims

### Claim 1

An anhydrous, proton-conductive medium comprising a poly(amic acid)-based polyimide polymer and at least one phosphorus compound from the group consisting of phosphorus oxides and phosphoric acids.

### Claim 2 (depends on 1)

The anhydrous, proton-conductive medium of claim 1, wherein said phosphorus oxides have a formula PxOy, wherein x=1 to 4 and y=4 to 10.

### Claim 3 (depends on 1)

The anhydrous, proton-conductive medium of claim 1, wherein said phosphoric acids have a formula HO(P(O)(OH)O)nH where n is a positive integer.

### Claim 4 (depends on 1)

The anhydrous, proton-conductive medium of claim 1, wherein said phosphoric acids have a formula HO(P(O)(OH)O)nH where n=1 to 10.

### Claim 5 (depends on 1)

The anhydrous, proton-conductive medium of claim 1, wherein said phosphoric acids have a formula HO(P(O)(OH)O)nH where n=1 to 4.

### Claim 6 (depends on 1)

The anhydrous, proton-conductive medium of claim 1, wherein said phosphoric acids comprise trimetaphosphoric acid.

### Claim 7

An anhydrous, proton-conductive medium comprising a phosphorus-oxide-doped poly(amic acid)-based polyimide polymer substrate.

### Claim 8 (depends on 7)

The anhydrous, proton-conductive medium of claim 7, wherein said poly(amic acid) is an aromatic poly(amic acid).

### Claim 9 (depends on 7)

The anhydrous, proton-conductive medium of claim 7, wherein said poly(amic acid) is an aliphatic poly(amic acid).

### Claim 10 (depends on 7)

The anhydrous, proton-conductive medium of claim 7, wherein said phosphorus oxide has the formula PxOy, with x=1 to 4 and y=4 to 10.

### Claim 11 (depends on 7)

The anhydrous, proton-conductive medium of claim 7, wherein said phosphorus oxide has the formula P4O10.

### Claim 12

An anhydrous, proton-conductive medium formed by a process comprising:
mixing a phosphorus oxide in a poly(amic acid) solution to form a mixture;
dispensing said mixture upon a support structure; and
substantially drying said mixture.

### Claim 13 (depends on 12)

The anhydrous, proton-conductive medium of claim 12, further comprising curing said mixture after drying.

### Claim 14 (depends on 12)

The anhydrous, proton-conductive medium of claim 12, wherein said poly(amic acid) is an aromatic poly(amic acid).

### Claim 15 (depends on 12)

The anhydrous, proton-conductive medium of claim 12, wherein said poly(amic acid) is an aliphatic poly(amic acid).

### Claim 16 (depends on 12)

The anhydrous, proton-conductive medium of claim 12, wherein said phosphorus oxide has the formula PxOy, with x=1 to 4 and y=4 to 10.

### Claim 17 (depends on 12)

The anhydrous, proton-conductive medium of claim 12, wherein said phosphorus oxide has the formula P4O10.

### Claim 18 (depends on 12)

The anhydrous, proton-conductive medium of claim 12, wherein the step of mixing a phosphorus oxide in a poly(amic acid) solution to form a mixture comprises first pre-dissolving said phosphorus oxide in a poly(amic acid)-compatible solvent.

### Claim 19 (depends on 18)

The anhydrous, proton-conductive medium of claim 18, wherein said poly(amic acid)-compatible solvent is chosen from the group consisting of N-methylpyrrolidone, N,N-dimethylformamide, N,N-dimethylacetamide and M-ethylpyrrolidone.

### Claim 20 (depends on 18)

The anhydrous, proton-conductive medium of claim 18, wherein said poly(amic acid)-compatible solvent comprises N-methylpyrrolidone.

### Claim 21 (depends on 18)

The anhydrous, proton-conductive medium of claim 18, wherein said poly(amic acid)-compatible solvent comprises a precursor solvent from which said poly(amic acid) has been formed.

### Claim 22

A process for forming an anhydrous, proton-conductive medium, the process comprising
mixing a phosphorus oxide in a poly(amic acid) solution to form a mixture;
dispensing said mixture upon a support structure; and
substantially drying said mixture.

### Claim 23 (depends on 22)

The process of claim 22, further comprising curing said mixture after drying.

### Claim 24 (depends on 22)

The process of claim 22, further comprising mixing said phosphorus oxide and said poly(amic acid) with a poly(amic acid)-compatible solvent to form said mixture.

### Claim 25 (depends on 22)

The process of claim 22, wherein said poly(amic acid) is an aromatic poly(amic acid).

### Claim 26 (depends on 22)

The process of claim 22, wherein said poly(amic acid) is an aliphatic poly(amic acid).

### Claim 27 (depends on 22)

The process of claim 22, wherein said phosphorus oxide has the formula PxOy, with x=1 to 4 and y=4 to 10.

### Claim 28 (depends on 22)

The process of claim 22, wherein said phosphorus oxide has the formula P4O10.

### Claim 29 (depends on 22)

The process of claim 22, wherein the step of mixing a phosphorus oxide in a poly(amic acid) solution to form a mixture comprises first pre-dissolving said phosphorus oxide in a poly(amic acid)-compatible solvent.

### Claim 30 (depends on 29)

The process of claim 29, wherein said poly(amic acid)-compatible solvent is chosen from the group consisting of N-methylpyrrolidone, N,N-dimethylformamide, N,N-dimethylacetamide and N-ethylpyrrolidone.

### Claim 31 (depends on 29)

The process of claim 29, wherein said poly(amic acid)-compatible solvent comprises N-methylpyrrolidone.

### Claim 32 (depends on 29)

The process of claim 29, wherein said poly(amic acid)-compatible solvent comprises a solvent from which said poly(amic acid) has been formed.