Stainless steel flux-cored wire
AssigneeKabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsHiroshi SUGAHARA, Tetsunao Ikeda, Hirohisa Watanabe
Life of this patent
Estimating the term…
Loading patent…
AssigneeKabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.)
InventorsHiroshi SUGAHARA, Tetsunao Ikeda, Hirohisa Watanabe
Estimating the term…
It is an object to provide a stainless steel flux-cored wire in which the amount of hexavalent chromium in fume can be reduced while maintaining the weldability excellent. The stainless steel flux-cored wire contains, as percentage to the total mass of the wire: Cr: 11-30 mass %; metal Si, Si oxide and Si compound: 0.5-4.0 mass % in total in terms of Si [Si]; fluorine compound: 0.01-1.0 mass % in terms of F [F]; TiO2: 1.5 mass % or above; ZrO2+Al2O3: 3.2 mass % or below; Na compound, K compound and Li compound: 0.50 mass % or below in total of each of an amount in terms of Na [Na], an amount in terms of K [K] and an amount in terms of Li [Li]; and satisfies {([Na]+[K]+[Li])×[Cr]2}/([Si]+4.7×[F])≦10, where [Cr] represents Cr content.
A flux-cored wire for arc welding filled up with flux in an outer sheath made of stainless steel containing, as percentage to the total mass of the wire:
Dependencies are inferred from the claim text.