# US 2012/0223050 A1 · Production of a security element provided with colored micro-depressions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0223050 A1
- Document ID: US20120223050A1
- Status: Published application
- Kind: A1
- Application number: 13/509,071
- Filed: 2010-11-04
- Published: 2012-09-06
- Earliest claimed: 2009-11-11
- Assignees: Giesecke & Devrient GmbH
- Inventors: Mario Keller
- Web page: https://patentgrep.com/patent/US20120223050A1

## CPC

- B42D 25/29: Securities; Bank notes
- B42D 25/328: Diffraction gratings; Holograms
- B42D 25/42: by photographic processes
- B42D 25/425: by deformation, e.g. embossing
- B42D 25/43: by removal of material
- B42D 25/324: Reliefs
- B42D 25/373: Metallic materials
- B42D 25/378: Special inks
- B42D 25/47: using adhesives
- B42D 2033/10
- B42D 2033/20
- B42D 2035/24
- B42D 2035/44
- B42D: BOOKS; BOOK COVERS; LOOSE LEAVES; PRINTED MATTER CHARACTERISED BY IDENTIFICATION OR SECURITY FEATURES; PRINTED MATTER OF SPECIAL FORMAT OR STYLE NOT OTHERWISE PROVIDED FOR; DEVICES FOR USE THEREWITH AND NOT OTHERWISE PROVIDED FOR; MOVABLE-STRIP WRITING OR READING APPARATUS

## Abstract

A method for producing a security element having microdepressions for security papers, with the microdepressions being colored with a certain color, involves the steps of (a) coating an upper side of a carrier with an embossable layer; (b1) forming microdepressions in the embossable layer to configure an embossed layer; (c) applying the certain color on the upper side, so that the color remains in the microdepressions; (b2) applying a structured protective layer on the coated upper side, wherein the structured protective layer does not cover the microdepressions that are to be colored with the certain color, after step (b1) and before step (c); and removing the structured protective layer and thereby a color toning after step (c).

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A method for producing a security element having microdepressions that are colored with a certain color comprising the following steps:
a) coating an upper side of a carrier with an embossable layer,
b1) forming microdepressions in the embossable layer to configure an embossed layer,
b2) applying a protective layer on the embossable layer, wherein the protective layer is structured so that it does not cover the microdepressions that are to be colored with the certain color,
c) applying the certain color on the carrier upper side, in a manner such that the color remains in the microdepressions as a filling,
d) removing the structured protective layer and thereby any color toning present outside the microdepressions , with the color filling being limited to the micro depressions.

### Claim 14 (depends on 13)

The method according to claim 13, wherein step b2) a structured protective layer is applied that has a window in which the microdepressions are disposed.

### Claim 15 (depends on 14)

The method according to claim 14, wherein
before step b2) the coated upper side is metalized,
in step b2) the structured protective layer is applied, with the protective layer being configured so that it protects the metalization from etching, and
after applying the structured protective layer, the metalization that is not protected by the protective layer and is disposed in the window is etched so as to demetalize the microdepressions.

### Claim 16 (depends on 15)

The method according to claim 15, wherein
in step b1) or before step b2), hologram structures are also formed in the embossable layer, with the hologram structures being metalized and provided with the protective layer and, after step d),
e) outside the hologram structures the upper side is provided with a protective coating and
f) areas of the hologram structures that are not provided with the protective coating are demetalized by etching.

### Claim 17 (depends on 13)

The method according to claim 13, wherein, in step b2), for applying the structured protective layer, first a separating layer is incorporated in the microdepressions, then the protective layer is applied and, through removal of the protective layer disposed in the microdepressions, the part of the protective layer which is disposed above the microdepressions is also detached and the protective layer is thereby structured.

### Claim 18 (depends on 13)

The method according to claim 13, wherein the upper side or a lower side of the carrier is provided with an adhesive layer.

### Claim 19 (depends on 13)

The method according to claim 13, wherein the upper side or a lower side of the carrier is provided with a primer print.

### Claim 20 (depends on 13)

The method according to claim 13, wherein in step c), a kiss print is used to apply color.

### Claim 21 (depends on 13)

The method according to claim 13, wherein, in step c) for color application on the upper side, color is applied over the surface and excess color is scraped off

### Claim 22 (depends on 13)

The method according to claim 13, wherein as protective layer a washing ink or a resist lacquer is used.

### Claim 23 (depends on 13)

The method according to claim 13, wherein as separating layer a washing ink or a resist lacquer is used.

### Claim 24 (depends on 13)

The method according to claim 13, wherein the steps b2) to d) are repeated with a further color that differs from the certain color, with the protective layer being structured differently in the steps (b2).

### Claim 25 (depends on 13)

The method according to claim 13, wherein the microdepressions have a depth of between 1.5 and 3.5 μm.