# US 2012/0222830 A1 · Method for producing paper or the like

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0222830 A1
- Document ID: US20120222830A1
- Status: Published application
- Kind: A1
- Application number: 13/509,373
- Filed: 2010-11-03
- Published: 2012-09-06
- Earliest claimed: 2009-11-13
- Assignees: Applied Chemicals Handels-GmbH
- Inventors: Alexander Frank
- Web page: https://patentgrep.com/patent/US20120222830A1

## CPC

- D21H 17/41: containing ionic groups
- D21H 17/63: Inorganic compounds
- D21H 21/10: Retention agents or drainage improvers
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

In a method for manufacturing paper or the like, in which cationic polymer microparticles comprised of polyacrylamide and a fine-particle inorganic component are added to the paper pulp following the final shearing step and prior to the headbox, whereupon the paper pulp is subjected to dehydration while forming sheets, followed by sheet drying, a polymer mixture comprising a linear cationic polymer and a linear anionic copolymer, whose overall ionicity is anionic, is additionally added immediately prior to the headbox.

## Claims

### Claim 1

A method for manufacturing paper or the like, in which cationic polymers comprised of polyacrylamide and a fine-particle inorganic component are added to the paper pulp following the final shearing step and prior to the headbox, whereupon the paper pulp is subjected to dehydration while forming sheets, followed by sheet drying, characterized in that an alkali-activated bentonite having a silicon dioxide content of less than 2% by weight, in particular an alkali-activated bentonite essentially completely consisting of montmorrillonite, is used as said fine-particle inorganic component and that a polymer mixture comprising a linear cationic polymer, namely a polydiallyl dimethyl ammonium chloride having a cationic charge of about 6 mol per kg dry product and a linear anionic copolymer, whose overall ionicity is anionic, namely a copolymer of acrylamide and sodium acrylate at a molar ratio of acrylamide to sodium acrylate of 50:50 to 70:30 and an anionic charge of about 4 mol per kg dry product, is additionally added immediately prior to the headbox.

### Claim 2 (depends on 1)

The method according to claim 1, characterized in that the linear cationic polymer is used at a particle size, in the non-swollen state, of less than 2 μm.

### Claim 3 (depends on 1)

The method according to claim 1, characterized in that a linear anionic copolymer having a particle size, in the non-swollen state, of between 30 and 250 μm is used.

### Claim 4 (depends on 1)

The method according to claim 1, characterized in that the proportion of the linear cationic polymer to the linear anionic copolymer in the polymer mixture ranges between 2:8 and 0.5:9.5.

### Claim 5 (depends on 1)

The method according to claim 1, characterized in that the polymer mixture is used as a suspension in oil and, in particular, in a mixture of isoparaffin oil, technical white oil, sorbitan monooleate as well as, optionally, additives like a stabilizer such as, e.g., a hydrophobically modified acrylic copolymer, a polymer-activating, surface-active material such as, e.g., a synthetic condensate of a primary alcohol and ethylene oxide as well as further additives selected from 2,2′-azobis(2-methylbutyronitrile), urea, or a sodium salt of diethylenetriamine pentacetic acid.

### Claim 6 (depends on 1)

The method according to claim 1, characterized in that the polymers contained in the polymer mixture are water-soluble.

### Claim 7 (depends on 1)

The method according to claim 1, characterized in that the polyacrylamide to be added following the final shearing step is used as a dispersion or emulsion in oil.

### Claim 8 (depends on 1)

The method according to claim 1, characterized in that bentonite having an internal surface area of at least 400 m2/g, particularly 600 to 850 m2/g, and a mean particle size of less than 2 μm is used as said alkali-activated bentonite.

### Claim 9 (depends on 1)

The method according to claim 1, characterized in that a bentonite having a negative surface charge and a positive edge charge is used as said alkali-activated bentonite.

### Claim 10 (depends on 7)

The method according to claim 7, characterized in that the alkali-activated bentonite is used with a pH in the suspension of at least 7.8, in particular at least 8.

### Claim 11 (depends on 1)

A The method according to claim 1, characterized in that the cationic polyacrylamide is at first added to the paper pulp, and the bentonite and, at the same time, the polymer mixture are added immediately prior to the headbox.

### Claim 12

(canceled)

### Claim 13

(canceled)

### Claim 14

(canceled)