Method for manufacturing basalt fiber
AssigneesNakagawa Sangyo Co., Ltd., Toyota Jidosha Kabushiki Kaisha
InventorsSumio Kamiya, Hironori Sasaki, Noriaki Nakagawa
Life of this patent
Estimating the term…
Loading patent…
AssigneesNakagawa Sangyo Co., Ltd., Toyota Jidosha Kabushiki Kaisha
InventorsSumio Kamiya, Hironori Sasaki, Noriaki Nakagawa
Estimating the term…
Basalt filament is manufactured such that the fiber diameter can be controlled and the filament is not severed during winding. A network former and a glass modifier are formed and maintained with respect to basalt rock ore, and the crystallization and binding of basalt fiber are inhibited, the heat-resistance property of basalt fiber is greatly improved from the conventional 750° C. to 850 or 900° C., and significant cost reduction is achieved over conventional products. The method includes: grinding basalt rock as a material; washing a resultant ground rock; melting the ground rock that has been washed; transforming a molten product into fiber; and drawing the fiber in an aligned manner, and winding it. The temperature of the molten product in the melting step is 1400 to 1650° C., and log η is 2.15 to 2.35 dPa·s and preferably 2.2 to 2.3 dPa·s, where η is the viscosity of the molten product.
1-9. (canceled)
Basalt filament manufactured by a method for manufacturing, comprising the steps of:
Dependencies are inferred from the claim text.