# US 2012/0075769 A1 · High temperature high current metalized film capacitor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0075769 A1
- Document ID: US20120075769A1
- Status: Published application
- Kind: A1
- Application number: 12/893,696
- Filed: 2010-09-29
- Published: 2012-03-29
- Earliest claimed: 2010-09-29
- Inventors: Edward M. Lobo; Paul Winsor, IV
- Web page: https://patentgrep.com/patent/US20120075769A1

## CPC

- H01G 4/32: Wound capacitors
- H01G 4/008: Selection of materials
- H01G 4/18: of synthetic material, e.g. derivatives of cellulose (H01G4/16 takes precedence)
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A rolled film capacitor includes a first dielectric layer of high crystallinity polypropylene and a first metalized electrode stack adjacent to and contacting the first dielectric layer. The first metalized electrode stack includes a first substrate located between first and second metallic films. The capacitor also includes a second dielectric layer of high crystallinity polypropylene, and a second metalized electrode stack adjacent to and contacting the second dielectric layer, the second metalized electrode stack comprising a second substrate located between third and fourth metallic films.

## Claims

### Claim 1

A rolled film capacitor, comprising:
a first dielectric layer of polypropylene having a crystallinity above 60%;
a first metalized electrode stack adjacent to and contacting the first dielectric layer, the first metalized electrode stack comprising a first substrate located between first and second metallic films;
a second dielectric layer of polypropylene having a crystallinity above 60%; and
a second metalized electrode stack adjacent to and contacting the second dielectric layer, the second metalized electrode stack comprising a second substrate located between third and fourth metallic films.

### Claim 2 (depends on 1)

The film capacitor of claim 1, where the first dielectric layer has a crystallinity of at least about 63%.

### Claim 3 (depends on 1)

The film capacitor of claim 1, where the second dielectric layer has a crystallinity of at least about 63%.

### Claim 4 (depends on 2)

The film capacitor of claim 2, where the first substrate comprises polyethylene terephthalate (PET).

### Claim 5 (depends on 4)

The film capacitor of claim 4, where the first metallic film comprises aluminum.

### Claim 6 (depends on 4)

The film capacitor of claim 4, where the first metallic film comprises zinc.

### Claim 7 (depends on 1)

The film capacitor of claim 1, where the first dielectric layer has a crystallinity of at least about 62%.

### Claim 8 (depends on 1)

The film capacitor of claim 1, where the second dielectric layer has a crystallinity of at least about 62%.

### Claim 9 (depends on 1)

The film capacitor of claim 1, where the first dielectric layer has a crystallinity of at least about 64%.

### Claim 10 (depends on 1)

The film capacitor of claim 1, where the second dielectric layer has a crystallinity of at least about 64%.

### Claim 11 (depends on 1)

The film capacitor of claim 1, where the first dielectric layer has a crystallinity of at least about 65%.

### Claim 12 (depends on 1)

The film capacitor of claim 1, where the second dielectric layer has a crystallinity of at least about 65%.

### Claim 13 (depends on 1)

The film capacitor of claim 1, where the first dielectric layer has a crystallinity of at least about 67%.

### Claim 14 (depends on 1)

The film capacitor of claim 1, where the second dielectric layer has a crystallinity of at least about 67%.

### Claim 15 (depends on 1)

The film capacitor of claim 1, where the first metallic film has a thickness of about 200-300 Angstroms.

### Claim 16

A rolled film capacitor, comprising:
a first dielectric film of high crystallinity polypropylene having an isotacticity great than about 98%;
a first metalized electrode stack adjacent to and contacting the first dielectric film, the first metalized electrode stack comprising a first substrate located between first and second metallic films;
a second dielectric film of high crystallinity polypropylene; and
a second metalized electrode adjacent to and contacting the second dielectric film, the second metalized electrode comprising a second substrate located between third and fourth metallic films.

### Claim 17

A rolled film capacitor, comprising:
a first dielectric layer of polypropylene having a crystallinity above 50%;
a first metalized electrode stack adjacent to and contacting the first dielectric layer, the first metalized electrode stack comprising a first substrate located between first and second metallic films;
a second dielectric layer of polypropylene having a crystallinity above 50%; and
a second metalized electrode stack adjacent to and contacting the second dielectric layer, the second metalized electrode stack comprising a second substrate located between third and fourth metallic films.

### Claim 18 (depends on 17)

The film capacitor of claim 17, where the first dielectric layer has a crystallinity of at least about 53%.

### Claim 19 (depends on 17)

The film capacitor of claim 17, where the second dielectric layer has a crystallinity of at least about 53%.

### Claim 20 (depends on 18)

The film capacitor of claim 18, where the first substrate comprises polyethylene terephthalate (PET).

### Claim 21 (depends on 20)

The film capacitor of claim 20, where the first metallic film comprises aluminum.

### Claim 22 (depends on 20)

The film capacitor of claim 20, where the first metallic film comprises zinc.

### Claim 23 (depends on 17)

The film capacitor of claim 17, where the first dielectric layer has a crystallinity of at least about 52%.

### Claim 24 (depends on 17)

The film capacitor of claim 17, where the second dielectric layer has a crystallinity of at least about 52%.

### Claim 25 (depends on 17)

The film capacitor of claim 17, where the first dielectric layer has a crystallinity of at least about 54%.

### Claim 26 (depends on 17)

The film capacitor of claim 17, where the second dielectric layer has a crystallinity of at least about 54%.

### Claim 27 (depends on 17)

The film capacitor of claim 17, where the first dielectric layer has a crystallinity of at least about 55%.

### Claim 28 (depends on 17)

The film capacitor of claim 17, where the second dielectric layer has a crystallinity of at least about 55%.

### Claim 29 (depends on 17)

The film capacitor of claim 17, where the first dielectric layer has a crystallinity of at least about 57%.

### Claim 30 (depends on 17)

The film capacitor of claim 17, where the second dielectric layer has a crystallinity of at least about 57%.

### Claim 31 (depends on 17)

The film capacitor of claim 17, where the first metallic film has a thickness of about 200-300 Angstroms.