# US 2012/0075629 A1 · Particle analysis for corrosion rate monitoring

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0075629 A1
- Document ID: US20120075629A1
- Status: Published application
- Kind: A1
- Application number: 13/214,480
- Filed: 2011-08-22
- Published: 2012-03-29
- Earliest claimed: 2010-09-27
- Assignees: ConocoPhillips Company
- Inventors: Omar Jesus YEPEZ; Ricky Eugene SNELLING
- Web page: https://patentgrep.com/patent/US20120075629A1

## CPC

- G01N 5/04: by removing a component, e.g. by evaporation, and weighing the remainder
- G01N 15/0205: by optical means
- G01N 17/006: {of metals}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

Methods and apparatus relate to measuring corrosion rate. Corrosive fluid contacts a metal powder altering physical properties of the metal powder due to resulting corrosion thereof. For example, the corrosion diminishes mass of the metal powder reducing particle size and particle surface area of the metal powder. Since these physical properties of the metal powder are indicative of the corrosion rate, analysis of the metal powder provides the corrosion rate based on difference in the property of the metal powder before and after the contact with the corrosive fluid.

## Claims

### Claim 1

A method, comprising:
contacting a metal powder with a corrosive liquid, wherein the metal powder has an average particle size less than 100 microns;
measuring a property of the metal powder to provide a measurement taken after the contacting of the metal powder with the corrosive liquid; and
determining a corrosion rate of the metal powder within the corrosive liquid based on a difference between the measurement and an initial value for the property before the contacting of the metal powder with the corrosive liquid.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the property is surface area of the metal powder.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the property is particle size distribution of the metal powder.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the determining of the corrosion rate is based on time of the contacting, surface area calculated from the property that is indicative of particle size, and weight change calculated using density of material forming the powder and change in the particle size determined from the difference in the measurement and the initial value.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the corrosive liquid includes naphthenic acid.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the metal powder includes iron.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the metal powder is made of iron and the corrosive liquid is a hydrocarbon containing naphthenic acid.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the metal powder has an average particle size between 5 and 10 microns.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the determining of the corrosion rate includes calibration of the difference between the measurement and the initial value for the property indicative of surface area to known changes in the surface area for given corrosion rates.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the measuring of the property includes analysis of light scattering through a suspension containing the metal powder.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising filtering, rinsing and drying the metal powder after the contacting of the metal powder with the corrosive liquid and then mixing the metal powder in a dispersing medium for measuring of the property.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising disposing the metal powder within a heated interior of an autoclave where the metal powder during the contacting is exposed to the corrosive liquid above ambient pressure.

### Claim 13 (depends on 1)

The method according to claim 1, wherein total contact time between the metal powder and the corrosive liquid is less than two hours.

### Claim 14

A method, comprising:
contacting a metal powder with a corrosive liquid;
measuring particle sizes of the metal powder by light diffraction analysis after the contacting of the metal powder with the corrosive liquid; and
determining a corrosion rate of the metal powder within the corrosive liquid utilizing an initial value for the particle sizes and a measurement obtained by the measuring of the particle sizes to assess change of the metal powder caused by corrosion.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the change of the metal powder caused by corrosion is surface area reduction.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the change of the metal powder caused by corrosion is reduction in average particle size.

### Claim 17 (depends on 14)

The method according to claim 14, wherein the determining of the corrosion rate includes a determination of weight change of the metal powder before and after the contacting and calculated using density of material forming the powder and difference in particle size distribution defined by the measurement and the initial value.

### Claim 18

A method, comprising:
contacting a metal powder with a corrosive liquid;
analyzing the metal powder contacted with the corrosive liquid to provide a measurement for surface area of the metal powder obtained as a function of particle size distribution; and
determining a corrosion rate of the metal powder within the corrosive liquid utilizing an initial value for the surface area before the contacting of the metal powder with the corrosive liquid and the measurement of the surface area.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the analyzing of the metal powder includes analysis of light scattering through a suspension containing the metal powder.

### Claim 20 (depends on 18)

The method according to claim 18, wherein the determining of the corrosion rate includes calibration of the difference between the measurement and the initial value for the surface area to known changes in the surface area for given corrosion rates.