# US 2012/0074405 A1 · Process for the Simultaneous Deposition of Crystalline and Amorphous Layers with Doping

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0074405 A1
- Document ID: US20120074405A1
- Status: Published application
- Kind: A1
- Application number: 13/314,595
- Filed: 2011-12-08
- Published: 2012-03-29
- Earliest claimed: 2008-04-21
- Assignees: Infineon Technologies AG
- Inventors: Herbert Schäfer; Martin Franosch; Thomas Meister; Josef Böck
- Web page: https://patentgrep.com/patent/US20120074405A1

## CPC

- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3441: {Conductivity type}
- H10P 14/3602: {In-situ cleaning}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

One embodiment of the present invention relates to method for the concurrent deposition of multiple different crystalline structures on a semiconductor body utilizing in-situ differential epitaxy. In one embodiment of the present invention a preparation surface is formed, resulting in two distinct crystalline regions, a monocrystalline silicon substrate region and an isolating layer region. A monocrystalline silicon layer and an amorphous silicon layer are concurrently formed directly onto the preparation surface in the monocrystalline silicon substrate region and the isolating layer region, respectively. Deposition comprises the formation of two or more sub-layers. The process parameters can be varied for each individual sub-layer to optimize deposition characteristics.

## Claims

### Claim 1

A method for the concurrent deposition of multiple crystalline structures on a semiconductor body by means of in-situ differential epitaxy, comprising:
forming a preparation surface associated with a semiconductor body, the preparation surface having a first region comprising monocrystalline silicon substrate and a second region comprising an isolating layer; and
forming two or more sub-layers, each using different process parameters, to concurrently provide a monocrystalline silicon layer having two or more sub-layers directly on the preparation surface in the first region and an amorphous silicon layer having two or more sub-layers directly on the preparation surface in the second region.

### Claim 2 (depends on 1)

The method of claim 1, wherein formation of the two or more sub-layers comprises:
depositing a first sub-layer directly on the preparation surface in the first and second region;
depositing a second sub-layer over the first sub-layer; and
depositing a third sub-layer over the second sub-layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the first sub-layer is deposited at a first pressure, the second sub-layer is deposited at a second pressure, and the third sub-layer is deposited at a third pressure.

### Claim 4 (depends on 3)

The method of claim 3, wherein the first pressure and the third pressure are constant.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first pressure is less than the third pressure, and wherein the second pressure varies between the first pressure and the third pressure.

### Claim 6 (depends on 5)

The method of claim 5, further comprising placing the semiconductor body in a deposition chamber located within a deposition system, wherein the deposition system guarantees that O2 and H2O partial pressures within the deposition chamber are so low that defect free monocrystalline growth is possible.

### Claim 7 (depends on 6)

The method of claim 6, further comprising providing a carrier gas within the deposition chamber, wherein the carrier gas comprises one of hydrogen (H2). argon (Ar), helium (He) or nitrogen (N).

### Claim 8 (depends on 7)

The method of claim 7, further comprising providing a doping gas within the deposition chamber, wherein the doping gas comprises one of arsine (AsH3), phosphine (PH3), or diborane (B2H6).

### Claim 9 (depends on 8)

The method of claim 8, further comprising providing a methylsilane gas within the deposition chamber, wherein the methylsilane gas achieves a carbon doping of the monocrystalline silicon layer and the amorphous silicon layer.

### Claim 10 (depends on 1)

The method of claim 1, wherein forming the preparation surface further comprises a third region comprising a polycrystalline silicon substrate, and wherein a polycrystalline silicon layer is formed directly on the preparation surface in the third region concurrently with forming the monocrystalline silicon layer and the amorphous silicon layer.

### Claim 11 (depends on 1)

The method of claim 1, wherein the isolating layer comprises an oxide or an oxynitride layer.

### Claim 12 (depends on 1)

The method of claim 1, further comprising performing in-situ annealing in hydrogen (H2) on the semiconductor body prior to concurrently forming the monocrystalline and amorphous silicon layers, wherein performing in-situ annealing in H2 removes oxygen from the first region of the preparation surface to form a monocrystalline oxygen-free silicon surface.

### Claim 13 (depends on 12)

The method of claim 12, further comprising performing a wet chemical etch prior performing in-situ annealing in H2 to remove a native oxide layer from the surface of the semiconductor body.

### Claim 14

A method for the concurrent deposition of two crystalline structures on a semiconductor body, comprising;
preparing the semiconductor body to have a monocrystalline silicon substrate region and an isolating layer region;
performing in-situ annealing in hydrogen (H2) on the semiconductor body to remove oxygen from the monocrystalline silicon substrate;
concurrently depositing a first sub-layer over the monocrystalline silicon substrate region and the isolating layer region at a constant first pressure following performance of in-situ annealing in H2;
concurrently depositing a second sub-layer over the monocrystalline silicon substrate region and the isolating layer region at a variable second pressure greater than the first pressure following deposition of the first sub-layer; and
concurrently depositing a third sub-layer over the monocrystalline silicon substrate region and the isolating layer region at a constant third pressure greater than the second pressure following the deposition of the second sub-layer;
wherein the first, second, and third sub-layers collectively form an amorphous silicon layer over the isolating layer region and a monocrystalline silicon layer over the monocrystalline silicon substrate region.

### Claim 15 (depends on 14)

The method of claim 14, further comprising providing a methylsilane gas within the deposition chamber, wherein the methylsilane gas achieves a carbon doping of the first, second, and third sub-layers.

### Claim 16 (depends on 14)

The method of claim 14, wherein the isolating layer region comprises an oxide or an oxynitride layer.

### Claim 17 (depends on 14)

The method of claim 14, further comprising an additional temperature step to convert the amorphous silicon layer into a converted polycrystalline layer.

### Claim 18 (depends on 14)

The method of claim 14, wherein the ratio of the thickness of the monocrystalline silicon layer to the thickness of the amorphous silicon layer is between 2:1 and 2:2.

### Claim 19

A method for the concurrent deposition of three crystalline structures on a semiconductor body, comprising:
preparing the semiconductor body to have a monocrystalline silicon substrate region, an isolating layer region, and a polycrystalline silicon substrate region;
performing in-situ annealing in hydrogen (H2) on the semiconductor body to remove oxygen from the monocrystalline silicon substrate;
concurrently depositing a first sub-layer over the monocrystalline silicon substrate region, the isolating layer region, and the polycrystalline silicon substrate region at a constant first pressure following performance of in-situ annealing in H2;
concurrently depositing a second sub-layer over the monocrystalline silicon substrate region, the isolating layer region, and the polycrystalline silicon substrate region following deposition of the first sub-layer; and
concurrently depositing a third sub-layer over the monocrystalline silicon substrate region, the isolating layer region, and the polycrystalline silicon substrate region at a constant third pressure following the deposition of the second sub-layer;
wherein the first pressure is less than the third pressure, and wherein the second sub-layer is deposited at a second pressure that varies between the first pressure and the third pressure;
and wherein the first, second, and third sub-layers collectively form an amorphous silicon layer over the isolating layer region and a monocrystalline silicon layer over the monocrystalline silicon substrate region, and a polycrystalline silicon layer over the polycrystalline silicon substrate region.

### Claim 20 (depends on 19)

The method of claim 19, further comprising providing a methylsilane gas within the deposition chamber, wherein the methylsilane gas achieves a carbon doping of the first, second, and third sub-layers.

### Claim 21 (depends on 19)

The method of claim 19, wherein the isolating layer region comprises an oxide or an oxynitride layer.

### Claim 22 (depends on 19)

The method of claim 19, further comprising an additional temperature step to convert the amorphous silicon layer into a converted polycrystalline layer, wherein the converted polycrystalline layer has a much lower surface roughness than the polycrystalline silicon layer.

### Claim 23 (depends on 19)

The method of claim 19, wherein the ratio of the thickness of the monocrystalline silicon layer to the thickness of the amorphous silicon layer is between 2:1 and 2:2, wherein the ratio of the thickness of the monocrystalline silicon layer to the thickness of the polycrystalline silicon layer is between 2:1 and 2:2, and wherein the ratio of the thickness of the polycrystalline silicon layer to the thickness of the amorphous silicon layer is greater than 1:1.

### Claim 24

A multi-crystalline structure formed on a semiconductor body, comprising means for:
preparing the semiconductor body to have an oxide or an oxynitride region and a monocrystalline silicon substrate region; and
concurrently forming an amorphous silicon layer directly on the oxide or the oxynitride region, and a monocrystalline silicon layer directly on the monocrystalline silicon substrate region by a process of forming multiple sub-layers at different pressures, wherein the ratio of a thickness of the monocrystalline silicon layer to a thickness of the amorphous silicon layer is between 2:1 and 2:2.

### Claim 25 (depends on 24)

The multi-crystalline structure of claim 24, further comprising means for:
preparing the semiconductor body to have a polysilicon substrate region; and
concurrently forming a polycrystalline silicon layer directly on a polysilicon substrate, wherein the ratio of a thickness of the monocrystalline silicon layer to a thickness of the polycrystalline silicon layer is between 2:1 and 2:2, and wherein the ratio of the thickness of the polycrystalline silicon layer to the thickness of the amorphous silicon layer is greater than 1:1.