# US 2012/0074347 A1 · Infrared attenuated polymeric foam insulation with flame retardant performance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0074347 A1
- Document ID: US20120074347A1
- Status: Published application
- Kind: A1
- Application number: 13/318,365
- Filed: 2010-06-01
- Published: 2012-03-29
- Earliest claimed: 2009-06-04
- Inventors: John Gordon-Duffy
- Web page: https://patentgrep.com/patent/US20120074347A1

## CPC

- C08J 9/0019: {halogenated}
- C08J 9/0023: {containing oxygen}
- C08J 9/0066: {Use of inorganic compounding ingredients}
- C08J 9/127: {Mixtures of organic and inorganic blowing agents}
- C08J 2201/03: Extrusion of the foamable blend
- C08J 2203/06: CO2, N2 or noble gases
- C08J 2203/12: Organic compounds only containing carbon, hydrogen and oxygen atoms, e.g. ketone or alcohol
- C08J 2203/14: Saturated hydrocarbons, e.g. butane; Unspecified hydrocarbons
- C08J 2325/04: Homopolymers or copolymers of styrene
- Y02P 20/10: Process efficiency
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Prepare a polymer foam by extrusion foaming a foamable thermoplastic polymer composition using a blowing agent containing 3 to 5 weight-percent (wt %) carbon dioxide, up to 5 wt % alcohol having 2-3 carbons, up to 0.7 wt % water and up to 2.5 weight-percent iso-butane; wherein the blowing agent comprises at least 0.1 wt % of water and/or alcohol having 2-3 carbons; two to five wt % infrared attenuating agent selected from petcokes and 100-700 nanometers size carbon black; 2.5 to 3.5 wt % brominated flame retardant; and at least 0.1 wt % of epoxy stabilizer wherein the resulting polymeric foam is characterized by having a density in a range of 30 to 37 kilograms per cubic meter, a unimodal cell size distribution, an average cell size of 0.15 to 0.4 millimeters, a thermal conductivity in a range of 28 to 35 milliwatts per meter*Kelvin and that passes the German B2 fire test.

## Claims

### Claim 1

A process for preparing extruded polymeric foam comprising providing a foamable polymer composition at an initial pressure and temperature in an extruder and then extruding the foamable polymer composition into an atmosphere of lower pressure than the initial pressure and allowing the foamable polymer composition to expand into polymeric foam; wherein the foamable polymer composition comprises:
a. a thermoplastic polymer matrix comprising a polymer component that contains all the polymers in the thermoplastic polymer matrix;
b. a blowing agent composition dispersed within the thermoplastic polymer matrix, the blowing agent composition comprising 3 to 5 weight-percent carbon dioxide, up to 5 wt % alcohol having 2-3 carbons, up to 0.7 wt % water and up to 2.5 weight-percent iso-butane; wherein the blowing agent comprises at least 0.1 weight-percent of water and/or alcohol having 2-3 carbons;
c. two weight-percent or more and five weight-percent or less of an infrared attenuating agent dispersed within the thermoplastic polymer matrix, the infrared attenuating agent selected from a group consisting of carbon black having an average particle size of 100-700 nanometers and petcokes;
d. 2.5 to 3.5 weight-percent of a brominated flame retardant dispersed within the thermoplastic polymer matrix; and
e. at least 0.1 weight-percent of epoxy stabilizer dispersed within the polymer matrix;
where all weight-percents are relative to total polymer component weight and wherein the resulting polymeric foam is characterized by having a density in a range of 30 to 37 kilograms per cubic meter, a unimodal cell size distribution with an average cell size in a range of greater than 0.15 and 0.4 millimeters or less, a thermal conductivity in a range of 28 to 35 milliwatts per meter*Kelvin and that passes the German B2 fire test.

### Claim 2 (depends on 1)

The process of claim 1, wherein the infrared attenuating agent comprises at least two weight-percent petcokes, more than two weight-percent carbon black or both.

### Claim 3 (depends on 1)

The process of claim 1, wherein at least 50 weight-percent of the polymer component is alkenyl aromatic polymer.

### Claim 4 (depends on 3)

The process of claim 3, wherein the alkenyl aromatic polymer is polystyrene homopolymer.

### Claim 5 (depends on 1)

The process of claim 1, wherein the blowing agent composition comprises iso-butane in a concentration range of 0.5 to 1.5 weight-percent based on total polymer component weight.

### Claim 6 (depends on 1)

The process of claim 1, wherein the epoxy stabilizer is epoxy cresol novolac.

### Claim 7

A polymeric foam comprising:
a. a thermoplastic polymer matrix comprising a polymer component that contains all the polymers in the thermoplastic polymer matrix and having cells dispersed therein;
b. two weight-percent or more and five weight-percent or less of an infrared attenuating agent dispersed within the thermoplastic polymer matrix, the infrared attenuating agent selected from a group consisting of carbon black having an average particle size of 100-700 nanometers and petcokes;
c. 2.5 to 3.5 weight-percent of a brominated flame retardant dispersed within the thermoplastic polymer matrix; and
d. at least 0.1 weight-percent of epoxy stabilizer dispersed within the polymer matrix;
where weight parts is relative to total polymer component weight and wherein the polymeric foam is characterized by having a density in a range of 30 to 37 kilograms per cubic meter, a unimodal cell size distribution with an average cell size in a range of 0.1 to 0.4 millimeters, a thermal conductivity in a range of 28 to 35 milliwatts per meter*Kelvin and that passes the German B2 fire test.

### Claim 8 (depends on 7)

The polymeric foam of claim 7, wherein the infrared attenuating agent comprises at least two weight-percent petcokes, more than two weight-percent carbon black or both.

### Claim 9 (depends on 7)

The polymeric foam of claim 7, wherein the polymer component is at least 50 weight-percent alkenyl aromatic polymer.

### Claim 10 (depends on 7)

The polymeric foam of claim 7, wherein the alkenyl aromatic polymer is polystyrene homopolymer.

### Claim 11 (depends on 7)

The polymeric foam of claim 7, wherein the epoxy stabilizer is epoxy cresol novolac.

### Claim 12 (depends on 7)

The polymeric foam of claim 7, wherein the polymeric foam has a primary surface and 98-percent or more of any 200 square centimeters portion of the primary surface that is centered on the polymeric foam's primary surface and extending to 80 percent of the foam's width is free of defects.