# US 2012/0074117 A1 · In-situ heating and co-annealing for laser annealed junction formation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0074117 A1
- Document ID: US20120074117A1
- Status: Published application
- Kind: A1
- Application number: 13/238,687
- Filed: 2011-09-21
- Published: 2012-03-29
- Earliest claimed: 2010-09-23
- Assignees: Varian Semiconductor Equipment Associates, Inc.
- Inventors: Deepak Ramappa; Paul Sullivan
- Web page: https://patentgrep.com/patent/US20120074117A1

## CPC

- H10P 14/3808: {using laser beams}
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/0608: {in the same heat affected zone [HAZ] (B23K26/0613, B23K26/0619 take precedence)}
- B23K 26/0619: {with spots located on opposed surfaces of the workpiece}
- B23K 26/354: by melting
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- B23K 2103/56: {being semiconducting}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

Improved methods of annealing a workpiece are disclosed. Lasers are used to both increase the temperature of the workpiece, and to laser melt anneal the workpiece. By utilizing lasers for both operations, the manufacturing complexity is reduced. Furthermore, laser melt anneal may provide better junctions and more well defined junction depths. By heating the workpiece either immediately before or after the laser melt anneal, the quality of the junction may be improved. Shallow annealing may be accomplished and annealing may occur in the presence of a species to form a passivation layer. If the workpiece is a solar cell, in-situ heating may improve open circuit voltage (Voc) or dark currents. Insitu heating of the substrate lowers the melting threshold of the substrate and also increases light absorption in the substrate. This reduces the power of the melt laser and hence reduces the residual damage.

## Claims

### Claim 1

A method of laser melt annealing a workpiece, comprising:
directing an incoming laser beam toward a workpiece;
dividing said incoming laser beam into a first laser beam and a second laser beam using an optical device disposed in a path of said incoming laser beam, wherein said first laser beam has a first wavelength at a first power level, to heat said workpiece and said second laser beam has a second wavelength at a second power level to laser melt anneal said workpiece.

### Claim 2 (depends on 1)

The method of claim 1, wherein said optical device is selected from the group consisting of a lens, prism, mirror and any combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein said optical device divides said incoming laser beam such that said first power level is less than said second power level.

### Claim 4 (depends on 1)

The method of claim 1, wherein said optical device divides said incoming laser beam such that said first laser beam has a greater width than said second laser beam.

### Claim 5 (depends on 1)

The method of claim 1, wherein said first laser beam and said second laser beam are moved relative to said workpiece.

### Claim 6

A method of laser melt annealing a workpiece, comprising:
directing a first laser beam, having a first wavelength at a first power level, toward said workpiece to heat said workpiece; and
directing a second laser beam, at least partially simultaneously with said first laser beam, said second laser beam having a second wavelength at a second power level, toward said workpiece to laser melt anneal said workpiece, wherein said first laser beam and said second laser beam are directed at opposite sides of said workpiece.

### Claim 7 (depends on 6)

The method of claim 6, wherein said first wavelength is longer than said second wavelength.

### Claim 8 (depends on 6)

The method of claim 6, wherein said first power level is less than said second power level.

### Claim 9 (depends on 6)

The method of claim 6, wherein said first laser beam and said second laser beam are moved relative to said workpiece.

### Claim 10

A method of laser melt annealing a workpiece, comprising:
implanting a portion of said workpiece;
directing a first laser beam, having a first wavelength at a first power level, toward said workpiece to heat said portion of said workpiece;
directing a second laser beam, at least partially simultaneously with said first laser beam, said second laser beam having a second wavelength at a second power level, toward said portion of said workpiece to laser melt anneal said workpiece;
and wherein said first laser beam and said second laser beam are moved relative to said workpiece so as to anneal only said implanted portions of said workpiece.

### Claim 11 (depends on 10)

The method of claim 10, wherein said first wavelength is longer than said second wavelength.

### Claim 12 (depends on 10)

The method of claim 10, wherein said first power level is less than said second power level.

### Claim 13

A method of laser melt annealing a workpiece, comprising:
directing a first laser beam, having a first wavelength at a first power level, toward said workpiece to heat said workpiece; and
directing a second laser beam, at least partially simultaneously with said first laser beam, said second laser beam having a second wavelength at a second power level, toward said workpiece to laser melt anneal said workpiece, wherein said first laser beam is directed toward a first side of said workpiece and is reflected back toward said workpiece using a mirror positioned on a second side opposite said first side.

### Claim 14 (depends on 13)

The method of claim 13, wherein said first wavelength is longer than said second wavelength.

### Claim 15 (depends on 13)

The method of claim 13, wherein said first power level is less than said second power level.

### Claim 16 (depends on 13)

The method of claim 13, wherein said first laser beam and said second laser beam are moved relative to said workpiece.