# US 2012/0073407 A1 · Method of recovering metal values from nickel-containing ores

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0073407 A1
- Document ID: US20120073407A1
- Status: Published application
- Kind: A1
- Application number: 13/200,782
- Filed: 2011-09-30
- Published: 2012-03-29
- Earliest claimed: 2007-05-03
- Assignees: Drinkard Metalox, Inc.
- Inventors: William F. Drinkard, JR.; Hans J. Woerner
- Web page: https://patentgrep.com/patent/US20120073407A1

## CPC

- C22B 23/0438: {Nitric acids or salts thereof}
- C22B 23/0469: {by chemical substitution, e.g. by cementation}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An improved method for processing of nickel-bearing ores, particularly saprolite and limonite, to recover the valuable minerals contained therein, comprising leaching the ore with nitric acid to form a slurry; separating the iron values by precipitation, removing the iron values; forming a liquid/solid residue in which nickel, cobalt and magnesium are in solution, and manganese and aluminum, when present, are solid residues in oxide form; conducting a liquid-solid separation and removing the solids; and recovering the nickel, cobalt, and manganese from the liquid-metal concentrate. The leachate is recovered and nitric acid from the leachate is recycled.

## Claims

### Claim 1

A method of recovering metal values from ores containing iron, nickel, cobalt, and magnesium, comprising:
a) leaching the ore with HNO3 for a sufficient time to form a slurry;
b) separating any undissolved residue from the slurry to form a solution:
c) precipitating the iron as Fe2O3.3H2O, and leaving a solution containing nickel and cobalt values;
d) performing thermal hydrolysis, or pH balance (shift), or sulfide precipitation, or solvent extraction to form Ni(OH)2 and Co(OH)2, or NiS and CoS, or Ni/Co salts in solid form, and removing the nickel-cobalt values as a precipitate;
e) recovering HNO3 and NOx from the process; and
f) reforming the removed NOx containing gases into nitric acid for further use.

### Claim 2 (depends on 1)

A method according to claim 1 wherein the leach is carried out at a temperature of 70° C. to 160° C. for a period of time of from about 30 minutes to about 3 hours.

### Claim 3 (depends on 1)

A method according to claim 1 wherein the nitric acid in the leach is a solution of 10 to 90 percent nitric acid.

### Claim 4 (depends on 3)

A method according to claim 3 wherein the nitric acid in the leach is a solution of 30 to 67 percent nitric acid.

### Claim 5 (depends on 1)

A method according to claim 1 wherein the leach step is followed by heating to a temperature of from about 125° C. to about 200° C. to form a liquid/solid residue in which the nickel, cobalt and magnesium values are in solution, and the iron and, manganese values are solid residues in oxide form.

### Claim 6 (depends on 1)

A method according to claim 1, wherein precipitation of iron is accomplished by thermal hydrolysis or by pH balancing of the solution.

### Claim 7 (depends on 1)

A method according to claim 1 wherein the pH balance to form nickel-cobalt salts is accomplished by mixing with the nickel-cobalt solution any of the group consisting of: an alkaline earth hydroxide. an alkaline earth carbonate, an alkaline earth oxide, an alkali metal hydroxide, or an alkali metal carbonate.

### Claim 8 (depends on 1)

A method according to claim 1 wherein the ore is crushed prior to leaching.

### Claim 9 (depends on 1)

A method according to claim 1 wherein the ores are sulfides.

### Claim 10 (depends on 1)

A method according to claim 1 further comprising:
during or after step d), performing thermal hydrolysis, pH balance (pH shift), sulfide precipitation, or solvent extraction to form Ni(OH)2 and Co(OH)2, or NiS and CoS, or Ni/Co salts in solid form, and removing the nickel-cobalt values as a precipitate.

### Claim 11

A method of recovering metal values from ores containing iron, nickel, cobalt, magnesium, and aluminum, comprising:
a) leaching the ore with HNO3 for a sufficient time to form a slurry;
b) separating any undissolved residue to form a solution:
c) precipitating the iron from the solution as Fe2O3.3H2O;
d) precipitating aluminum as Al2O3, and leaving a solution containing nickel and cobalt values;
e) performing thermal hydrolysis, or pH balance (shift), or sulfide precipitation, or solvent extraction to form Ni(OH)2 and Co(OH)2, or NiS and CoS, or Ni/Co salts in solid form, and removing the nickel-cobalt values as a precipitate;
f) recovering HNO3 and NOx from the process; and
g) reforming the removed NOx containing gases into nitric acid for further use.

### Claim 12 (depends on 11)

A method according to claim 11 wherein the leach is carried out at a temperature of 70° C. to 160° C. for a period of time of from about 30 minutes to about 3 hours.

### Claim 13 (depends on 11)

A method according to claim 11 wherein the nitric acid in the leach is a solution of 10 to 90 percent nitric acid.

### Claim 14 (depends on 13)

A method according to claim 13 wherein the nitric acid in the leach is a solution of 30 to 67 percent nitric acid.

### Claim 15 (depends on 11)

A method according to claim 11 wherein the leach step is followed by heating to a temperature of from about 125° C. to about 200° C. to form a liquid/solid residue in which the nickel, cobalt and magnesium values are in solution, and the iron, manganese, and aluminum values are solid residues in oxide form.

### Claim 16 (depends on 11)

A method according to claim 11, wherein precipitation of iron is accomplished by thermal hydrolysis, or by pH balancing of the solution.

### Claim 17 (depends on 1)

A method according to claim 1 wherein the pH balance to form nickel-cobalt salts is accomplished by mixing with the nickel-cobalt solution any of the group consisting of: an alkaline earth hydroxide. an alkaline earth carbonate, an alkaline earth oxide, an alkali metal hydroxide, or an alkali metal carbonate.

### Claim 18 (depends on 11)

A method according to claim 11 wherein the ore is crushed prior to leaching.

### Claim 19 (depends on 11)

A method according to claim 11 wherein the ores are sulfides.

### Claim 20 (depends on 11)

A method according to claim 11, further comprising:
during or after step e), performing thermal hydrolysis, pH balance (pH shift), sulfide precipitation, or solvent extraction to form Ni(OH)2 and Co(OH)2, or NiS and CoS, or Ni/Co salts in solid form, and removing the nickel-cobalt values as a precipitate.

### Claim 21

A method of recovering metal values from sulfide ores containing iron, nickel, cobalt, magnesium, and aluminum, comprising:
a) leaching the ore with HNO3 for a sufficient time to form a slurry;
b) separating any undissolved residue from the slurry to form a solution:
c) precipitating the iron from the solution as Fe2O3.3H2O;
d) precipitating aluminum as Al2O3, and leaving a solution containing nickel and cobalt values;
e) performing thermal hydrolysis, or pH balance (shift), or sulfide precipitation, or solvent extraction to form Ni(OH)2 and Co(OH)2, or NiS and CoS, or Ni/Co salts in solid form, and removing the nickel-cobalt values as a precipitate;
f) recovering HNO3 and NOx from the process; and
g) reforming the removed NOx containing gases into nitric acid for further use.

### Claim 22 (depends on 21)

A method according to claim 21 further comprising: during or after step e), performing thermal hydrolysis, pH balance (pH shift), sulfide precipitation, or solvent extraction to form Ni(OH)2 and Co(OH)2, or NiS and CoS, or Ni/Co salts in solid form, and removing the nickel-cobalt values as a precipitate.