# US 2012/0073210 A1 · Method of grooving a chemical-mechanical planarization pad

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0073210 A1
- Document ID: US20120073210A1
- Status: Published application
- Kind: A1
- Application number: 12/893,666
- Filed: 2010-09-29
- Published: 2012-03-29
- Earliest claimed: 2010-09-29
- Assignees: Innopad, Inc.
- Inventors: Paul LEFEVRE; Oscar K. HSU; David Adam WELLS; John Erik ALDEBORGH; Marc C. JIN; Guangwei WU; Anoop MATHEW
- Web page: https://patentgrep.com/patent/US20120073210A1

## CPC

- B24B 37/205: {provided with a window for inspecting the surface of the work being lapped}
- B24B 37/26: characterised by the shape of the lapping pad surface, e.g. grooved
- B24D 18/00: Manufacture of grinding tools {or other grinding devices}, e.g. wheels, not otherwise provided for
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- B24D: TOOLS FOR GRINDING, BUFFING OR SHARPENING (abrading-bodies specially designed for tumbling apparatus, e.g. abrading-balls B24B31/14; honing tools B24B33/08; lapping tools B24B37/11)

## Abstract

A method of forming a chemical mechanical polishing pad. The method includes polymerizing one or more polymer precursors and forming a chemical-mechanical planarization pad including a surface, forming grooves in the surface defining lands between the grooves, wherein the grooves have a first width, and shrinking the lands from a first land length (L1) at the surface to a second land length (L2) at the surface, wherein the second land length (L2) is less than the first land length (L1) and the grooves have a second width (W2) wherein (W1)≦(X)(W2), wherein (X) has a value in the range of 0.01 to 0.75.

## Claims

### Claim 1

A method of forming a chemical-mechanical planarization pad, comprising:
polymerizing one or more polymer precursors and forming a chemical-mechanical planarization pad including a surface;
forming grooves in said surface defining lands between said grooves, wherein said grooves have a first width (W1); and
shrinking said lands from a first land length (L1) at said surface to a second land length (L2) at said surface, wherein said second land length (L2) is less than said first land length (L1) and said grooves have a second width (W2) wherein (W1)≦(X)(W2), wherein (X) has a value in the range of 0.01 to 0.75.

### Claim 2 (depends on 1)

The method of claim 1, wherein shrinking said lands comprises further polymerizing said polymer precursors after forming grooves in said surface.

### Claim 3 (depends on 1)

The method of claim 1, wherein said grooves have a first depth (D1) and after shrinking have a second depth (D2) wherein (D1)≦(Y)(D2) and (Y) has a value in the range of 0.80 to 0.95.

### Claim 4 (depends on 1)

The method of claim 1, wherein said (L1)≧(Z)(L2) and (Z) has a value in the range of 1.1 to 1.4.

### Claim 5 (depends on 1)

The method of claim 1, wherein shrinking said lands comprises heating said chemical-mechanical planarization pad at a temperature in the range of 110° F. to 400° F. for a period of time.

### Claim 6 (depends on 5)

The method of claim 5, wherein shrinking said lands further comprises cooling said chemical-mechanical planarization pad at a temperature of 80° F. to 150° F. for a period of time.

### Claim 7 (depends on 1)

The method of claim 1, wherein said chemical-mechanical planarization pad includes at least one embedded structure in a polymer matrix.

### Claim 8 (depends on 7)

The method of claim 7, wherein said embedded structure is not present in at least a portion of said polymer matrix and said chemical-mechanical planarization pad includes a window integral to said pad defined by said portion of said pad where said embedded structure is not present.

### Claim 9 (depends on 7)

The method of claim 7, wherein said at least one embedded structure includes soluble material.

### Claim 10

A method of forming chemical-mechanical planarization pad, comprising:
forming a chemical-mechanical planarization pad including a surface, wherein said chemical-mechanical planarization pad is formed by polymerizing polymer precursors to a selected degree of conversion;
forming one or more grooves into said surface of said chemical-mechanical planarization pad, wherein said grooves have a first width (W1) and a first depth (D1) and define lands between the grooves; and
thermally treating said chemical-mechanical planarization pad with said grooves formed in said surface, increasing said degree of conversion, and shrinking said lands wherein said grooves exhibit a second width (W2) and a second depth (D2), wherein said second width (W2) is greater than said first width (W1) and said second depth (D2) is greater than said first depth (D1).

### Claim 11 (depends on 10)

The method of claim 10, wherein said lands have a first length (L1) at said surface and after shrinking have a second length (L2) at said surface, wherein said second land length (L2) is less than said first land length (L1) wherein (L1)≧(Z)(L2) and (Z) has a value in the range of 1.1 to 1.4.

### Claim 12 (depends on 10)

The method of claim 10, wherein thermally treating said chemical-mechanical planarization pad includes at least partially immersing said chemical-mechanical planarization pad in a liquid bath or an oven.

### Claim 13 (depends on 10)

The method of claim 10, wherein thermally treating said chemical mechanical planarization pad includes heating said pad at a temperature in the range of 110° F. to 400° F. for a period of 10 hours or greater.

### Claim 14 (depends on 10)

The method of claim 10, wherein thermally treating said chemical mechanical planarization pad includes heating said pad at a temperature in the range of 160° F. to 190° F. for a period of 16 hours to 90 hours.

### Claim 15 (depends on 10)

The method of claim 10, wherein thermally treating said chemical-mechanical planarization pad includes cooling said chemical-mechanical planarization pad at an intermediate temperature in the range of 80° C. to 150° C. for a period of 10 minutes or greater.

### Claim 16 (depends on 10)

The method of claim 10, wherein thermally treating said chemical-mechanical planarization pad includes cooling said chemical-mechanical planarization pad at an intermediate temperature in the range of 100° F. to 130° F. for a period of 10 minutes to 120 minutes.

### Claim 17 (depends on 10)

The method of claim 10, wherein said chemical-mechanical planarization pad includes at least one embedded structure in a polymer matrix.

### Claim 18 (depends on 17)

The method of claim 17, wherein said embedded structure is not present in at least a portion of said polymer matrix and said chemical-mechanical planarization pad includes a window integral to said pad defined by said portion of said pad where said embedded structure is not present.

### Claim 19 (depends on 10)

The method of claim 10, wherein said embedded structure comprises one or a plurality of fibers.

### Claim 20 (depends on 10)

The method of claim 10, wherein said at least one embedded structure includes soluble material.