# US 2012/0057855 A1 · Heat Treatment Apparatus Emitting Flash of Light

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0057855 A1
- Document ID: US20120057855A1
- Status: Published application
- Kind: A1
- Application number: 13/298,562
- Filed: 2011-11-17
- Published: 2012-03-08
- Earliest claimed: 2007-02-09
- Assignees: Dainippon Screen Mfg. Co., Ltd.
- Inventors: Kenichi Yokouchi
- Web page: https://patentgrep.com/patent/US20120057855A1

## CPC

- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- F27B 5/18: Arrangement of controlling, monitoring, alarm or like devices
- F27B 17/0025: {specially adapted for treating semiconductor wafers}
- F27D 5/0037: {Supports specially adapted for semi-conductors}
- H10P 14/2923: {being conductive materials, e.g. metallic silicides}
- H10P 72/0432: {mainly by conduction}
- H10P 72/0436: {mainly by radiation}
- H10P 72/7624: {characterised by the mechanical construction of the susceptor, stage or support}
- H10P 72/7626: {characterised by the construction of the shaft}
- F27D 11/02: Ohmic resistance heating
- F27D 13/00: Apparatus for preheating charges; Arrangements for preheating charges
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE

## Abstract

Flash lamps connected to short-pulse circuits and flash lamps connected to long-pulse circuits are alternately arranged in a line. The duration of light emission from the flash lamps connected to the long-pulse circuits is longer than the duration of light emission from the flash lamps connected to the short-pulse circuits. A superimposing of a flash of light with a high peak intensity from the flash lamps that emit light for a short time and a flash of light with a gentle peak from the flash lamps that emit light for a long time can increase the temperature of even a deep portion of a substrate to an activation temperature or more without heating a shallow portion near the substrate surface more than necessary. This achieves the activation of deep junctions without causing substrate warpage or cracking.

## Claims

### Claim at position 1

-10. (canceled)

### Claim 11

A heat treatment method irradiating a substrate with a flash of light from a flash lamp to heat the substrate, comprising:
(a) a first irradiation step of irradiating said substrate with a flash of light for a duration of a first irradiation time; and
(b) a second irradiation step of irradiating said substrate with a flash of light for a duration of a second irradiation time longer than said first irradiation time,
wherein,
at least a part of the irradiation of a flash of light of said second irradiation step is superimposed on the irradiation of a flash of light of said first irradiation step.

### Claim 12 (depends on 11)

The heat treatment method according to claim 11, wherein
said first irradiation step and said second irradiation step are started at the same time.

### Claim 13 (depends on 11)

The heat treatment method according to claim 11, wherein
said first irradiation step and said second irradiation step are started at different times.

### Claim 14 (depends on 11)

The heat treatment method according to claim 11, wherein
said first irradiation time is approximately 1.0 milliseconds; and
said second irradiation time is approximately 3.0 milliseconds.

### Claim 15 (depends on 11)

The heat treatment method according to claim 11, wherein
a surface temperature of said substrate is risen to a treatment temperature not less than a predetermined value by the irradiation of flash of light of said first irradiation step, and the surface temperature of said substrate is maintained at said treatment temperature for not less than a predetermined duration of time by the irradiation of a flash of light by said second irradiation step.

### Claim 16

A heat treatment method irradiating a substrate with a flash of light from a flash lamp to heat the substrate, comprising:
(a) a first irradiation step of irradiating said substrate with a flash of light with a first peak intensity; and
(b) a second irradiation step of irradiating said substrate with a flash of light with a second peak intensity lower than said first peak intensity,
wherein,
at least a part of the irradiation of a flash of light of said second irradiation step is superimposed on the irradiation of a flash of light of said first irradiation step.

### Claim 17 (depends on 16)

The heat treatment method according to claim 16, wherein
said first irradiation step and said second irradiation step are started at the same time.

### Claim 18 (depends on 16)

The heat treatment method according to claim 16, wherein
said first irradiation step and said second irradiation step are started at different times.

### Claim 19 (depends on 16)

The heat treatment method according to claim 16, wherein
irradiation time of a flash of light in said first irradiation step is approximately 1.0 milliseconds; and
irradiation time of a flash of light in said second irradiation step is approximately 3.0 milliseconds.

### Claim 20 (depends on 16)

The heat treatment method according to claim 16, wherein
a surface temperature of said substrate is raised to a treatment temperature not less than a predetermined value by the irradiation of a flash of light of said first irradiation step, and the surface temperature of said substrate is maintained at said treatment temperature for not less than a predetermined duration of time by the irradiation of a flash of light by said second irradiation step.