# US 2012/0055590 A1 · Aluminum-lithium alloys, and methods for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0055590 A1
- Document ID: US20120055590A1
- Status: Published application
- Kind: A1
- Application number: 13/228,400
- Filed: 2011-09-08
- Published: 2012-03-08
- Earliest claimed: 2010-09-08
- Assignees: Alcoa Inc.
- Inventors: Rajeev G. Kamat; John M. Newman; Ralph R. Sawtell; Jen C. Lin
- Web page: https://patentgrep.com/patent/US20120055590A1

## CPC

- C22C 21/08: with silicon
- C22C 21/02: with silicon as the next major constituent
- C22C 21/10: with zinc as the next major constituent
- C22C 21/14: with silicon
- C22C 21/16: with magnesium
- C22F 1/053: of alloys with zinc as the next major constituent
- C22F 1/057: of alloys with copper as the next major constituent
- F16L 9/02: of metal (F16L9/16 - F16L9/22 take precedence)
- F24S 23/82: {characterised by the material or the construction of the reflector}
- Y02B 10/20: Solar thermal
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL
- F24S: SOLAR HEAT COLLECTORS; SOLAR HEAT SYSTEMS (for producing mechanical power from solar energy F03G6/00)
- Y02B: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO BUILDINGS, e.g. HOUSING, HOUSE APPLIANCES OR RELATED END-USER APPLICATIONS

## Abstract

New Al—Li alloy bodies and methods of producing the same are disclosed. The new Al—Li alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new Al—Li alloy bodies may realize improved strength and other properties.

## Claims

### Claim 1

A method comprising:
(a) preparing an aluminum alloy body for post-solutionizing cold work, wherein the aluminum alloy body includes an aluminum alloy having 0.25 to 5.0 wt. % lithium;
(i) wherein the preparing step comprises solutionizing of the aluminum alloy body;
(b) after the preparing step (a), cold working the aluminum alloy body by at least 25%; and
(c) after the cold working step (b), thermally treating the aluminum alloy body;
wherein the cold working and the thermally treating steps are accomplished to achieve an increase in long-transverse tensile yield strength as compared to a reference-version of the aluminum alloy body in the as cold-worked condition.

### Claim 2 (depends on 1)

The method of claim 1, wherein the preparing step (a) comprises:
casting the aluminum alloy body via a semi-continuous casting process.

### Claim 3 (depends on 2)

The method of claim 2, wherein the preparing step (a) comprises:
homogenizing the aluminum alloy body; and
hot working the aluminum alloy body;
wherein the solutionizing step (a)(i) occurs after the hot working step.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The method of claim 1, wherein the preparing step (a) comprises:
continuously casting the aluminum alloy body.

### Claim 6 (depends on 5)

The method of claim 5, wherein the preparing step (a) comprises:
concomitant to the continuously casting step, completing the solutionizing step (a)(i).

### Claim at position 7

7-9. (canceled)

### Claim 10 (depends on 1)

The method of claim 1, wherein the solutionizing step (a)(i) comprises quenching the aluminum alloy body, and wherein the quenching occurs in the absence of deformation of the aluminum alloy body.

### Claim 11 (depends on 1)

The method of claim 1, comprising forming the aluminum alloy body into a shape during the thermal treatment step (c).

### Claim 12 (depends on 1)

The method of claim 1, wherein no purposeful thermal heating treatments are applied to the aluminum alloy body between the solutionizing step (a)(i), and the cold working step (b).

### Claim at position 11

13-14. (canceled)

### Claim 15 (depends on 1)

The method of claim 1 or PI, wherein the cold working step (b) occurs in the absence of purposeful heating of the aluminum alloy body.

### Claim 16

(canceled)

### Claim 17 (depends on 1)

The method of claim 1, wherein the cold working step (b) comprises reducing the aluminum alloy body to its substantially final form.

### Claim 18 (depends on 17)

The method of claim 17, wherein the cold working step (b) comprises cold rolling the aluminum alloy body to final gauge.

### Claim 19

(canceled)

### Claim 20 (depends on 19)

The method of claim 19, wherein the cold working step (b) comprises cold working the aluminum alloy body from 35% to 90%.

### Claim 21

(canceled)

### Claim 22 (depends on 1)

The method of claim 1, wherein the thermally treating step (c) comprises maintaining the aluminum alloy body below its recrystallization temperature.

### Claim 23

(canceled)

### Claim 24 (depends on 22)

The method of claim 22, wherein the cold rolling step (b) and the thermally treating step (c) are performed such that the aluminum alloy body realizes a predominately unrecrystallized microstructure.

### Claim at position 22

25-26. (canceled)

### Claim 27

An aluminum alloy body comprising 0.25 to 5.0 wt. % lithium, wherein the aluminum alloy body realizes at least 5% higher tensile yield strength over a referenced aluminum alloy body;
wherein the referenced aluminum alloy body has the same composition as the aluminum alloy body;
wherein the referenced aluminum alloy body is processed to a T87 temper; and
wherein the referenced aluminum alloy body has a tensile yield strength that is within 1 ksi of its peak tensile yield strength.

### Claim at position 24

28-29. (canceled)

### Claim 30 (depends on 27)

The aluminum alloy body of claim 27, wherein the aluminum alloy body realizes an elongation of more than 4%.

### Claim 31

(canceled)

### Claim 32 (depends on 27)

The aluminum alloy body of claim 27, wherein the aluminum alloy body realizes a normalized R-value of at least 2.0.

### Claim at position 28

33-34. (canceled)

### Claim 35 (depends on 27)

The aluminum alloy body of claim 27, wherein the aluminum alloy body is predominately unrecrystallized.

### Claim 36 (depends on 35)

The aluminum alloy body of claim 35, wherein the aluminum alloy body is at least 75% unrecrystallized.

### Claim 37

A method comprising:
(a) solutionizing an aluminum alloy body, wherein the aluminum alloy body includes an aluminum alloy having 0.25-5.0 wt. % lithium;
(b) after the solutionizing step (a), cold working the aluminum alloy body by at least 25%;
(i) wherein, after the cold working step (b), the aluminum alloy body is in its substantially final form; and
(c) after the cold working step (b), thermally treating the aluminum alloy body.