Geothermal grout, and methods of preparing and utilizing same
OwnerJeffrey J. Konczakinventor
Life of this patent
Estimating the term…
Abstract
A thermally enhanced, single component, geothermal grout from recycled materials, such as class F fly ash and cement kiln dust. Additional components can include a mid-range water reducer and a dry caustic.
Claims2
1-19. (canceled)
A method of preparing a thermally enhanced geothermal grout from recycled materials, comprising the steps of:
- preparing a single component dry grout mixture comprising approximately 50-80% class F fly ash and approximately 20-50% cement kiln dust;
- adding approximately five gallons of water to approximately 70 pounds of said dry grout mixture;
- adding a mid-range water reducer at an addition rate of approximately 0-8 fluid ounce equivalent per hundred-weight of said dry grout mixture;
- and
- adding dry sodium hydroxide at an addition rate of between approximately 0-12 dry ounces per hundred weight of said dry grout mixture.
2 more elements